CN2152655Y - 耐磨陶瓷橡胶衬板 - Google Patents

耐磨陶瓷橡胶衬板 Download PDF

Info

Publication number
CN2152655Y
CN2152655Y CN 93233642 CN93233642U CN2152655Y CN 2152655 Y CN2152655 Y CN 2152655Y CN 93233642 CN93233642 CN 93233642 CN 93233642 U CN93233642 U CN 93233642U CN 2152655 Y CN2152655 Y CN 2152655Y
Authority
CN
China
Prior art keywords
ceramic
rubber lining
wear
rubber
lining board
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 93233642
Other languages
English (en)
Inventor
胡新杰
朱远东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUNAN ELECTRICAL POWER CERAMICS AND APPLIANCE FACTORY
Original Assignee
HUNAN ELECTRICAL POWER CERAMICS AND APPLIANCE FACTORY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUNAN ELECTRICAL POWER CERAMICS AND APPLIANCE FACTORY filed Critical HUNAN ELECTRICAL POWER CERAMICS AND APPLIANCE FACTORY
Priority to CN 93233642 priority Critical patent/CN2152655Y/zh
Application granted granted Critical
Publication of CN2152655Y publication Critical patent/CN2152655Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型介绍的耐磨陶瓷橡胶衬板,由陶瓷顶 板、橡胶层底板及粘胶层复合或镶嵌复合而成。与现 有用锰钢或普通钢材所做的衬板相比,其磨损率仅为 锰钢的1/260;既可节省钢材,又可延长更换周期, 同时也改善工人劳动强度。

Description

本实用新型涉及一种耐磨陶瓷橡胶衬板,是一种适应于电力、冶金行业输料系统的耐磨内衬板。
目前,在电力、冶金的输料系统中,多半采用钢材加工成的金属件作输送载体。由于钢材的耐磨性有限,所以在送料系统的某些部位,如下料斗,旋风分离器等部位最易磨损,这样使输料管道使用寿命短、更换频繁;既增加生产成本,又加重了工人劳动强度。近些年,常用硬度较大的锰钢板制作衬板,以加强易损部位的抗磨性,但运用中仍不如人意,生产实践迫切需要一种耐磨性能更高的衬板。
本实用新型的目的是提供一种耐磨陶瓷橡胶衬板,希望其既能加强输料通道易损部位的耐磨强度、减少更换频次、又能降低生产成本、减轻劳动强度。
这种耐磨陶瓷橡胶衬板,由陶瓷层顶板、和橡胶层底板经粘胶层复合而成;或者也可以由陶瓷顶板与橡胶底板镶嵌、粘胶复合而成。
该陶瓷顶板由高铝钢玉材料制成。
根据以上方案制作的耐磨陶瓷橡胶衬板,与现用锰钢衬板相比其优点是:硬度和耐磨性能有明显提高,在相同环境内锰钢板每30分钟磨损0.0523克,而耐磨陶瓷橡胶衬板每30分钟仅磨损0.0002克;磨损量仅相当于锰钢的1/260;经某电厂磨煤机(装于出口处作内衬)三个多月运行表明:耐磨陶瓷衬板仅磨损0.02mm,锰钢磨损1.5mm,而普通A3钢则磨损2mm。也就是说耐磨陶瓷橡胶衬板的耐磨性,相当于锰钢的75倍,相当于普通钢材的100倍。因而,可以部分取代钢材,延长了更换周期,降低了工人劳动强度,提高了劳动生产率。
附图1、2、3为本实用新型的结构示意图。
其中图1为纯胶结型复合耐磨陶瓷橡胶衬板,其陶瓷层顶板(1)与橡胶层底板(3)之间设置着一层粘结层(2)。
附图2给出是胶结、镶嵌复合耐磨陶瓷橡胶衬板。其陶瓷层顶板(1)经其背面的凹凸面,与橡胶底板(3)上的凸凹面经粘结层(3)复合固接呈一体。
图3是耐磨陶瓷橡胶衬板的陶瓷层顶板(1)卧嵌于橡胶层底板(3)内。

Claims (3)

1、一种耐磨陶瓷橡胶衬板,其特征是该衬板由陶瓷层顶板(1)与橡胶层底板(2)经粘胶层(3)复合而成。
2、一种耐磨陶瓷橡胶衬板,其特征是该衬板由陶瓷2顶板(1)与橡胶底板(2)镶嵌、粘胶复合而成。
3、根据权利要求1和2的耐磨陶瓷橡胶衬板,其陶瓷层顶板(1)、高铝钢玉材料制成。
CN 93233642 1993-04-03 1993-04-03 耐磨陶瓷橡胶衬板 Expired - Fee Related CN2152655Y (zh)