Prior art keywords
polymer
core
sheath
component
elongation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2002007289A
Other languages
English (en)
Other versions
JP3778086B2 (ja
JP2003213527A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2002007289A priority Critical patent/JP3778086B2/ja
Priority claimed from JP2002007289A external-priority patent/JP3778086B2/ja
Publication of JP2003213527A publication Critical patent/JP2003213527A/ja
Publication of JP2003213527A5 publication Critical patent/JP2003213527A5/ja
Application granted granted Critical
Publication of JP3778086B2 publication Critical patent/JP3778086B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Claims (2)

  1. 鞘両成分をポリエチレンテレフタレートとし、芯成分のポリマーの固有粘度(IV)をX、鞘成分のポリマーの固有粘度(IV)をYとしたとき、X−Y≧0.25を満足する組み合わせのポリマーを用いて芯鞘の重量複合比95:5〜75:25で口金下に加熱筒を設置して溶融紡糸を行い、次いでホットローラーで延伸する破断強度6.5cN/dtex以上のスクリーン紗用ポリエステルモノフィラメントの製造方法。
  2. 破断伸度が15〜30%、10%伸張時のモジュラスが破断強度の70〜100%であることを特徴とする請求項1記載の製造方法で製造したスクリーン紗用ポリエステルモノフィラメント。
JP2002007289A 2002-01-16 2002-01-16 スクリーン紗用ポリエステルモノフィラメントおよび製造方法 Expired - Lifetime JP3778086B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2002007289A JP3778086B2 (ja) 2002-01-16 2002-01-16 スクリーン紗用ポリエステルモノフィラメントおよび製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2002007289A JP3778086B2 (ja) 2002-01-16 2002-01-16 スクリーン紗用ポリエステルモノフィラメントおよび製造方法

Publications (3)

Publication Number Publication Date
JP2003213527A JP2003213527A (ja) 2003-07-30
JP2003213527A5 true JP2003213527A5 (ja) 2005-07-07
JP3778086B2 JP3778086B2 (ja) 2006-05-24

Family

ID=27645843

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2002007289A Expired - Lifetime JP3778086B2 (ja) 2002-01-16 2002-01-16 スクリーン紗用ポリエステルモノフィラメントおよび製造方法

Country Status (1)

Country Link
JP (1) JP3778086B2 (ja)

Families Citing this family (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2005240266A (ja) * 2004-01-26 2005-09-08 Toray Ind Inc スクリーン紗用ポリエステルモノフィラメント
EP1793022B1 (en) 2005-07-28 2010-12-01 Teijin Fibers Limited (spun-dyed) polyester monofilament
JP4661501B2 (ja) * 2005-09-29 2011-03-30 東レ株式会社 スクリーン紗用モノフィラメント
JP2010077563A (ja) * 2008-09-26 2010-04-08 Toray Ind Inc ポリエステルモノフィラメント
JP5336615B2 (ja) * 2012-01-06 2013-11-06 帝人株式会社 スクリーン紗用モノフィラメント
WO2020067224A1 (ja) * 2018-09-27 2020-04-02 東レ株式会社 スクリーン紗用ポリエステルモノフィラメントおよびダイレクトデジタル製版用メッシュ織物

Similar Documents

Publication Publication Date Title
ATE526439T1 (de) Polypropylenfaser, verfahren zu ihrer herstellung und ihre anwendung
JP2005256268A (ja) 皮革様シート状物およびその製造方法
JP2006505712A5 (ja)
JP2003213527A5 (ja)
CN102758311A (zh) 凹凸伸缩无纺布及其制造方法
JP4419503B2 (ja) パイル繊維およびパイル布帛
JP2003213528A5 (ja)
JP2006511726A5 (ja)
CN100334272C (zh) 复合纤维及其制造方法
JP2008075224A5 (ja)
JP2006200064A5 (ja)
JP5819735B2 (ja) 冷感に優れた混繊糸
TR199902157A2 (xx) Y�ksek denyeli iplik �retme tekni�i
JP2005113309A (ja) 異形断面ポリトリメチレンテレフタレート繊維
CN203080244U (zh) 一种电气胶带基布用缝编非织造布
JP4316783B2 (ja) 長繊維不織布の製造方法
JP2006176937A (ja) 抗ピル性細繊度アクリル系繊維及びその製造方法並びに紡績糸
JP2007231473A (ja) 混繊複合糸及びその製造法
JP3886808B2 (ja) ポリ乳酸自発捲縮繊維
JP3462914B2 (ja) エアバッグ用糸条
JP4310833B2 (ja) 安全ネット
JP2000345433A (ja) ストレッチ性織編物用ポリエステル複合繊維
JP4955278B2 (ja) エアレイド不織布用ポリエステル系繊維およびその製造方法
JP2008207777A (ja) 車両内装材
JP2000256954A (ja) 伸縮性不織布