JP2004331897A5 - - Google Patents

Download PDF

Info

Publication number
JP2004331897A5
JP2004331897A5 JP2003132514A JP2003132514A JP2004331897A5 JP 2004331897 A5 JP2004331897 A5 JP 2004331897A5 JP 2003132514 A JP2003132514 A JP 2003132514A JP 2003132514 A JP2003132514 A JP 2003132514A JP 2004331897 A5 JP2004331897 A5 JP 2004331897A5
Authority
JP
Japan
Prior art keywords
resistance
meth
polymerized
stickiness
glass transition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2003132514A
Other languages
English (en)
Japanese (ja)
Other versions
JP2004331897A (ja
JP4434622B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2003132514A priority Critical patent/JP4434622B2/ja
Priority claimed from JP2003132514A external-priority patent/JP4434622B2/ja
Publication of JP2004331897A publication Critical patent/JP2004331897A/ja
Publication of JP2004331897A5 publication Critical patent/JP2004331897A5/ja
Application granted granted Critical
Publication of JP4434622B2 publication Critical patent/JP4434622B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP2003132514A 2003-05-12 2003-05-12 熱重合型アクリル塗料,塗装金属板及びその製造方法 Expired - Fee Related JP4434622B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2003132514A JP4434622B2 (ja) 2003-05-12 2003-05-12 熱重合型アクリル塗料,塗装金属板及びその製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2003132514A JP4434622B2 (ja) 2003-05-12 2003-05-12 熱重合型アクリル塗料,塗装金属板及びその製造方法

Publications (3)

Publication Number Publication Date
JP2004331897A JP2004331897A (ja) 2004-11-25
JP2004331897A5 true JP2004331897A5 (enExample) 2006-06-08
JP4434622B2 JP4434622B2 (ja) 2010-03-17

Family

ID=33507338

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2003132514A Expired - Fee Related JP4434622B2 (ja) 2003-05-12 2003-05-12 熱重合型アクリル塗料,塗装金属板及びその製造方法

Country Status (1)

Country Link
JP (1) JP4434622B2 (enExample)

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4885497B2 (ja) * 2005-08-11 2012-02-29 日新製鋼株式会社 液晶バックライト反射板用白色塗装金属板
JP2007217561A (ja) * 2006-02-16 2007-08-30 Nisshin Steel Co Ltd 熱重合型アクリル塗料
JP4845626B2 (ja) * 2006-07-28 2011-12-28 日新製鋼株式会社 異臭の少ない塗膜形成用塗料組成物
JP5110844B2 (ja) * 2006-10-06 2012-12-26 日新製鋼株式会社 塗装金属材料および塗膜の製法
EP2369637B1 (en) 2008-12-12 2014-02-26 Toray Industries, Inc. Film for sealing back side of solar cell, material for sealing back side of solar cell, and solar cell module

Similar Documents

Publication Publication Date Title
JP2004516338A5 (enExample)
JP2005529870A5 (enExample)
JP2010501670A5 (enExample)
JP2009035602A5 (enExample)
JP2004361692A5 (enExample)
WO2001074964A1 (en) Vibration damper composition
JP2005508436A5 (enExample)
JP2008291071A5 (enExample)
DE60311644D1 (de) Thermisch aushaertbare zusammensetzung, verfahren und artikel
JP2004532847A5 (enExample)
EP1550690A4 (en) HEAT SHRINKABLE FOIL
WO2005003250A3 (fr) Composition silicone reticulable en gel adhesif
JP2005533138A5 (enExample)
DE602007012453D1 (de) Chloroprenpolymerlatex und herstellungsverfahren dafür
WO2009055378A3 (en) (meth)acrylic film and marking film using same
TW200604217A (en) Radiation-sensitive resin composition, spacer, and method of forming the same
JP2009046535A5 (enExample)
JP2013517158A5 (enExample)
JP2007051233A5 (enExample)
JP2004331897A5 (enExample)
JP2007210240A5 (enExample)
EP1489116A4 (en) DIBLOCK COPOLYMER AND THESE ADHESIVE ADHESIVE COMPOSITIONS
TW200636037A (en) Pressure-sensitive adhesive composition and optical element
JP2005306967A5 (enExample)
JP2005532435A5 (enExample)