DE735234C - Process for finishing fresh wood veneers - Google Patents

Process for finishing fresh wood veneers

Info

Publication number
DE735234C
DE735234C DEJ68391D DEJ0068391D DE735234C DE 735234 C DE735234 C DE 735234C DE J68391 D DEJ68391 D DE J68391D DE J0068391 D DEJ0068391 D DE J0068391D DE 735234 C DE735234 C DE 735234C
Authority
DE
Germany
Prior art keywords
veneers
wood veneers
fresh wood
finishing
wood
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DEJ68391D
Other languages
German (de)
Inventor
Paul Jaeger
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to DEJ68391D priority Critical patent/DE735234C/en
Application granted granted Critical
Publication of DE735234C publication Critical patent/DE735234C/en
Expired legal-status Critical Current

Description

Verfahren zur Veredelung frischer Holzfurniere Durch das Patent 724 228 ist es bekanntgeworden, feuchte Furniere kalt nachzuwalzen, um das beschädigte Holzgefüge wieder in Ordnung zu bringen. Dabei lassen sich die Poren des Holzes nicht oder nur insoweit zusammenpressen, als sie nicht mit Wasser gefüllt sind. Die so vorbehandelten frischen Furniere müssen daher, um die Veredelung zu vollenden, in halbtrocken-- und trockenem Zustand wiederholt nachgewalzt werden, um den für das trockene Furnier gewünschten Grad von Dichtigkeit, Elastizität und Haltbarkeit zu erreichen.Process for the finishing of fresh wood veneers Through the patent 724 228 it has become known to re-roll damp veneers cold to remove the damaged Bringing the wood structure back in order. In doing so, the pores of the wood do not compress or only to the extent that they are not filled with water. The fresh veneers pretreated in this way must therefore, in order to complete the finishing, be re-rolled repeatedly in a semi-dry and dry state in order to achieve the the dry veneer desired degree of tightness, elasticity and durability to reach.

Da es nun einerseits bei frischen Furnieren wegen des Wassergehalts unmöglich ist, sie in gleicher Weise zu veredeln wie die trockenen Furniere, andererseits aber auch die lufttrockenen Furniere oft noch einen zu hohen Grad von Feuchtigkeit besitzen, so kann es vorkommen, daß sich auch bei letzteren erst nach dem Walzen herausstellt, daß infolge noch zu hohen Wassergehalts des Furniers ein voll zufriedenstellendes Ergebnis nicht erreicht werden konnte, das Furnier vielmehr durch weitere Abgabe von Feuchtigkeit an der Luft sich noch mehr oder weniger wirft oder verzieht.Since it is now on the one hand with fresh veneers because of the water content it is impossible to refine them in the same way as the dry veneers, on the other hand but also the air-dry veneers often still have too high a degree of moisture own, it can happen that even with the latter only after rolling it turns out that, as the water content of the veneer is still too high, a completely satisfactory one Result could not be achieved, the veneer rather through further delivery moisture in the air is more or less thrown or warped.

Um nun sicher züx sein, daß die den Walzprozeß durchmachenden Furniere auch einen genügenden und richtigen Trockengrad erhalten, ohne daß eine Nachprüfung im einzelnen notwendig wäre, kann man diesem Übelstand dadurch abhelfen, daß mindestens eine der beiden Walzen, zwischen welchen das feuchte Furnier hindurchgeführt wird, so stark erhitzt wird, daß die im -Holz noch enthaltene überschüssige Feuchtigkeitsmenge durch Verdampfen entfernt wird, wobei aber gleichzeitig durch den ausgeübten Walzendruck das -Holz am Schwinden verhindert und darüber hinaus vielleicht noch etwas mehr gedehnt wird. Dieses Erwärmen bei gleichzeitig ausgeführtem starken Druck hat den Vorteil, daß auch feuchte Furniere, die direkt von der Messer- oder Schälmaschine kommen, gleich fertig veredelt und getrocknet, dabei aber vor dem Schwinden und Welligwerden bewahrt werden können, wenn man sie je nach Holzart und Stärke ein- oder mehrmals oder durch mehrereIiintereinander gelagerte heiße Druckwalzen laufen iäßt.Now to be sure that the veneers going through the rolling process also get a sufficient and correct degree of dryness without a check would be necessary in detail, one can remedy this problem by at least one of the two rollers between which the damp veneer is passed, is heated so much that the excess amount of moisture still contained in the wood is removed by evaporation, but at the same time by the exerted roller pressure the wood prevents it from shrinking and perhaps a little more is stretched. This heating with simultaneous strong pressure has the Advantage that also moist veneers, which are directly from the knife or peeling machine come, finished and dried right away, but before shrinking and Waviness can be preserved if you change them depending on the type of wood and Strength one or more times or through several hot pressure rollers mounted one behind the other runs.

Dabei ist es möglich, noch zu erreichen, daß dem Arbeitsgut dadurch eine besondere Form ,gegeben wird, daß nur eine heiße Walze beim letzten Durchgang Verwendung findet, wodurch das Furnier selbsttätig nach der der heißen Walze zugekehrten Seite etwas hohl wird bzw. nach der kalten Walze zu sich wölbt. Dieser Effekt ist für manche Zwecke, z. B. Schuhbedarf, erwünscht.It is still possible to achieve that the work item thereby a special shape, given that only a hot roller on the last pass Is used, whereby the veneer automatically after facing the hot roller Page becomes a little hollow or bulges after the cold roller. This effect is for some purposes, e.g. B. Shoe supplies, desired.

Claims (2)

PATENTANSPRÜCHE: i. Verfahren zur Veredelung frischer Holzfurniere nach Patent 724 228, dadurch gekennzeichnet, daß die noch feuchten Furniere durch heiße Walzen getrocknet und gleichzeitig unter Beseitigung möglichst aller Zellenhohlräume verdichtet werden. PATENT CLAIMS: i. Process for finishing fresh wood veneers according to patent 724 228, characterized in that the still moist veneers through hot rollers dried and at the same time removing as many cell cavities as possible be condensed. 2. Anwendungsform des Verfahrens, gekennzeichnet dadurch, daß infolge der Erhitzung von nur einer Walze das Arbeitsgut beim Durchlaufen nach einer Seite gewölbt wird.2. Application of the method, characterized in that As a result of the heating of only one roller, the work material when passing through after one Side is arched.
DEJ68391D 1940-12-06 1940-12-06 Process for finishing fresh wood veneers Expired DE735234C (en)