GB1441612A - Method of making photographic silver halide materials - Google Patents
Method of making photographic silver halide materialsInfo
- Publication number
- GB1441612A GB1441612A GB268773A GB268773A GB1441612A GB 1441612 A GB1441612 A GB 1441612A GB 268773 A GB268773 A GB 268773A GB 268773 A GB268773 A GB 268773A GB 1441612 A GB1441612 A GB 1441612A
- Authority
- GB
- United Kingdom
- Prior art keywords
- silver halide
- silver
- halide
- emulsions
- emulsion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
1441612 Internally-sensitive photographic silver halide emulsions KODAK Ltd 18 Jan 1974 [18 Jan 1973 29 March 1973] 2687/73 Heading G2C Photographic silver halide emulsions having internal sensitivity are made by laying down further silver halide on to the grains of a surface sensitive or surface fogged silver halide emulsion by making alternate additions of silver ions and halide ions. Thereto such that alternate excesses of silver and halide ions are produced in the emulsion. Depending on the number of cycles of alternate excesses of silver and halide ion, the emulsions may show some surface and some internal sensitivity or only internal sensitivity, the latter requiring 7-20 cycles. The desensitizing effect of certain optically sensitizing dyes on the original emulsion is reduced or eliminated by the layer of further silver halide laid down. The internally sensitive silver halide emulsions obtained as above give direct positive images on image-wise exposure and development with a fogging developer.
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB268773A GB1441612A (en) | 1973-01-18 | 1973-01-18 | Method of making photographic silver halide materials |
DE19742402130 DE2402130C3 (en) | 1973-01-18 | 1974-01-17 | Process for the preparation of a silver halide photographic emulsion containing internally sensitive silver halide grains |
BE139995A BE809950A (en) | 1973-01-18 | 1974-01-18 | Photographic emulsion with internally sensitised grains - mfd by pptn of silver halide on surface sensitised or fogged grains by alternate addn. of excess silver halide ions |
JP799674A JPS581408B2 (en) | 1973-01-18 | 1974-01-18 | Shin-halogen storage case |
US502695A US3917485A (en) | 1973-01-18 | 1974-09-03 | Method of making photographic silver halide emulsions and products thereof |
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB268773A GB1441612A (en) | 1973-01-18 | 1973-01-18 | Method of making photographic silver halide materials |
GB1512773 | 1973-03-29 |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1441612A true GB1441612A (en) | 1976-07-07 |
Family
ID=26237669
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB268773A Expired GB1441612A (en) | 1973-01-18 | 1973-01-18 | Method of making photographic silver halide materials |
Country Status (3)
Country | Link |
---|---|
JP (1) | JPS581408B2 (en) |
DE (1) | DE2402130C3 (en) |
GB (1) | GB1441612A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4539290A (en) * | 1983-09-27 | 1985-09-03 | E. I. Du Pont De Nemours And Company | Process for pulsed flow, balanced double jet precipitation |
US4666669A (en) * | 1983-09-27 | 1987-05-19 | E. I. Du Pont De Nemours And Company | Apparatus for pulsed flow, balanced double jet precipitation |
Families Citing this family (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63264740A (en) * | 1986-12-22 | 1988-11-01 | Fuji Photo Film Co Ltd | Silver halide photographic sensitive material |
JPH0769579B2 (en) * | 1987-11-26 | 1995-07-31 | 富士写真フイルム株式会社 | Silver halide photographic light-sensitive material |
US5156946A (en) * | 1988-05-30 | 1992-10-20 | Fuji Photo Film Co., Ltd | Silver halide photographic materials |
GB8821433D0 (en) * | 1988-09-13 | 1988-10-12 | Ciba Geigy Ag | Photographic emulsions |
EP0376500B1 (en) * | 1988-12-27 | 1994-04-13 | Ilford Ag | Process for the spectral sensitisation of a silver halide emulsion |
EP0382950B1 (en) * | 1989-02-17 | 1995-05-10 | Agfa-Gevaert N.V. | Process for the production of silver halide emulsions |
-
1973
- 1973-01-18 GB GB268773A patent/GB1441612A/en not_active Expired
-
1974
- 1974-01-17 DE DE19742402130 patent/DE2402130C3/en not_active Expired
- 1974-01-18 JP JP799674A patent/JPS581408B2/en not_active Expired
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4539290A (en) * | 1983-09-27 | 1985-09-03 | E. I. Du Pont De Nemours And Company | Process for pulsed flow, balanced double jet precipitation |
US4666669A (en) * | 1983-09-27 | 1987-05-19 | E. I. Du Pont De Nemours And Company | Apparatus for pulsed flow, balanced double jet precipitation |
Also Published As
Publication number | Publication date |
---|---|
DE2402130A1 (en) | 1974-08-01 |
JPS581408B2 (en) | 1983-01-11 |
DE2402130C3 (en) | 1980-08-21 |
JPS49106321A (en) | 1974-10-08 |
DE2402130B2 (en) | 1979-12-13 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1151782A (en) | Photographic silver halide emulsions | |
GB1528836A (en) | Photographic colour silver halide materials | |
GB935249A (en) | Improvements in sensitive photographic materials | |
GB1387033A (en) | Photographic direct-positive process and silver halide emulsion therefor | |
GB1166451A (en) | Photographic Reproduction | |
GB1441612A (en) | Method of making photographic silver halide materials | |
GB1159856A (en) | Sensitive Photographic Silver Halide Materials | |
GB1160524A (en) | Photographic Materials and methods | |
GB1318723A (en) | Sensitive photographic materials | |
GB1139896A (en) | Light- and heat-sensitive recording materials and information recording processes using such materials | |
JPS5366731A (en) | Formation of hard tone photographic image | |
GB1086657A (en) | Photographic silver halide light sensitive materials | |
GB1080976A (en) | Improvements in or relating to colour photography | |
JPS5789749A (en) | Silver halide photographic sensitive material | |
GB1257257A (en) | ||
JPS5752048A (en) | Direct positive type photographic sensitive silver halide material | |
GB1155053A (en) | Sensitive Silver Halide Photographic Materials | |
GB1178683A (en) | Sensitive Silver Halide Photographic Materials | |
JPS5415731A (en) | Silver halide photographic material | |
GB1237192A (en) | Information-recording processes and materials | |
GB1195838A (en) | A Method of Producing Photographic Images | |
GB1250151A (en) | ||
GB1189416A (en) | Fixing Composition for Photographic Silver Halide Light-Sensitive Elements | |
JPS5320326A (en) | Color photographic image formation | |
GB1195608A (en) | Fog Inhibition in Photographic Elements |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed | ||
PCNP | Patent ceased through non-payment of renewal fee |