DE118776C - - Google Patents

Info

Publication number
DE118776C
DE118776C DENDAT118776D DE118776DA DE118776C DE 118776 C DE118776 C DE 118776C DE NDAT118776 D DENDAT118776 D DE NDAT118776D DE 118776D A DE118776D A DE 118776DA DE 118776 C DE118776 C DE 118776C
Authority
DE
Germany
Prior art keywords
hat
stump
finish
machine
cylinder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
DENDAT118776D
Other languages
German (de)
Publication of DE118776C publication Critical patent/DE118776C/de
Active legal-status Critical Current

Description

KAISERLICHESIMPERIAL

PATENTAMT.PATENT OFFICE.

Die vorliegende Maschine hat den Zweck, eine bisher meist sehr fehlerhaft mit der Hand ausgeführte Arbeit durch eine selbstthätige Vorrichtung auszuführen, die die Arbeit weit vollkommener und regelmäfsiger leistet und dabei eine viel gröfsere Leistungsfähigkeit besitzt.The purpose of the present machine is to fix a so far mostly very flawed by hand to carry out work carried out by an automatic device which extends the work far performs more perfectly and regularly and at the same time has a much greater efficiency.

Auf beiliegender Zeichnung ist eine Maschine der neuen Art dargestellt.The enclosed drawing shows a new type of machine.

Fig. ι ist eine Vorderansicht,Fig. Ι is a front view,

Fig. 2 ein Schnitt in Richtung der Linie A-B nach Fig. 1, undFig. 2 is a section in the direction of the line AB of Fig. 1, and

Fig. 3 zeigt einen Hutstumpen.Fig. 3 shows a hat stump.

Die Maschine besteht im Wesentlichen aus zwei Kautschukwalzen A und B, welche über einander in einem Gestell gelagert sind. Die Achsen α und b der Walzen sind aus Eisen hergestellt und in Lagerklötzen C gelagert, die in den Ständern D mit geringer Reibung gleiten können.The machine essentially consists of two rubber rollers A and B, which are mounted one above the other in a frame. The axes α and b of the rollers are made of iron and mounted in bearing blocks C, which can slide in the uprights D with little friction.

Die Oberwalze B wird gegen die untere A mit Hülfe von auf den Hebeln F verstellbaren Gewichten E mehr oder weniger stark geprefst. Auf diese Weise ist es ermöglicht, den oberen Cylinder mit einer genau bestimmbaren Kraft gegen den unteren bezw. auf den zwischen beiden Walzen geführten Hutstumpen zu pressen.The upper roller B is pressed more or less strongly against the lower A with the aid of weights E adjustable on the levers F. In this way, it is possible to bezw the upper cylinder with a precisely determinable force against the lower. to press on the hat stump guided between the two rollers.

Die untere Walze A taucht bis zu ihrer Achse in einen Behälter G ein, welcher die Appretur oder das Ueberzugmaterial aufnimmt; da diese Appretur bei gewöhnlicher Temperatur hart ist, so mufs man sie erhitzen. Hierzu ist der Behälter G mit einer Umhüllung H versehen ; der Raum zwischen Behälter und Hülle wird mit Wasser angefüllt, welches durch einen Gasbrenner / oder auf sonstige Weise erhitzt wird.The lower roller A is immersed up to its axis in a container G, which receives the finish or the coating material; as this finish is hard at ordinary temperature, it must be heated. For this purpose, the container G is provided with an envelope H ; the space between the container and the shell is filled with water, which is heated by a gas burner or in some other way.

Die Appreturflüssigkeit befindet sich in einem über der Maschine angeordneten gröfseren Behälter, welcher gleichfalls erhitzt wird und von welchem dieselbe, wie Fig. 1 angiebt, durch ein Rohr J in dem Mafse des stattfindenden Verbrauches zugeleitet wird. Der Cylinder A wird durch eine Handkurbel oder auch durch Maschinenkraft in Umdrehung versetzt.The finishing liquid is in a larger container arranged above the machine, which is also heated and from which, as FIG. 1 indicates, it is fed through a pipe J in proportion to the consumption that takes place. The cylinder A is set in rotation by a hand crank or by machine power.

Wenn ein Hutstumpen ganz und gar appretirt werden soll, so läfst man ihn auf beiden Seiten durch beide Cylinder hindurchgehen. Der untere Cylinder nimmt aus dem Behälter die Appretur heraus und imprägnirt den Hutstumpen. Es ist aus diesem Grunde nothwendig, dafs der auf den Cylinder B ausgeübte Druck genau regulirbar ist, denn man mufs im Auge behalten, dafs die Appretur nicht den Filz oder das Gewebe des Stumpens ganz durchdringt, weil sonst auf der Innenseite des Hutes Flecke entstehen würden, welche den Hut unbrauchbar machen.If a hat stump is to be completely finished, it is allowed to pass through both cylinders on both sides. The lower cylinder takes the finish out of the container and impregnates the hat stump. For this reason it is necessary that the pressure exerted on the cylinder B can be precisely regulated, for one must keep in mind that the finish does not penetrate the felt or the fabric of the stump completely, because otherwise stains would appear on the inside of the hat which make the hat unusable.

Es ist darum ein sehr grofser Vortheil vorliegender Maschine, dafs das Imprägniren vollständig gleichmäfsig geschieht, ohne dafs ein stellenweises Durchdringen der Appreturmasse nach der Innenseite stattfinden könnte. Ferner ist aber die vorliegende Maschine dann noch von besonderem Vortheil gegen die Handarbeit, wenn es sich darum handelt, Hutstumpen zu appretiren, die später zur Herstellung von theilweise harten und theilweise weichen Hüten verwendet werden.It is therefore a very great advantage of the present machine that the impregnation is complete occurs evenly without penetrating the finishing compound in places could take place on the inside. But then the present machine is still further of particular advantage over handicraft when it comes to hat stumps to finish, which will later be used to produce partly hard and partly soft hats are used.

Wenn es sich beispielsweise darum handelt, einen Stumpen zu appretiren, bei welchem der Theil α (Fig. 3) weich und nur der mit b be
zeichnete Theil hart, d. h. mit Appretur über-
If, for example, it is a question of finishing a stump in which the part α (Fig. 3) is soft and only the part with b be
The part drew hard, that is, covered with finish

zogen werden soll, so dreht man die Walze a nur um einen bestimmten Betrag. Da der obere Theil der Walze noch nicht mit Schlichte überzogen ist, so legt man den Stumpen so ein, dafs der Theil α zuerst zwischen die Walzen geschoben wird. Man wird natürlich vorher auf dem Cylinder ein Zeichen anbringen, so dafs man den Cylinder A genau wieder in seine Anfangsstellung zurückdrehen kann, und dafs der nothwendige Theil des Cylinders A beständig in der Appreturmasse verbleibt, ein anderer jedoch niemals mit dieser in Berührung kommt.is to be pulled, the roller a is only rotated by a certain amount. Since the upper part of the roller has not yet been coated with size, the stump is placed in such a way that the part α is first pushed between the rollers. A mark will of course be made beforehand on the cylinder so that cylinder A can be turned exactly back into its starting position, and that the necessary part of cylinder A remains permanently in the finishing compound, but another never comes into contact with it.

Der Hutstumpen wurde deshalb gewöhnlich überhaupt nicht mit Steife getränkt, weil es bisher noch keine mechanischen Mittel zur Ausführung dieser Operation gab, und die Handarbeit nur sehr ungleichmäfsige und daher sehr unvollkommene Resultate lieferte. Die Steifigkeit, welche der Stumpen durch die vorliegende Behandlung mit Appretur erhalten, verliert sich bei der weiteren Behandlung sehr leicht dadurch wieder, dafs der zur Aufquellung des Filzes vor dem Aufziehen der Stumpen auf die Form verwendete Dampf eine gewisse vorübergehende Aufweichung der Steife zur Folge hat.The hat stump was usually not soaked in stiffness at all because of it so far there was no mechanical means of performing this operation, and manual labor only gave very irregular and therefore very imperfect results. The stiffness, which of the stumps received by the present treatment with finishing is lost in the further treatment, again very easily, by the fact that the swelling of the felt some temporary steam used before drawing the stump onto the mold Causes the stiffness to soften.

Da man es durch vorliegende Erfindung in der Hand hat, die Tiefe des Eindringens der Steife nach Belieben zu regeln, so erhält man unter allen Umständen einen in Bezug auf die Steifigkeit und Feinheit vollkommenen Hutstumpen. Since one has it in hand by the present invention, the depth of penetration of the To regulate stiffness at will, one gets one in relation to the under all circumstances Rigidity and delicacy perfect hat stumps.

Claims (1)

Patent-Anspruch:Patent claim: Eine Maschine zum Imprägniren von Hutstumpen, gekennzeichnet durch zwei gegen einander mehr oder weniger stark durch Federn oder Gegengewichte geprefste Kautschukwalzen, von welchen die untere in einen mittelst Wasserbad geheizten und die Appretur aufnehmenden Behälter eintaucht.A machine for the impregnation of hat stumps, characterized by two against Rubber rollers pressed together to a greater or lesser extent by springs or counterweights, of which the lower one is heated in a water bath and receives the finish Immerses the container. Hierzu ι Blatt Zeichnungen.For this purpose ι sheet of drawings.
DENDAT118776D Active DE118776C (en)