CN208393968U - 一种可热封式抗老化镭射防伪pet膜 - Google Patents

一种可热封式抗老化镭射防伪pet膜 Download PDF

Info

Publication number
CN208393968U
CN208393968U CN201820487743.XU CN201820487743U CN208393968U CN 208393968 U CN208393968 U CN 208393968U CN 201820487743 U CN201820487743 U CN 201820487743U CN 208393968 U CN208393968 U CN 208393968U
Authority
CN
China
Prior art keywords
coating
heat sealable
pet film
aging
pet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201820487743.XU
Other languages
English (en)
Inventor
范国训
谢秦
毛群波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changzhou Zhongheng New Material Co., Ltd
Original Assignee
CHANGZHOU ZHONGHENG NEW MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGZHOU ZHONGHENG NEW MATERIAL Co Ltd filed Critical CHANGZHOU ZHONGHENG NEW MATERIAL Co Ltd
Priority to CN201820487743.XU priority Critical patent/CN208393968U/zh
Application granted granted Critical
Publication of CN208393968U publication Critical patent/CN208393968U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型公开了一种可热封式抗老化镭射防伪PET膜,包括依次设置的PET基膜层、镀铝层、EVA胶粘层和抗老化母料涂层;所述PET基膜层的上表面涂覆有PVOH涂层,所述PVOH涂层的上表面依次设置有全息镭射涂层和防伪涂层,所述抗老化母料涂层的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层。本实用新型PET膜中,由于在PVOH涂层上设置了全息镭射涂层和防伪层,使得PET膜整体具有很好的防伪效果。在抗老化母料涂层的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层,增加了PET膜表面的张力,热封时,将薄膜的可热封涂层相对设置,直接热封即可,自粘性好,成本低。

Description

一种可热封式抗老化镭射防伪PET膜
技术领域
本实用新型涉及一种可热封式抗老化镭射防伪PET膜。
背景技术
PET膜又名耐高温聚酯薄膜。它具有优异的物理性能、化学性能及尺寸稳定性、透明性、可回收性,可广泛的应用于磁记录、感光材料、电子、电气绝缘、工业用膜、包装装饰、屏幕保护、光学级镜面表面保护等领域。
虽然PET薄膜本身对于水、氧气以及二氧化碳气体以及具有较高的阻隔性能,但是对于一些对阻隔性有特殊要求的场合,如番茄制品、对微量氧气敏感的熟产品等等,仅用PET作为包装材料就不能满足要求了。作为包装材料,可热封性是一种基本的性能,PET由于分子链本身是刚性的,加之生产过程中的热定型使得其结晶度高而导致熔点比较高,因此,PET薄膜自身不能热封结合,很大程度上限制了包装材料的使用。并且现有的PET薄膜的抗老化效果不理想,影响了使用寿命。
另外,现有的很多需要PET膜包装的产品都需要防伪功能,而现有的PET膜不具有防仿功能或防伪功能不佳。
实用新型内容
本实用新型目的是针对现有技术存在的缺陷提供一种可热封式抗老化镭射防伪PET膜。
本实用新型为实现上述目的,采用如下技术方案:一种可热封式抗老化镭射防伪PET膜,包括依次设置的PET基膜层、镀铝层、EVA胶粘层和抗老化母料涂层;所述PET基膜层的上表面涂覆有PVOH涂层,所述PVOH涂层的上表面依次设置有全息镭射涂层和防伪涂层,所述抗老化母料涂层的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层。
本实用新型的有益效果:本实用新型PET膜中由于在上PET基膜层的上表面设置了PVOH涂层,可以大大提高PET膜的整体强度;增加了镀铝层,使PET膜的水氧阻隔率下降到最低,接近于零,能更好的保护产品。由于在PVOH涂层上设置了全息镭射涂层和防伪层,使得PET膜整体具有很好的防伪效果。其中,将PVOH涂层设置在PET基膜层和全息镭射涂层之间,可以避免PVOH涂层直接暴露在空气中而受到潮湿,避免PVOH的氧气阻隔性降低。在抗老化母料涂层的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层,增加了PET膜表面的张力,热封时,将薄膜的可热封涂层相对设置,直接热封即可,自粘性好,成本低。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
图1所示,涉及一种可热封式抗老化镭射防伪PET膜,包括依次设置的PET基膜层1、镀铝层2、EVA胶粘层3和抗老化母料涂层4;所述PET基膜层1的上表面涂覆有PVOH涂层11,所述PVOH涂层11的上表面依次设置有全息镭射涂层12和防伪涂层13,所述抗老化母料涂层4的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层41。
本实用新型PET膜中由于在上PET基膜层的上表面设置了PVOH涂层,可以大大提高PET膜的整体强度;增加了镀铝层,使PET膜的水氧阻隔率下降到最低,接近于零,能更好的保护产品。由于在PVOH涂层上设置了全息镭射涂层和防伪层,使得PET膜整体具有很好的防伪效果。其中,将PVOH涂层设置在PET基膜层和全息镭射涂层之间,可以避免PVOH涂层直接暴露在空气中而受到潮湿,避免PVOH的氧气阻隔性降低。在抗老化母料涂层的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层,增加了PET膜表面的张力,热封时,将薄膜的可热封涂层相对设置,直接热封即可,自粘性好,成本低。
以上所述仅为本实用新型的较佳实施例,并不用以限制本实用新型,凡在本实用新型的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本实用新型的保护范围之内。

Claims (1)

1.一种可热封式抗老化镭射防伪PET膜,其特征在于:包括依次设置的PET基膜层(1)、镀铝层(2)、EVA胶粘层(3)和抗老化母料涂层(4);所述PET基膜层(1)的上表面涂覆有PVOH涂层(11),所述PVOH涂层(11)的上表面依次设置有全息镭射涂层(12)和防伪涂层(13),所述抗老化母料涂层(4)的下表面设有由热塑弹性烯烃聚合物制成的可热封涂层(41)。
CN201820487743.XU 2018-04-08 2018-04-08 一种可热封式抗老化镭射防伪pet膜 Active CN208393968U (zh)