CN2322716Y - 等强度钢筋整形滚轧螺纹连接接头 - Google Patents
等强度钢筋整形滚轧螺纹连接接头 Download PDFInfo
- Publication number
- CN2322716Y CN2322716Y CN 98202776 CN98202776U CN2322716Y CN 2322716 Y CN2322716 Y CN 2322716Y CN 98202776 CN98202776 CN 98202776 CN 98202776 U CN98202776 U CN 98202776U CN 2322716 Y CN2322716 Y CN 2322716Y
- Authority
- CN
- China
- Prior art keywords
- reinforcing bar
- thread
- sleeve
- joint
- shaping
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种等强度钢筋整形滚轧螺纹连接接头,由接头钢筋、套筒组成,其特征是:经挤压整形消除表面纵横肋后的接头钢筋滚轧有螺纹,圆柱形套筒从两端向内加工螺纹,套筒中部螺纹相汇处为不同螺距的交界点,在套筒的两端设置有螺纹导向角。该钢筋连接接头采用无切削滚轧加工,既保证钢筋连接部分螺纹的强度,又使连接套筒体积、重量相比其它螺纹连接套筒大大减小,而且施工制作中不产生大量废屑,便于现场施工制作。
Description
本实用新型属于建筑结构构件,涉及一种钢筋螺纹连接接头。
钢筋机械连接的方法主要有:钢筋锥螺纹连接技术,即先将两根被连接钢筋端头加工出锥螺纹,然后将其插入有相应锥螺纹套筒的两端,通过旋转螺纹套筒将两根被连接的钢筋连接起来,构成螺纹套筒连接接头。这种接头现场拼接简单,速度快。但由于在被连接的钢筋母材上车制螺纹,削弱了钢筋截面,使接头的承载力低于钢筋实际的承载能力,从而使被连接钢筋不能发挥其强度,另有钢筋冷挤压连接技术,它是将两根被连接钢筋插入钢制套筒内,用径向挤压力将钢制套筒挤压变形,使钢筋与套筒握裹在一起,从而达到钢筋连接的作用。此种方法虽然在连接过程中,对钢筋母材没有损伤,接头可以充分发挥钢筋的强度,但也存在着钢筋密集处,连接机械放不进去而不能工作,以及需要较多的工作人员和携带较大的超高压液压设备在现场进行现场操作等不利因素,且连接套筒体积大,材料价格高,因而这种接头的应用范围受到了限制。
本实用新型的目的是,提供一种新型的等强度整形滚轧直螺纹钢筋连接套筒,其对现有的螺纹套筒连接接头进行改进,采用无切削滚轧加工,既保证钢筋连接部分螺纹的强度,又使连接套筒体积、重量相比其它螺纹连接套筒大大减小,而且施工制作中不产生大量废屑,便于现场施工制作。
本实用新型的等强度钢筋整形滚轧螺纹连接接头,由接头钢筋、套筒组成,其特征是:经挤压整形后的接头钢筋的端部滚轧有强化的螺纹,圆柱形套筒从两端向内加工螺纹,套筒中部螺纹相汇处为不同螺距的交界点;
所述的接头钢筋端部强化的螺纹为直螺纹或锥螺纹,直螺纹的公称直径M16-M42毫米,钢筋整形长度及螺纹加工长度为0.8-1.5倍的原钢筋直径,滚轧螺距为2.0-4.0毫米;锥螺纹的锥度为0.5°-8°,钢筋整形长度及螺纹加工长度为0.5-1.5倍的原钢筋直径;
所述的连接套筒长度为单根被连接钢筋的螺纹长度的1.8-2.2倍,套筒内螺纹为直螺纹或锥螺纹,螺纹旋向为两端右旋螺纹或分别为右、左旋螺纹;
在接头钢筋的原钢筋与直螺纹过渡处有倒向角;
在套筒两端设置有与接头钢筋相应的螺纹导向角。
本实用新型的等强度钢筋整形滚轧螺纹连接接头,其制造方法是,通过先挤压整形消除连接钢筋端头表面的纵横肋,再进行滚轧螺纹加工,对连接套筒加工出相应的内螺纹,在套筒中部螺纹相汇处为不同螺距的交界点,施工时,使用专用的扭力扳手,将套筒拧紧在钢筋连接部位,这样就可实现钢筋的连接。
等强度钢筋整形滚轧螺纹连接接头具有以下优点:
1、钢筋连接部分经过整形和螺纹滚轧加工,两次冷作强化,钢筋的连接表面纤维组织未被损坏,且组织更加紧密,内部晶粒进一步细化,使钢筋连接螺纹的连接强度大大提高,能满足或超过钢筋本身的承载能力,而且连接套筒体积很小,比普通锥螺纹连接套筒节省钢材40%以上,比冷挤压连接套筒节省钢材100%以上。
2、由于钢筋被连接部分经挤压整形强化后,钢筋此处的直径要比原直径减小,所以连接套筒的直径就可相应的减小,套筒径向突出钢材较少,这样接头既可满足或超过钢筋的承载能力,又可满足混凝土结构所规定的混凝土保护层最小厚度的要求。
3、现场施工方便快捷。
4、由于采用滚轧螺纹加工的方法,可以提高模具和刀具的寿命,降低制造成本。
5、套筒采用两端分别加工螺纹的加工方式,套筒中部螺纹交界处的螺距不同,这样可使连接钢筋接头插入套筒内的长度相同,保证钢筋连接的整体强度;在套筒两端分别设置有根据不同规格直径钢筋的螺纹导向角,以便于现场施工的螺纹连接和保护螺纹。
本实用新型的等强度钢筋整形滚轧螺纹连接接头经测试,性能达到《钢筋机械连接通用技术规程》JGJ101-96中钢筋接头性能的A级,套筒体积、重量相比其它螺纹连接的连接套筒大大减小,所以等强度钢筋整形滚轧螺纹连接接头具有连接精度好,强度高,套筒体积小,可降低原材料的损耗,降低成本,便于现场施工制作,适用于钢筋接头的连接。
以下结合附图及实施例,对等强度钢筋整形滚轧螺纹连接接头做进一步描述。
图1为等强度钢筋整形滚轧螺纹连接接头(直螺纹)结构示意图
图2为等强度钢筋整形滚轧螺纹连接接头(锥螺纹)结构示意图
图3为直螺纹钢筋接头通过整形挤压模具图
图4为锥螺纹钢筋接头通过整形挤压模具图
图5为经过整形挤压的直螺纹钢筋接头
图6为经过整形挤压的锥螺纹钢筋接头
如图可见,一种等强度钢筋整形滚轧螺纹连接接头,由接头钢筋、套筒组成,其特征是:经模具5挤压整形消除表面纵横肋后的接头钢筋1的端都滚轧有螺纹,圆柱形套筒2从两端向内加工螺纹,套筒中部螺纹相汇处为不同螺距交界点3,在接头钢筋原钢筋和直螺纹过渡处和套筒的两端设置有螺纹导向角4,所述的钢筋直径为22毫米,螺纹直径22.5毫米,螺距2.5毫米,套筒长度45毫米,套筒外径34毫米,螺纹中径20.88毫米,螺纹小径19.79毫米。
Claims (6)
1、一种等强度钢筋整形滚轧螺纹连接接头,由接头钢筋、套筒组成,其特征是:经挤压整形后的接头钢筋的端部滚轧有强化的螺纹,圆柱形套筒从两端向内加工螺纹,套筒中部螺纹相汇处为不同螺距的交界点。
2、如权利要求1所述的等强度钢筋整形滚轧螺纹连接接头,其特征是:所述的接头钢筋端部强化的螺纹为直螺纹,钢筋整形长度及螺纹长度为0.8-1.5倍的原钢筋直径。
3、如权利要求1所述的等强度钢筋整形滚轧螺纹连接接头,其特征是:所述的接头钢筋端部强化的螺纹为锥螺纹,锥螺纹锥度在0.5°-8°,钢筋整形长度及螺纹加工长度为0.5-1.5倍的原钢筋直径。
4、如权利要求1所述的等强度钢筋整形滚轧螺纹连接接头,其特征是:所述的连接套筒长度为单根被连接钢筋的螺纹长度的1.8-2.2倍,套筒内螺纹为直螺纹或锥螺纹,螺纹旋向为两端右旋螺纹或分别为右、左旋螺纹。
5、如权利要求1所述的等强度钢筋整形滚轧螺纹连接接头,其特征是:在所述的接头钢筋原钢筋与直螺纹过渡处有倒向角。
6、如权利要求1所述的等强度钢筋整形滚轧螺纹连接接头,其特征是:所述的套筒两端设置有螺纹导向角。