CN214875979U - 一种新型预印遇热即粘的烟包盒条 - Google Patents
一种新型预印遇热即粘的烟包盒条 Download PDFInfo
- Publication number
- CN214875979U CN214875979U CN202121311169.0U CN202121311169U CN214875979U CN 214875979 U CN214875979 U CN 214875979U CN 202121311169 U CN202121311169 U CN 202121311169U CN 214875979 U CN214875979 U CN 214875979U
- Authority
- CN
- China
- Prior art keywords
- preprinted
- cigarette packet
- preprinting
- novel
- glue
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型公开了一种新型预印遇热即粘的烟包盒条,包括烟包盒条本体,所述烟包盒条本体上设有用于包装的粘接面,所述粘接面上设有采用凹版印刷工艺印刷的预印胶块点。本实用新型烟标包装可直接折盒成型,无需二次上胶,不仅不另增设备及投入,降低设备维修成本。预印遇热即粘的烟包更适合于软包小盒包装,方便粘接,粘接牢固不易翘边。热熔胶采用水性胶体为原料,无毒、无害、安全、环保。
Description
技术领域:
本实用新型涉及一种新型预印遇热即粘的烟包盒条。
背景技术:
常规的烟包盒条包装成型过程中需要使用热熔胶,会出现胶量大小不一、胶的点位不到位、胶点形状不规则、胶液厚度不均匀等现象,产生烟包异型部位无法粘胶、易翘角、烟包形状易变形等问题,特别是复合镭射膜烟标,常出现粘接不牢固易翘边,形成假粘等质量问题,严重影响烟包表面平整度。而且,在生产过程中为保持用胶清洁和设备正常,每班包装机需对粘胶机构进行清洁,其粘胶机构需定期保养维修,影响仪器的有效作业率。
发明内容:
本实用新型是为了解决上述现有技术存在的问题而提供一种新型预印遇热即粘的烟包盒条。
本实用新型所采用的技术方案有:
一种新型预印遇热即粘的烟包盒条,包括烟包盒条本体,所述烟包盒条本体上设有用于包装的粘接面,所述粘接面上设有采用凹版印刷工艺印刷的预印胶块点。
进一步地,所述预印胶块点由热熔胶采用凹版印刷工艺印刷于粘接面上固化而成。
进一步地,所述热熔胶为水性热熔胶。
进一步地,所述预印胶块点为方形预印胶块点或异形预印胶块点或圆形预印胶块点。
进一步地,所述预印胶块点的宽度小于粘接面的宽度。
本实用新型采用凹版印刷工艺,将液态的热熔胶胶水印刷于盒条表面,热熔胶胶水经预热烘干固化成固体胶,固化于表面。烟包盒条包装成型后,不用再单独上热熔胶,在输送过程通道中,直接对预印胶块点进行加热干燥,即可形成粘连,达到烟包包装成型的要求。由此产生的有益效果为:本实用新型烟标包装可直接折盒成型,无需二次上胶,不仅不另增设备及投入,降低设备维修成本。预印遇热即粘的烟包更适合于软包小盒包装,方便粘接,粘接牢固不易翘边。热熔胶采用水性胶体为原料,无毒、无害、安全、环保。
附图说明:
图1是本实用新型所述的烟用硬盒包装纸预印胶块点示意图。
图2是本实用新型所述的烟用软盒包装纸预印胶块点示意图。
图3是本实用新型所述的烟用条盒包装纸预印胶块点示意图。
图中:
1、烟包盒条本体;11、粘接面;
2、方形预印胶块点;3、异形预印胶块点;4、圆形预印胶块点。
具体实施方式:
下面结合附图对本实用新型作进一步的说明。
如图1,本实用新型一种新型预印遇热即粘的烟包盒条,包括烟包盒条本体1,烟包盒条本体1上设有用于包装的粘接面11。在粘接面11上设有采用凹版印刷工艺印刷的预印胶块点。
本实用新型中的预印胶块点是由热熔胶采用凹版印刷工艺印刷于粘接面11上固化而成。
固化后预印胶块点的宽度小于粘接面11的宽度,使预印胶块点加热热涨后不伸出烟包盒条本体1的外表面,保证美观。
取已完成分切清废前所有工序的商标纸大张,在图1中的粘接面11区域,采用凹版印刷工艺,将液态水性热熔胶胶水印刷于粘接面11的8个预印胶块点,预热烘干,再进行清废及后续工序。胶块的形状、大小、位置可根据实际需要任意改变(预印胶块点形状可以为方形预印胶块点2或异形预印胶块点3或圆形预印胶块点4。
在烟盒折叠成型后,将预印胶块点加热软化,进行粘接作业,最终形成包装烟盒。
热熔胶为水性热熔胶,无毒、无害、使用更安全、环保。该胶水在粘接面11上印刷的厚度为40-70μm。预热烘干并形成预印胶块点的烘干温度为110~150℃。形成预印胶块点后,预印胶块点加热软化的软化温度为70-110℃。
使用时,烟标包装上包装机器,可直接折盒成型,无需二次上胶,包装在输送过程通道中,通过对预印胶块点进行加热干燥,实现烟标包装的粘接形成,实现烟标生产中的一次成型,不需要另加设备及投入,只增加辅料胶液成本,降低设备维修成本提升了卷烟产品的美誉度。
以上所述仅是本实用新型的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本实用新型原理的前提下还可以作出若干改进,这些改进也应视为本实用新型的保护范围。
Claims (5)
1.一种新型预印遇热即粘的烟包盒条,包括烟包盒条本体(1),所述烟包盒条本体(1)上设有用于包装的粘接面(11),其特征在于:所述粘接面(11)上设有采用凹版印刷工艺印刷的预印胶块点。
2.如权利要求1所述的新型预印遇热即粘的烟包盒条,其特征在于:所述预印胶块点由热熔胶采用凹版印刷工艺印刷于粘接面(11)上固化而成。
3.如权利要求2所述的新型预印遇热即粘的烟包盒条,其特征在于:所述热熔胶为水性热熔胶。
4.如权利要求1所述的新型预印遇热即粘的烟包盒条,其特征在于:所述预印胶块点为方形预印胶块点(2)或异形预印胶块点(3)或圆形预印胶块点(4)。
5.如权利要求1所述的新型预印遇热即粘的烟包盒条,其特征在于:所述预印胶块点的宽度小于粘接面(11)的宽度。