ES8203973A1 - Procedimiento de afinado de un bano de metal en un crisol con insuflado de oxigeno por arriba y crisol para su reali- zacion - Google Patents
Procedimiento de afinado de un bano de metal en un crisol con insuflado de oxigeno por arriba y crisol para su reali- zacionInfo
- Publication number
- ES8203973A1 ES8203973A1 ES498382A ES498382A ES8203973A1 ES 8203973 A1 ES8203973 A1 ES 8203973A1 ES 498382 A ES498382 A ES 498382A ES 498382 A ES498382 A ES 498382A ES 8203973 A1 ES8203973 A1 ES 8203973A1
- Authority
- ES
- Spain
- Prior art keywords
- crucible
- refining
- molten metal
- injectors
- metal bath
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
PROCEDIMIENTO DE AFINADO DE METAL Y CRISOL PARA SU REALIZACION. EL PROCEDIMIENTO CONSISTE EN INYECTAR POR EL PIE DEL CRISOL UN GAS DE AGITACION EN LAS PROXIMIDADES DE LA PARED LATERAL, EN LAS PROXIMIDADES DE LA VERTICAL DEL PIE DE BASCULADO DEL CRISOL; DURANTE EL AFINADO SE DETERMINAN LOS PARAMETROS INDICATIVOS DE LA TENDENCIA A LA NITRURACION DEL BAÑO. EL CRISOL PRESENTA INCORPORADOS A SU REVERTIMIENTO INYECCIONES PARA LA INSUFLACION DEL GAS DE AGITACION, LOCALIZADOS EN EL FONDO DEL CRISOL EL MENOS, SEGUN UNA CORONA PERIFERICA SITUADA EN LAS PROXIMIDADES INMEDIATAS A LA PARED REFRACTARIA LATERAL DEL CRISOL.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
LU82069A LU82069A1 (fr) | 1980-01-09 | 1980-01-09 | Procede d'affinage d'un bain de metal |
Publications (2)
Publication Number | Publication Date |
---|---|
ES8203973A1 true ES8203973A1 (es) | 1982-04-01 |
ES498382A0 ES498382A0 (es) | 1982-04-01 |
Family
ID=19729324
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES498382A Granted ES498382A0 (es) | 1980-01-09 | 1981-01-08 | Procedimiento de afinado de un bano de metal en un crisol con insuflado de oxigeno por arriba y crisol para su reali- zacion |
Country Status (17)
Country | Link |
---|---|
US (1) | US4369060A (es) |
EP (1) | EP0032350B1 (es) |
JP (1) | JPS56102508A (es) |
AT (1) | ATE14144T1 (es) |
AU (1) | AU540800B2 (es) |
BR (1) | BR8100113A (es) |
CA (1) | CA1172048A (es) |
CS (1) | CS242866B2 (es) |
DE (1) | DE3070844D1 (es) |
ES (1) | ES498382A0 (es) |
IN (1) | IN154540B (es) |
LU (1) | LU82069A1 (es) |
PL (1) | PL229121A1 (es) |
PT (1) | PT72324B (es) |
RO (1) | RO81955A (es) |
SU (1) | SU1190993A3 (es) |
ZA (1) | ZA8177B (es) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2501722B1 (fr) * | 1981-03-11 | 1986-08-14 | Siderurgie Fse Inst Rech | Procede de brassage pneumatique d'un bain metallique |
US4488903A (en) * | 1984-03-14 | 1984-12-18 | Union Carbide Corporation | Rapid decarburization steelmaking process |
AT382889B (de) * | 1984-03-15 | 1987-04-27 | Voest Alpine Ag | Spueleinrichtung fuer ein metallurgisches gefaess |
US4529442A (en) * | 1984-04-26 | 1985-07-16 | Allegheny Ludlum Steel Corporation | Method for producing steel in a top oxygen blown vessel |
US4599107A (en) * | 1985-05-20 | 1986-07-08 | Union Carbide Corporation | Method for controlling secondary top-blown oxygen in subsurface pneumatic steel refining |
AT384034B (de) * | 1986-02-03 | 1987-09-25 | Voest Alpine Ag | Spueleinrichtung fuer ein metallurgisches gefaess |
FR2632971B1 (fr) * | 1988-06-17 | 1993-09-03 | Vallourec | Procede de traitement des aciers liquides par injection de gaz a travers le fond de poche |
LU92813B1 (en) * | 2015-09-02 | 2017-03-20 | Wurth Paul Sa | Enhanced pressurising of bulk material in lock hoppers |
Family Cites Families (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR1210459A (fr) * | 1957-12-02 | 1960-03-09 | A R B E D | Procédé de fabrication d'acier et convertisseur pour ce procédé ou procédés similaires |
BE609232A (fr) * | 1961-10-16 | 1962-04-16 | Centre Nat Rech Metall | Perfectionnements aux procédés d'affinage de la fonte |
US3854932A (en) * | 1973-06-18 | 1974-12-17 | Allegheny Ludlum Ind Inc | Process for production of stainless steel |
FR2322202A1 (fr) * | 1975-08-29 | 1977-03-25 | Siderurgie Fse Inst Rech | Procede d'elaboration d'acier par soufflage d'oxygene |
US4198230A (en) * | 1977-05-04 | 1980-04-15 | Eisenwerk-Gesellschaft Maximilianshutte Mbh | Steelmaking process |
US4195985A (en) * | 1977-12-10 | 1980-04-01 | Eisenwerk-Gesellschaft Maximilianshutte Mbh. | Method of improvement of the heat-balance in the refining of steel |
US4280838A (en) * | 1979-05-24 | 1981-07-28 | Sumitomo Metal Industries, Ltd. | Production of carbon steel and low-alloy steel with bottom blowing basic oxygen furnace |
-
1980
- 1980-01-09 LU LU82069A patent/LU82069A1/fr unknown
- 1980-12-31 AT AT80401900T patent/ATE14144T1/de not_active IP Right Cessation
- 1980-12-31 DE DE8080401900T patent/DE3070844D1/de not_active Expired
- 1980-12-31 EP EP80401900A patent/EP0032350B1/fr not_active Expired
-
1981
- 1981-01-02 US US06/222,512 patent/US4369060A/en not_active Expired - Fee Related
- 1981-01-06 ZA ZA00810077A patent/ZA8177B/xx unknown
- 1981-01-07 AU AU66046/81A patent/AU540800B2/en not_active Ceased
- 1981-01-08 BR BR8100113A patent/BR8100113A/pt unknown
- 1981-01-08 RO RO81103090A patent/RO81955A/ro unknown
- 1981-01-08 ES ES498382A patent/ES498382A0/es active Granted
- 1981-01-08 CA CA000368097A patent/CA1172048A/fr not_active Expired
- 1981-01-08 PL PL22912181A patent/PL229121A1/xx unknown
- 1981-01-08 SU SU813229952A patent/SU1190993A3/ru active
- 1981-01-08 PT PT72324A patent/PT72324B/pt unknown
- 1981-01-08 JP JP81381A patent/JPS56102508A/ja active Pending
- 1981-01-09 IN IN22/CAL/81A patent/IN154540B/en unknown
- 1981-01-28 CS CS81163A patent/CS242866B2/cs unknown
Also Published As
Publication number | Publication date |
---|---|
LU82069A1 (fr) | 1981-09-10 |
PT72324A (en) | 1981-02-01 |
PL229121A1 (es) | 1981-09-18 |
CS242866B2 (en) | 1986-05-15 |
AU6604681A (en) | 1981-07-16 |
EP0032350A3 (en) | 1981-08-26 |
ES498382A0 (es) | 1982-04-01 |
JPS56102508A (en) | 1981-08-17 |
PT72324B (en) | 1981-12-18 |
RO81955B (ro) | 1983-06-30 |
ZA8177B (en) | 1982-01-27 |
SU1190993A3 (ru) | 1985-11-07 |
BR8100113A (pt) | 1981-07-21 |
EP0032350B1 (fr) | 1985-07-03 |
CA1172048A (fr) | 1984-08-07 |
ATE14144T1 (de) | 1985-07-15 |
IN154540B (es) | 1984-11-10 |
AU540800B2 (en) | 1984-12-06 |
EP0032350A2 (fr) | 1981-07-22 |
US4369060A (en) | 1983-01-18 |
DE3070844D1 (en) | 1985-08-08 |
RO81955A (ro) | 1983-07-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4518422B1 (en) | Process and apparatus for refining steel in a metallurgical vessel | |
ES8203973A1 (es) | Procedimiento de afinado de un bano de metal en un crisol con insuflado de oxigeno por arriba y crisol para su reali- zacion | |
GB1207003A (en) | Apparatus and method for continuous refining of molten metals | |
FR2501722B1 (fr) | Procede de brassage pneumatique d'un bain metallique | |
EP0160376A3 (en) | Method for producing steel in a top oxygen blown vessel | |
EG16915A (en) | Process for the removal of contaminating elements from pig-iron steel other meter metals and metal alloys | |
ES8100349A1 (es) | Un metodo para aumentar la duracion del revestimiento refractario de un recipiente revestido con material refractario basico | |
JPS5739113A (en) | Steel-making process by converter | |
ES8402879A1 (es) | Procedimiento mejorado para aumentar la cantidad de refrigerante en la obtencion de acero mediante insuflado de oxigeno. | |
Sasaki et al. | A Newly Developed Hot Metal Treatment Has Changed the Idea of Mass Production of Pure Steel | |
JPS552759A (en) | Manufacture of ultra-low-carbon stainless steel | |
ES8705925A1 (es) | Un metodo para tratar acero fundido | |
JPS5378913A (en) | Refining method for steel for decreasing generating amount of slag | |
Karpenko | Decarburization in the blowing zone when refining an open-hearth bath by liquid and gaseous oxygen | |
JPS5623213A (en) | Melting method of low phosphorus steel in oxygen top blowing steel making method | |
Spenceley et al. | Metal Refining Processes | |
JPS6447805A (en) | Production of silicon-containing cast iron | |
Bauvois | Process for decarburizing steel in an enclosed vacuum chamber and an enclosed vacuum chamber for this process | |
Spenceley et al. | Improvements in or Relating to a Process for Melting and/or Refining Steel | |
JPS5684411A (en) | Steel making using pure oxygen top and bottom blown converter | |
JPS57161018A (en) | Refining method for molten iron | |
Simaro et al. | Development and Installation of New Equipment and Processes in the New EAF Shop at Acindar Plant No. 2 | |
Babenko | Efficiency of technology for processing the pig iron containing 0. 3-0. 6% of phosphorus in basic oxygen furnace | |
JPS6473012A (en) | Refining method by using top and bottom blowing refining furnace | |
Nakashima et al. | Process for Refining Molten Steel |