DE320621C - Process for making leather waterproof and non-slip - Google Patents
Process for making leather waterproof and non-slipInfo
- Publication number
- DE320621C DE320621C DE1913320621D DE320621DD DE320621C DE 320621 C DE320621 C DE 320621C DE 1913320621 D DE1913320621 D DE 1913320621D DE 320621D D DE320621D D DE 320621DD DE 320621 C DE320621 C DE 320621C
- Authority
- DE
- Germany
- Prior art keywords
- leather
- solution
- resin
- celluloid
- slip
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zum Wasserdicht- und Nichtschlüpfrigmachen von Leder. Die Erfindung betrifft ein -Verfahren zur Behandlung von Leder mit Gummi und bezweckt hanptsächlich, die Widerstandsfähigkeit des Leders gegen Feuchtigkeit zu erhöhen sowie ferner das Gleiten des Leders auf feuchten oder fettigen Oberflächen zu verhindern.Method of waterproofing and non-slippery leather. the The invention relates to a method for treating leather with rubber and aims mainly to increase the leather's resistance to moisture and also to prevent the leather from sliding on damp or greasy surfaces.
Es wurde bereits vorgeschlagen, einen wasserdichten Überzug aus Leder mit Hilfe von in Azeton und Amylazetat gelöstem Zelluloid herzustellen, wobei die Haut nach der Behandlung in einem Bad von Alkohol und weißem Schellack weiter behandelt wird.A waterproof cover made of leather has already been proposed with the help of celluloid dissolved in acetone and amyl acetate, whereby the Skin treated further after treatment in a bath of alcohol and white shellac will.
Es wurde weiter vorgeschlagen, das Leder nach der obigen Behandlung mit einer Lösung von Schwefelkohlenstoff und Kautschuk unter Zusatz von Steinkohlenteeröl und Leinöl zu behandeln.It was further suggested that the leather after the above treatment with a solution of carbon disulfide and rubber with the addition of coal tar oil and linseed oil to treat.
Im Gegensatz hierzu wird durch die Erfindung eine Tränkung des Leders dadurch bewirkt, daß es mit Kautsckuklösungen wachsender Stärke und schließlich mit einer Kautschuklösung unter Zusatz von Zelluloid- und Harzlösungen behandelt wird, wodurch nicht nur das Leder haltbarer und wasserdicht wird, sondern auch eine größere Haftfähigkeit erhält; diese Eigenschaften verb=eiben dem Leder dauernd bis zur völligen Abnutzung.In contrast, the invention impregnates the leather thereby causing it to grow strength and eventually with chewy solutions treated with a rubber solution with the addition of celluloid and resin solutions which not only makes the leather more durable and waterproof, but also a gets greater adhesiveness; these properties persist in the leather until to complete wear and tear.
Benutzt man beispielsweise das bekannte Verfahren, das Leder in einer Trommel mit einer Kautschuklösung zu behandeln, so wird gemäß der Erfindung dieser Kautschuklösung eine Lösung von Zelluloid in Azeton oder anderein geeigneten Lösungsmittel zugesetzt. Dieser Zusatz wird zweckmäßig dann gemacht, nachdem die Trommelbehandlung einige Zeit in Wirkung gewesen ist. Dieser Zusatz soll die -Widerstandsfähigkeit des Leders gegen Wässer und Feuchtigkeit erhöhen. Um ferner das Leder nicht schlüpfrig zu machen, wenn es auf feuchten oder fettigen Oberflächen benutzt wird, werden der Kautschuklösung Wachholderharz, Äther, Bernstein und Benzol zugesetzt.For example, if the known method is used, the leather in one Treating the drum with a rubber cement, according to the invention, this Rubber cement a solution of celluloid in acetone or other suitable solvent added. This addition is conveniently made after the tumbling treatment has been in effect for some time. This addition is said to increase the resilience of the leather against water and moisture. Furthermore, the leather is not slippery if it is used on damp or greasy surfaces, the Juniper resin, ether, amber and benzene are added to the rubber solution.
Es wurde gefunden, daß Benzol bester Beschaffenheit die wirksamste Lösung gibt; da dieses jedoch verhältnismäßig kostspielig ist, so kann aus wirtschaftlichen Rücksichten eine gewisse Menge eines billigeren Lösungsmittels, beispielsweise geringeres Benzol oder Naphtha, benutzt werden. Die Mengenverhältnisse des Lösungsmittels können je nach den Umständen geändert werden.It has been found that the best quality benzene is the most effective Solution there; However, since this is relatively expensive, it can be economical Consider a certain amount of a cheaper solvent, for example less Benzene or naphtha. The proportions of the solvent can be changed depending on the circumstances.
Gute Ergebnisse werden erzielt, wenn bei dem bekannten Trommelverfahren am Ende der Behandlung das Zelluloid und die anderen Stoffe zugesetzt werden. Beispielsweise wird bei der Behandlung von =5 bis 2o Häuten von Durchschnittsgewicht eine Lösung von Zelluloid in Azeton zugesetzt, nachdem die Behandlung eine Zeitlang fortgeschritten ist. Hierauf wird in geeigneten Zwischenräumen in Methyläther gelöstes Wachholderharz, in Benzol gelöstes Bernsteinharz und etwa eine gleiche Menge von Naphtha oder geringerem Benzol zugesetzt. Die bei, der Trommelbehandlung benutzte Gummilösung ist gebildet aus 214 kg feinem, hartem Paragummi, der in 22,71 Naphtha und 37,81 Benzin gelöst istk Die Menge dieser Stoffe hängt ab von der-Beschaffenheit des Gummis ttntl Mt-y@eiti4ffeiheit und dem Gewicht der Häute. Die obigen Mengenverhältnisse sind angegeben für Durchschnittsqualitäten und Gewichte.Good results are achieved when using the known drum method at the end of the treatment the celluloid and the other substances are added. For example becomes a solution when treating = 5 to 20 skins of average weight of celluloid in acetone added after the treatment progressed for a while is. Juniper resin dissolved in methyl ether is then added in suitable spaces. Amber resin dissolved in benzene and about an equal amount of naphtha or less Benzene added. The rubber solution used for drum treatment is made of 214 kg of fine, hard para rubber, which is in 22.71 naphtha and 37.81 Gasoline is dissolved. The amount of these substances depends on the nature of the rubber ttntl Mt-y @ eiti4ffeiheit and the weight of the skins. The above proportions are given for average qualities and weights.
Die Zelluloidlösung, von weicher 5,7 1 gebraucht werden, wird zusammengesetzt aus Zelluloid in Azeton in einem Verhältnis von 255,2 g Zelluloid und etwa 4,25 1 Lösungsmittel.The celluloid solution, of which 5.7 liters are needed, is made up of celluloid in acetone in a ratio of 255.2 grams of celluloid and about 4.25 1 solvent.
Die Lösung von Bernsteinharz, von welcher etwa 2,8 1 gebraucht werden, wird zusammengesetzt aus 1,35 kg Bernsteinharz in 1,7 kg Benzin und =,7 kg Naphtha. Es werden ferner o,7 1 Wachholderharzlösung gebraucht, die aus 513 g Harz in 85o g Äther zusammengesetzt ist.The solution of amber resin, of which about 2.8 1 are needed, is composed of 1.35 kg of amber resin in 1.7 kg of gasoline and = .7 kg of naphtha. Furthermore, 0.7 1 juniper resin solution is needed, which is made from 513 g resin in 85o g ether is composed.
Das Verfahren vollzieht sich so, daß bei der Endbehandlung in der Trommel die Zelluloidlösung nach einer zwei- bis dreistündigen Behandlung zugesetzt wird. Nach einer weiteren Behandlung von 112 bis 2 Stunden wird die Bernsteinharzlösung allmählich zugesetzt, und sodann nach einem weiteren Zeitraum von 2 bis 3 Stunden setzt man die Lösung von Wachholderharz allmählich zu.The process is carried out in such a way that the final treatment in the Drum the celluloid solution added after two to three hours of treatment will. After another treatment for 112 to 2 hours, the amber resin solution becomes added gradually, and then after an additional period of 2 to 3 hours the solution of juniper resin is added gradually.
Die angegebenen Lösungsmittel können gegen andere gleichwertige vertauscht werden.The specified solvents can be exchanged for other equivalent solvents will.
Das angegebene Verfahren erhöht die Wasser- und Feuchtigkeitsbeständigkeit des Leders ganz erheblich. Außerdem faßt ein solches Leder besser auf feuchten und fettigen Oberflächen. Wenn andere Häute, wie beispielsweise Kalb-, Ziegen- oder Schafhäute o. dgl., behandelt werden, so ändern sich entsprechend die angegebenen Verhältnisse.The specified procedure increases the water and moisture resistance of the leather quite considerably. In addition, such a leather holds better on damp and greasy surfaces. If other hides, such as veal, goat or Sheep skins or the like are treated, the specified change accordingly Conditions.
Claims (1)