CN216864349U - 一种阳极钢爪热粘合修复设备 - Google Patents
一种阳极钢爪热粘合修复设备 Download PDFInfo
- Publication number
- CN216864349U CN216864349U CN202122592251.1U CN202122592251U CN216864349U CN 216864349 U CN216864349 U CN 216864349U CN 202122592251 U CN202122592251 U CN 202122592251U CN 216864349 U CN216864349 U CN 216864349U
- Authority
- CN
- China
- Prior art keywords
- steel claw
- machine head
- repair
- pole
- thermal bonding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型涉及一种阳极钢爪热粘合修复设备,属于电解铝技术领域。钢爪承接移动车安装在热粘机头前面,钢棒输送台安装在热粘机头的一侧;变压器的出线端一极通过干式电缆与电压分配器的一极相连,变压器的出线端另一极通过干式电缆与热粘机头的液压缸上端相连接,电压分配器另一端通过干式电缆与钢爪承接移动车相连接;液压泵站放在热粘机头的一侧。本实用新型的设备可以使得钢爪热粘合修复具有结合强度高(达到甚至超过母材的强度),修复速度快(每个爪头粘合只要2‑3分钟),成本低,是其它修复手段的1/3或1/4,是阳极钢爪修复工艺的极端工艺。
Description
技术领域
本实用新型涉及一种阳极钢爪热粘合修复设备,属于电解铝技术领域。
背景技术
电解铝行业阳极钢爪是大宗消耗件,长期以来,阳极钢爪修复工艺就是人工电焊修复、闪光焊、电渣熔焊或电渣焊(包括电渣丝极和板极),均是熔合焊接方法,均存在不同的不足,各工艺主要存在以下缺陷:
人工焊接:这是最原始的阳极钢爪修复工艺,就是切除已损坏的钢爪,用电焊补上一段钢棒,缺点是焊接面积小、使用寿命短、焊接处电阻大、发热异常严重。
闪光焊:由于焊接过程是在空气中,在碰焊过程中反复氧化,焊缝成分氧化铁成分高、脆性大、电阻高、使用寿命短。
电渣熔焊:效率低、成本高、能耗高、操作复杂。
电渣丝焊及电渣板极焊:成本高、效率低、焊接部位质量稳定性差,操作繁琐。
实用新型内容
本实用新型目的在于针对上述阳极钢爪修复工艺中的缺陷,开发出一种低成本,高效率,质量稳定的阳极钢爪热粘合修复设备。从而可以克服目前阳极钢爪修复工艺的不足,集低成本、高效率、质量好于一体,具有显著的综合优势,达到又快、又好、又省的理想状态。
本实用新型为了实现上述目的,采用如下技术方案:
一种阳极钢爪热粘合修复设备,钢爪承接移动车安装在热粘机头前面,钢棒输送台安装在热粘机头的一侧;
变压器的出线端一极通过干式电缆与电压分配器的一极相连,变压器的出线端另一极通过干式电缆与热粘机头的液压缸上端相连接,电压分配器另一端通过干式电缆与钢爪承接移动车相连接。
进一步的,钢棒输送台的一侧设置有操作台。
进一步的,液压泵站放在热粘机头通过液压油管与热粘机头的下油管相连接。
本实用新型的有益效果
本实用新型的设备可以使得钢爪热粘合修复具有结合强度高(达到甚至超过母材的强度),修复速度快(每个爪头粘合只要2-3分钟),成本低,是其它修复手段的1/3或1/4,是阳极钢爪修复工艺的极端工艺。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
下面将结合本实用新型实施例中的附图,对本实用新型实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本实用新型一部分实施例,而不是全部的实施例。基于本实用新型中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本实用新型保护的范围。
一种阳极钢爪热粘合修复设备,钢爪承接移动车1安装在热粘机头2前面,钢棒输送台3安装在热粘机头2的一侧;
变压器4的出线端一极通过干式电缆与电压分配器5的一极相连,变压器4的出线端另一极通过干式电缆与热粘机头2的液压缸8上端相连接,电压分配器5另一端通过干式电缆与钢爪承接移动车1相连接;
液压泵站6放在热粘机头2的一侧。
进一步的,钢棒输送台3的一侧设置有操作台7。
进一步的,液压泵站6放在热粘机头2一侧,通过液压油管与热粘机头2的下油管相连接。
将阳极钢爪吊装至钢爪承运车上,钢棒吊至输送小车上,给钢棒装上具有弹性抱紧装置的干式护套,钢棒端面离干式护套上端面30mm,将钢棒送至热粘头固定位置,将钢爪送至指定粘合位置,在干式护套30mm内腔加入热粘剂,在低压大电流的作用下热粘剂快速熔化,对两端面快速加热,2-3分钟即可,在油缸的大压力作用下,两端面粘压结合,完成热粘合过程。
本发明的技术原理:阳极钢爪热粘合技术就是快速形成的高温浅层(温度1500℃±100℃,热粘剂深均20-30mm)热粘剂液中对被粘合的两端面(上端面及下端面)在2-3分钟内快速加热到1200-1300℃的微熔塑性状态。在30-50吨的大压力的作用下挤压,两个端面产生塑性变形并牢固结合,实现粘合的效果,这个过程中由于热粘剂液的保护两端面与空气隔绝而无氧化现象,保证结合强度及结合面积。
上文中提到的全部方案中,涉及两个部件之间连接的可以根据实际情况选择焊接、螺栓和螺母配合连接、螺栓或螺钉连接或者其它公知的连接方式,在此不一一赘述,上文中凡是涉及有写固定连接的,优先考虑是焊接,尽管已经示出和描述了本实用新型的实施例,对于本领域的普通技术人员而言,可以理解在不脱离本实用新型的原理和精神的情况下可以对这些实施例进行多种变化、修改、替换和变型,本实用新型的范围由所附权利要求及其等同物限定。
Claims (3)
1.一种阳极钢爪热粘合修复设备,其特征在于:钢爪承接移动车(1)安装在热粘机头(2)前面,钢棒输送台(3)安装在热粘机头(2)的一侧;
变压器(4)的出线端一极通过干式电缆与电压分配器(5)的一极相连,变压器(4)的出线端另一极通过干式电缆与热粘机头(2)的液压缸(8)上端相连接,电压分配器(5)另一端通过干式电缆与钢爪承接移动车(1)相连接。
2.根据权利要求1所述的阳极钢爪热粘合修复设备,其特征在于:钢棒输送台(3)的一侧设置有操作台(7)。
3.根据权利要求1所述的阳极钢爪热粘合修复设备,其特征在于:液压泵站(6)放在热粘机头(2)一侧,通过液压油管与热粘机头(2)的下油管相连接。