DE199719C - - Google Patents
Info
- Publication number
- DE199719C DE199719C DENDAT199719D DE199719DA DE199719C DE 199719 C DE199719 C DE 199719C DE NDAT199719 D DENDAT199719 D DE NDAT199719D DE 199719D A DE199719D A DE 199719DA DE 199719 C DE199719 C DE 199719C
- Authority
- DE
- Germany
- Prior art keywords
- necks
- heads
- electric current
- sagging
- lost
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
BERLIN. GEDRUCKT IN DER REICHSORUCKEREI.
Claims (2)
1. Verfahren zur Entfernung der verlorenen Köpfe bei Herstellung von Stahlgußstücken,
dadurch gekennzeichnet, daß die Hälse der verlorenen Köpfe mit Hilfe eines elektrischen Stromes, der durch
erstere geleitet wird, bis zur Vollendung des Nachsackens oder noch einige Zeit nachher in geschmolzenem Znstande erhalten
und alsdann die Köpfe von dem Gußstück abgetrennt werden, bevor die
Hälse erstarrt sind. ■
2. Verfahren nach Anspruch 1, dadurch gekennzeichnet, daß der Querschnitt der
Hälse so weit verringert wird, daß ohne Anwendung des elektrischen Stromes ein ordentliches Nachsacken nicht stattfinden
könnte, und daß die Köpfe vor oder nach der Erstarrung der Hälse abgetrennt
werden.