DE99678C - - Google Patents
Info
- Publication number
- DE99678C DE99678C DENDAT99678D DE99678DC DE99678C DE 99678 C DE99678 C DE 99678C DE NDAT99678 D DENDAT99678 D DE NDAT99678D DE 99678D C DE99678D C DE 99678DC DE 99678 C DE99678 C DE 99678C
- Authority
- DE
- Germany
- Prior art keywords
- bell
- during
- pouring
- metal
- bells
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
KAISERLICHES
PATENTAMT.
Man hat bisher zersprungene Glocken in der Weise reparirt, dafs die Kanten der Risse mittelst
einer Legirung von höherem Schmelzpunkt als dem des Glockenmetalls in annähernd geschmolzenen Zustand gebracht werden, worauf
die Risse mit einer der Glockenbronze ähnlichen Legirung ausgefüllt werden. Dieses
Metall vereinigt sich dann vollständig mit dem Glockengut. Die Glocke ist während der
Arbeit mit Sand gefüllt, um die Erwärmung und Abkühlung gleichförmig zu erhalten.
Dieses Verfahren gelingt jedoch nicht immer, da die Glocken während der Abkühlung vielfach
wieder zerspringen.
Die vorliegende Erfindung bezieht sich nun auf ein Verfahren, welches diesem Uebelstande
abhelfen soll.. Es hat sich nämlich gezeigt, dafs die Gefahr des Zerspringens stets vorhanden
ist, wenn die Glocke gleichförmig erwärmt oder abgekühlt wird, und dafs dieser
Gefahr nur dadurch sicher vorgebeugt werden kann, dafs die Glocke zuerst nur an ihrer
dicksten Stelle, d. h. in der Höhe des Klöppelanschlags, und erst später ganz erwärmt wird.
Ebenso darf nach dem Eingiefsen des Metalls in den Sprung und während des ersten Stadiums
der Abkühlung nur der genannte Theil der Glocke erwärmt werden.
Die Reparatur der Glocke wird im Uebrigen unter Verwendung eines beliebigen Erwärmungsmittels
in der oben angegebenen Weise ausgeführt. Nachdem der Rifs sorgfältigst gereinigt
worden ist, werden die Kanten des Risses vor dem Anbringen der Formen mit
Borax oder einem anderen geeigneten Flufsmittel bestreut. Nach dem Eingiefsen des
Metalls und dem Herausnehmen der Formen wird nur der stärkste Theil der Glocke am
Rande einer Erwärmung ausgesetzt, welche man dann allmälig abnehmen und schliefslich
ganz aufhören läfst.
Die Erwärmung wird also während der Operation am genannten Theil concentrirt.
Claims (1)
- Patent-Anspruch:Verfahren zum Ausbessern gesprungener Glocken und dergl. mittelst Erwärmung der Kanten des Sprunges und Eingiefsen von geschmolzenem Metall, dadurch gekennzeichnet, dafs die Erwärmung der Glocke vor, während und nach dem Eingiefsen am stärksten Theil des Glockengutes in der Höhe des Klöppelanschlags stattfindet.