JP2004232074A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2004232074A5 JP2004232074A5 JP2003034583A JP2003034583A JP2004232074A5 JP 2004232074 A5 JP2004232074 A5 JP 2004232074A5 JP 2003034583 A JP2003034583 A JP 2003034583A JP 2003034583 A JP2003034583 A JP 2003034583A JP 2004232074 A5 JP2004232074 A5 JP 2004232074A5
- Authority
- JP
- Japan
- Prior art keywords
- dew point
- surface layer
- annealing
- atmosphere
- contact resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000137 annealing Methods 0.000 description 4
- 239000002344 surface layer Substances 0.000 description 3
- 238000010438 heat treatment Methods 0.000 description 1
- 239000011159 matrix material Substances 0.000 description 1
- 229910052814 silicon oxide Inorganic materials 0.000 description 1
- 229910001220 stainless steel Inorganic materials 0.000 description 1
- 239000010935 stainless steel Substances 0.000 description 1
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2003034583A JP4340448B2 (ja) | 2002-03-28 | 2003-02-13 | 燃料電池セパレータ用フェライト系ステンレス鋼及びその製造方法 |
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2002092995 | 2002-03-28 | ||
| JP2002354690 | 2002-12-06 | ||
| JP2003034583A JP4340448B2 (ja) | 2002-03-28 | 2003-02-13 | 燃料電池セパレータ用フェライト系ステンレス鋼及びその製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2004232074A JP2004232074A (ja) | 2004-08-19 |
| JP2004232074A5 true JP2004232074A5 (enExample) | 2006-03-30 |
| JP4340448B2 JP4340448B2 (ja) | 2009-10-07 |
Family
ID=32966222
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2003034583A Expired - Lifetime JP4340448B2 (ja) | 2002-03-28 | 2003-02-13 | 燃料電池セパレータ用フェライト系ステンレス鋼及びその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP4340448B2 (enExample) |
Families Citing this family (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2006302729A (ja) * | 2005-04-22 | 2006-11-02 | Nisshin Steel Co Ltd | 固体高分子型燃料電池用ステンレス鋼製セパレータ及び固体高分子型燃料電池 |
| EP1906477A1 (en) | 2005-06-22 | 2008-04-02 | Nippon Steel Corporation | Separator for solid polymer electrolyte fuel cell of stainless steel, titanium or titanium alloy, process for producing the same, and method for evaluating warping and twisting of separator |
| JP5014644B2 (ja) | 2006-02-27 | 2012-08-29 | 新日本製鐵株式会社 | 固体高分子型燃料電池用セパレータおよびその製造方法 |
| CN101680045B (zh) | 2007-03-06 | 2015-08-19 | Ati资产公司 | 减少在铁素体不锈钢上形成电阻层的方法 |
| KR100993412B1 (ko) * | 2008-12-29 | 2010-11-09 | 주식회사 포스코 | 고분자 연료전지 분리판용 스테인리스강 및 그 제조방법 |
| CA2769855C (en) | 2009-08-03 | 2015-01-06 | Nippon Steel Corporation | Titanium material for solid polymer fuel cell separator use and method of production of same |
| JP6037882B2 (ja) * | 2012-02-15 | 2016-12-07 | 新日鐵住金ステンレス株式会社 | 耐スケール剥離性に優れたフェライト系ステンレス鋼板及びその製造方法 |
| JP6071608B2 (ja) | 2012-03-09 | 2017-02-01 | 新日鐵住金ステンレス株式会社 | 耐酸化性に優れたフェライト系ステンレス鋼板 |
| CA2907970C (en) | 2013-03-27 | 2021-05-25 | Nippon Steel & Sumikin Stainless Steel Corporation | Hot-rolled ferritic stainless-steel plate, process for producing same, and steel strip |
| JP2014198868A (ja) * | 2013-03-29 | 2014-10-23 | 日立金属株式会社 | 固体酸化物形燃料電池用ステンレス鋼の製造方法 |
| JP6489770B2 (ja) * | 2013-09-26 | 2019-03-27 | 日新製鋼株式会社 | 非水電解液環境での溶出量の少ないステンレス鋼板およびその製造方法ならびに非水電解液二次電池の外装部材 |
| US11189846B2 (en) * | 2017-04-28 | 2021-11-30 | Flosfia Inc. | Electrically-conductive member and method of manufacturing the same |
| JP7278476B2 (ja) * | 2020-04-15 | 2023-05-19 | 日鉄ステンレス株式会社 | フェライト系ステンレス鋼材およびその製造方法 |
| JP7563919B2 (ja) * | 2020-08-25 | 2024-10-08 | 日鉄ステンレス株式会社 | フェライト系ステンレス鋼及びその製造方法 |
-
2003
- 2003-02-13 JP JP2003034583A patent/JP4340448B2/ja not_active Expired - Lifetime
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2004232074A5 (enExample) | ||
| EP1596068A3 (en) | Vacuum pump | |
| JP2005511892A5 (enExample) | ||
| EP1383165A3 (en) | Peeling method | |
| EP2072483A3 (en) | Ceramic-copper foil bonding method | |
| EP1965419A3 (en) | Absorber layer candidates and techniques for application | |
| JP2005513811A5 (enExample) | ||
| EP1217682A3 (en) | Method of forming thin film of inorganic solid electrolyte | |
| WO2005087677A3 (en) | Coated article with zinc oxide over ir reflecting layer and corresponding method | |
| CA2520700A1 (en) | A method of producing a ni based alloy | |
| WO2006001541A3 (en) | Aluminum heat exchange tube and process for fabricating same | |
| WO2007008643A3 (en) | Insulating glass (ig) window unit including heat treatable coating with specific color characteristics and low sheet resistance | |
| JP2002510751A5 (enExample) | ||
| EP1369747A3 (en) | Electrophotographic lamination film, a method of producing the same, and a method of forming an image | |
| CN103882193A (zh) | 一种外层氧化的冷轧无取向电工钢退火方法 | |
| CN103173700B (zh) | Al-Cu-Li-X铝锂合金表面脱锂层的制备方法 | |
| JP2006093552A5 (enExample) | ||
| JP2003321299A5 (enExample) | ||
| WO2017067049A1 (zh) | 一种发热体的加工工艺 | |
| JP2006152061A5 (enExample) | ||
| CA2319974A1 (en) | A stainless steel sheet having cu-enriched grains dispersed in its matrix and/or a cu-condensed layer | |
| WO2004080659A3 (en) | Antistatic composition and part holder | |
| CN106587040A (zh) | 石墨烯薄膜的衬底转移方法 | |
| WO2009050840A1 (ja) | 絶縁膜の形成方法及び半導体素子 | |
| EP1750301A3 (en) | On-die heating circuit and control loop for rapid heating of the die |