FR2367563A1 - Procede et installation - Google Patents
Procede et installationInfo
- Publication number
- FR2367563A1 FR2367563A1 FR7631803A FR7631803A FR2367563A1 FR 2367563 A1 FR2367563 A1 FR 2367563A1 FR 7631803 A FR7631803 A FR 7631803A FR 7631803 A FR7631803 A FR 7631803A FR 2367563 A1 FR2367563 A1 FR 2367563A1
- Authority
- FR
- France
- Prior art keywords
- die
- steel
- vis
- cooling medium
- contiguous
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Fabrication de fils à partir d'un jet d'acier liquide contenant du silicium et du manganèse et projeté à travers une filière dans une enceinte contenant un milieu refroidisseur réactif. Selon l'invention, le milieu refroidisseur est un mélange gazeux ayant vis-à-vis de l'acier, au moins dans la zone 22, contiguë à la filière 23, un pouvoir d'oxydation tel que le produit d'oxydation de l'acier, à l'équilibre thermochimique correspondant à la température régnant au voisinage de l'orifice de la filière, soit de la silice.
Priority Applications (14)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7631803A FR2367563A1 (fr) | 1976-10-15 | 1976-10-15 | Procede et installation |
AU22656/77A AU510822B2 (en) | 1976-02-27 | 1977-02-27 | Gas separation by adsorption at sub-atmospheric pressure |
CA288,762A CA1106133A (fr) | 1976-10-15 | 1977-10-14 | Gaz reactif de refroidissement pour la fabrication de fil d'acier |
IT69304/77A IT1090894B (it) | 1976-10-15 | 1977-10-14 | Procedimento e dispositivo per la fabbricazione dei fili mediante proiezione di un getto metallico liquido in un mezzo raffreddante |
ES463224A ES463224A1 (es) | 1976-10-15 | 1977-10-14 | Procedimiento para fabricar cables a partir de chorros de acero liquido. |
DE2746339A DE2746339C3 (de) | 1976-10-15 | 1977-10-14 | Verwendung eines Gasgemischs als Kühlmedium beim Stranggießen von Stahldrähten |
JP52123970A JPS5935310B2 (ja) | 1976-10-15 | 1977-10-15 | 液状金属の噴流をこの中に噴出することによって金属線を製造するためのガス冷媒 |
LU78328A LU78328A1 (fr) | 1976-10-15 | 1977-10-17 | |
GB43152/77A GB1586790A (en) | 1976-10-15 | 1977-10-17 | Method of and plant for the manufacture of wires from liquid metal |
AU29783/77A AU510922B2 (en) | 1976-10-15 | 1977-10-17 | Reactive gaseous cooling in melt extrusion |
BE181796A BE859795A (fr) | 1976-10-15 | 1977-10-17 | Procede et installation de fabrication d'un fil par projection d'un jet de metal liquide dans un milieu refroidisseur gazeux |
AT740977A AT357712B (de) | 1976-10-15 | 1977-10-17 | Einrichtung zum stranggiessen von stahldraehten |
SE7711664A SE432545B (sv) | 1976-10-15 | 1977-10-17 | Anvendning av en gasblandning som kylmedium vid strengpressning av staltradar |
US05/842,896 US4131151A (en) | 1976-10-15 | 1977-10-17 | Reactive gaseous cooling medium for the manufacture of wire |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7631803A FR2367563A1 (fr) | 1976-10-15 | 1976-10-15 | Procede et installation |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2367563A1 true FR2367563A1 (fr) | 1978-05-12 |
FR2367563B1 FR2367563B1 (fr) | 1982-02-05 |
Family
ID=9179066
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7631803A Granted FR2367563A1 (fr) | 1976-02-27 | 1976-10-15 | Procede et installation |
Country Status (13)
Country | Link |
---|---|
US (1) | US4131151A (fr) |
JP (1) | JPS5935310B2 (fr) |
AT (1) | AT357712B (fr) |
AU (1) | AU510922B2 (fr) |
BE (1) | BE859795A (fr) |
CA (1) | CA1106133A (fr) |
DE (1) | DE2746339C3 (fr) |
ES (1) | ES463224A1 (fr) |
FR (1) | FR2367563A1 (fr) |
GB (1) | GB1586790A (fr) |
IT (1) | IT1090894B (fr) |
LU (1) | LU78328A1 (fr) |
SE (1) | SE432545B (fr) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2460169A1 (fr) * | 1979-07-02 | 1981-01-23 | Michelin & Cie | Procede de refroidissement d'un fil metallique a partir d'un jet liquide |
FR2636552A1 (fr) * | 1988-09-21 | 1990-03-23 | Michelin & Cie | Procedes et dispositifs pour obtenir des fils en alliages metalliques amorphes |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3861452A (en) * | 1971-05-10 | 1975-01-21 | Establissements Michelin Raiso | Manufacture of thin, continuous steel wires |
GB1425915A (en) * | 1972-06-22 | 1976-02-25 | British Steel Corp | Rolling mills |
US3788786A (en) * | 1972-08-30 | 1974-01-29 | Monsanto Co | Orifice assembly for extruding low-viscosity melts |
-
1976
- 1976-10-15 FR FR7631803A patent/FR2367563A1/fr active Granted
-
1977
- 1977-10-14 DE DE2746339A patent/DE2746339C3/de not_active Expired
- 1977-10-14 IT IT69304/77A patent/IT1090894B/it active
- 1977-10-14 ES ES463224A patent/ES463224A1/es not_active Expired
- 1977-10-14 CA CA288,762A patent/CA1106133A/fr not_active Expired
- 1977-10-15 JP JP52123970A patent/JPS5935310B2/ja not_active Expired
- 1977-10-17 LU LU78328A patent/LU78328A1/xx unknown
- 1977-10-17 AT AT740977A patent/AT357712B/de not_active IP Right Cessation
- 1977-10-17 BE BE181796A patent/BE859795A/fr not_active IP Right Cessation
- 1977-10-17 SE SE7711664A patent/SE432545B/xx not_active IP Right Cessation
- 1977-10-17 AU AU29783/77A patent/AU510922B2/en not_active Expired
- 1977-10-17 US US05/842,896 patent/US4131151A/en not_active Expired - Lifetime
- 1977-10-17 GB GB43152/77A patent/GB1586790A/en not_active Expired
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2460169A1 (fr) * | 1979-07-02 | 1981-01-23 | Michelin & Cie | Procede de refroidissement d'un fil metallique a partir d'un jet liquide |
FR2636552A1 (fr) * | 1988-09-21 | 1990-03-23 | Michelin & Cie | Procedes et dispositifs pour obtenir des fils en alliages metalliques amorphes |
EP0360104A1 (fr) * | 1988-09-21 | 1990-03-28 | Compagnie Generale Des Etablissements Michelin-Michelin & Cie | Procédés et dispositifs pour obtenir des fils en alliages métalliques amorphes |
US5000251A (en) * | 1988-09-21 | 1991-03-19 | Compagnie Generale Des Etablissements Michelin-Michelin & Cie | Methods and apparatus for obtaining wires of amorphous metallic alloys |
Also Published As
Publication number | Publication date |
---|---|
ATA740977A (de) | 1979-12-15 |
ES463224A1 (es) | 1978-06-16 |
SE7711664L (sv) | 1978-04-16 |
FR2367563B1 (fr) | 1982-02-05 |
US4131151A (en) | 1978-12-26 |
DE2746339A1 (de) | 1978-04-20 |
BE859795A (fr) | 1978-02-15 |
DE2746339B2 (fr) | 1979-11-08 |
IT1090894B (it) | 1985-06-26 |
JPS5935310B2 (ja) | 1984-08-28 |
AU2978377A (en) | 1979-04-26 |
SE432545B (sv) | 1984-04-09 |
GB1586790A (en) | 1981-03-25 |
LU78328A1 (fr) | 1978-06-12 |
CA1106133A (fr) | 1981-08-04 |
DE2746339C3 (de) | 1980-07-24 |
AT357712B (de) | 1980-07-25 |
JPS5350014A (en) | 1978-05-08 |
AU510922B2 (en) | 1980-07-17 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR2376821A1 (fr) | Procede de fabrication de silicium tres pur | |
US3565345A (en) | Production of an article of high purity metal oxide | |
US4386258A (en) | High frequency magnetic field coupling arc plasma reactor | |
US2829960A (en) | Method and metallurgical device for the refining of steel | |
FI874025A0 (fi) | Modifierade keramiska strukturer och foerfaranden foer framstaellning av dessa. | |
US3565346A (en) | Method and apparatus for forming an article of high purity metal oxide | |
FR2367563A1 (fr) | Procede et installation | |
KR860001333A (ko) | 고온 생성가스의 냉각장치 | |
KR950032659A (ko) | 현탁 용융방법 및 장치 | |
US20050257570A1 (en) | Method and device for producing a blank mold from synthetic quartz glass by using a plasma-assisted deposition method | |
JPS561250A (en) | Production of rapidly cooled alloy sheet | |
US2295591A (en) | Method for preventing corrosion of hydrogen chloride burners and coolers | |
US2405580A (en) | Method for producing alkali metal oxides | |
GB836275A (en) | Process for the production of finely divided ferromagnetic iron oxide | |
GB1161077A (en) | Process for the Preparation of Finely Divided Titanium Dioxide. | |
EP0128987A3 (en) | Tuyere and method for blowing gas into molten metal | |
SU1066944A1 (ru) | Способ изготовлени труб из кварцевых и высококремнеземистых стекол | |
JPS61136901A (ja) | 重炭化水素を部分的に酸化するバーナー及び同酸化方法 | |
FR2372819A1 (fr) | Procede pour debarrasser un anhydride phtalique de la 1,4-naphtoquinone contenue en impurete, et produit obtenu par ce procede | |
FR2441581A1 (fr) | Procede pour la fabrication par la voie pyrogene d'oxyde finement divise d'un metal et/ou d'un metalloide | |
Miller et al. | Reactions of Titanium Tetrachloride in a Radio-Frequency Plasma Torch | |
BE904787A (fr) | Procede et dispositif destines a la fabrication notamment , d'acier | |
JPS5635714A (en) | Operating method of continuous type molten steel degassing equipment | |
JPS56158809A (en) | Protecting method for bottom blowing nozzle of gas for metal refining furnace | |
SU1675343A1 (ru) | Фурма |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |