FI67410B - Foerfarande foer rengoering av katoder - Google Patents
Foerfarande foer rengoering av katoder Download PDFInfo
- Publication number
- FI67410B FI67410B FI803136A FI803136A FI67410B FI 67410 B FI67410 B FI 67410B FI 803136 A FI803136 A FI 803136A FI 803136 A FI803136 A FI 803136A FI 67410 B FI67410 B FI 67410B
- Authority
- FI
- Finland
- Prior art keywords
- cathodes
- katoder
- foerfarande foer
- washing
- electrolyte
- Prior art date
Description
1 67410
Menetelmä katodien puhdistamiseksi
Keksinnön kohteena on menetelmä elektrolyyttisesti tuotettujen metallikatodien, erityisesti kuparikatodien 5 puhdistamiseksi.
Kuparin sähköisessä raffinoinnissa ovat anodit ja katodit kosketuksessa elektrolyytin kanssa, joka kupari-ionien ja rikkihapon ohella sisältää joukon muita alkuaineita osaksi merkittävissä väkevyyksissä. Eräästä tyypil-10 lisestä tällaisen elektrolyytin koostumuksesta annetaan seuraava esimerkki:
Elektrolyyttikoostumus g/l:ssa:
Cu 42; Ni 20; As Sb 0,5; Co 0,18; Fe 0,10; Mn 0,11;
Zn 0,17; Pb 0,018; Na 0,39; K 0,012; Mg 0,13; Ca 0,31; 15 H_ SO. 180.
2 4
Katodeja käynnistettäessä tarttuu elektrolyyttejä katodien pinnoille ja aiheuttavat sisäänsulamalla osan kuparin epäpuhtauksista. Elektrolyyttikuparin kokonaisepä-puhtaudet ovat tavallisesti 20-50 ppm. Jokunen prosentti 20 epäpuhtauksista sulatetussa kuparissa johtuu elektrolyytin tarttumisesta katodipinnoille.
Sentähden on huolehdittava että katodit elektrolyy-sikennosta nostamisen jälkeen pestään perusteellisesti. Tavallisesti tämä pesuvaihe käsittää katodien upottamisen 25 kuumaan veteen, höyryllä suihkuttamisen tai suurpainevedellä puhdistamisen. Nämä menettelytavat ovat kuitenkin epätäydellisiä silloin, kun katodien pinnat eivät ole sileitä vaan niissä on uurteita, nyppylöitä ja syöpymisvikoja.
Keksinnön mukaiselle menetelmälle on ominaista, että 30 käyteään ultraäänipesua, jolloin sammiossa kuumilla pesuvesillä, joista kaasu on poistettu ultraäänivärähtelyillä kHz-alueilla aikaansaadaan kavitaatiorakkuloita ja ajoittaista liikkumista, jotka myös huuhtelevat elektrolyytti-ja mahdollisesti lietteen tarttumiset karkeilta katodipin-35 noilta suihkunomaisesti. Pesuvaiheen äänikäsittely kestää 2 minuuttiin asti. Pesusammiosta poistamisen jälkeen haih- 2 67410 tuu tarttunut kuuma pesuvesi. Joidenkin minuuttien kuluttua on katodi kuiva ja käyttökelpoinen.
Kaikki elektrolyyteille tarttuvat seuraavassa sula-tusvaiheessa lasketut epäpuhtaudet voidaan poistaa lähes 5 jäljettömiin, jolloin rikin vähentyminen erityisesti korostuu. Vesiliukoinen jäämärikkipitoisuus katodilla alenee alle 1 ppm.
Piirroksen mukaan kuvataan pesulaite katodien puhdistamiseksi .
10 Elektrolyyttikennoista nostolaitteen avulla otetut katodit 2 upotetaan pesusäiliöön 1, joka on täytetty kuumalla vedellä, josta kaasut on poistettu ja jota lisäksi voidaan kuumentaa kuumennusputken 7 kautta. Nosturin purkamiseksi voidaan katodit vaihtoehtoisesti siirtää kulje-15 tusketjujärjestelmän kautta pesusammion läpi. Säiliöön 1 on sijoitettu ultraääni-upposekoittimia 3. Sekoittimia sekoitetaan ultraäänigeneraattorin 4 avulla HF-kaapelin 6 kautta; generaattorin syöttö tapahtuu liitäntäkaapin 5 kautta. Puhdistusvaiheen läpi kulkeva vierailla aineilla 20 rikastunut pesuvesi juoksee jatkuvasti pois yläjuoksun 9 kautta ja korvautuu jatkuvasti puhtaalla vedellä, jota tulee johdosta 8. Säiliön jaksottainen puhdistaminen kiinto-ainekerrostumista voi tapahtua säiliön tyhjennysaukon 10 kautta.