CN208230812U CN201820738744.7U CN201820738744U CN208230812U CN 208230812 U CN208230812 U CN 208230812U CN 201820738744 U CN201820738744 U CN 201820738744U CN 208230812 U CN208230812 U CN 208230812U
Authority
CN
China
Prior art keywords
copper pipe
crystallizer copper
nozzle
inlet opening
crystallizer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201820738744.7U
Other languages
English (en)
Inventor
马龙
马焕群
孙成麟
程睦林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qinhuangdao Hanfeng Changbai Crystallizer Co Ltd
Original Assignee
Qinhuangdao Hanfeng Changbai Crystallizer Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qinhuangdao Hanfeng Changbai Crystallizer Co Ltd filed Critical Qinhuangdao Hanfeng Changbai Crystallizer Co Ltd
Priority to CN201820738744.7U priority Critical patent/CN208230812U/zh
Application granted granted Critical
Publication of CN208230812U publication Critical patent/CN208230812U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Continuous Casting (AREA)

Abstract

一种带喷嘴的结晶器铜管,包括矩型的结晶器铜管,所述结晶器铜管的下部外侧设有环形的进水槽,所述结晶器铜管的下端面分布有进水孔,该进水孔为与所述结晶器铜管的下端面垂直的圆形盲孔,所述的进水孔与所述的进水槽相连通,所述进水孔的下端设有向铸坯表面喷射水雾的喷嘴。本实用新型的有益效果是:进入结晶器铜管下部进水孔内的冷却水能够对装配密封结构处的铜管部分进行冷却,同时喷嘴喷射的冷却水能够喷射到初出结晶器铜管的铸坯表面,对初出结晶器铜管的铸坯进行有效的冷却,从而保证钢坯质量,提高连铸生产效率。

Description

带喷嘴的结晶器铜管
技术领域
本实用新型涉及用于金属连续铸造的结晶器铜管,具体涉及一种带喷嘴的结晶器铜管。
背景技术
结晶器铜管外表面与水套之间形成一定的水缝,将结晶器铜管内钢水的热量传递给水,使通过结晶器铜管的钢水形成具有一定强度和形状的铸坯壳。由于结晶器铜管装入结晶器后在铜管下部外侧设有密封结构,造成铜管下端有一小段不能通过水冷散热,并且铸坯在初出结晶器铜管时,二冷一段喷嘴也不能实现对初出结晶器铜管的铸坯进行有效的冷却,导致铸坯在此段的冷却强度减弱,影响钢坯质量和生产效率。
发明内容
本实用新型的目的在于针对上述问题,提供一种带喷嘴的结晶器铜管,以有效解决铸坯在结晶器铜管的下部以及在初出结晶器铜管时冷却强度减弱的问题。
实现上述目的的技术方案是:一种带喷嘴的结晶器铜管,包括矩型的结晶器铜管,所述结晶器铜管的下部外侧设有环形的进水槽,所述结晶器铜管的下端面分布有进水孔,该进水孔为与所述结晶器铜管的下端面垂直的圆形盲孔,所述的进水孔与所述的进水槽相连通,所述进水孔的下端设有向铸坯表面喷射水雾的喷嘴。
上述的带喷嘴的结晶器铜管,所述的喷嘴通过锥管螺纹配合与所述的进水孔相连接。
上述的带喷嘴的结晶器铜管,所述喷嘴的进水方向与出水方向成75°偏转。
上述的带喷嘴的结晶器铜管,所述的进水槽为方形截面槽。
本实用新型的有益效果是:进入结晶器铜管下部进水孔内的冷却水能够对装配密封结构处的铜管部分进行冷却,同时经喷嘴喷射的冷却水能够喷射到初出结晶器铜管的铸坯表面,对初出结晶器铜管的铸坯进行有效的冷却,从而保证钢坯质量,提高连铸生产效率。
附图说明
图1是本带喷嘴的结晶器铜管主视图。
图2是图1的左视图。
图3是图1的M向视图。
图4是图1的I局部放大图。
图中:1、结晶器铜管;2、进水槽;3、进水孔;4、喷嘴。
具体实施方式
结合附图对本实用新型的具体实施方式进行说明。
如图1、图2、图3和图4,本带喷嘴的结晶器铜管包括矩型的结晶器铜管1,该结晶器铜管1的上部设有卡板槽。在结晶器铜管1的下部外侧设有环形的进水槽2,该进水槽2可以采用矩形截面槽、∪型截面槽、方形截面槽,附图实施例的进水槽2为方形截面槽。在结晶器铜管1的下端面分布有进水孔3,该进水孔3为均匀分布在结晶器铜管1的四个侧面的圆形盲孔,并且该进水孔3与结晶器铜管1的下端面垂直设置,进水孔3的上端与进水槽2相连通,在进水孔3的下端通过锥管螺纹配合固定安装喷嘴4,该喷嘴4采用进水方向与出水方向成75°偏转的扁平形水雾侧喷喷嘴,各喷嘴4的出水方向分别朝向其各自相对的铸坯表面。
本实用新型的技术方案同样适用于圆型的结晶器铜管。

Claims (4)

1.一种带喷嘴的结晶器铜管,包括矩型的结晶器铜管(1),其特征是:所述结晶器铜管(1)的下部外侧设有环形的进水槽(2),所述结晶器铜管(1)的下端面分布有进水孔(3),该进水孔(3)为与所述结晶器铜管(1)的下端面垂直的圆形盲孔,所述的进水孔(3)与所述的进水槽(2)相连通,所述进水孔(3)的下端设有向铸坯表面喷射水雾的喷嘴(4)。
2.根据权利要求1所述的带喷嘴的结晶器铜管,其特征是:所述的喷嘴(4)通过锥管螺纹配合与所述的进水孔(3)相连接。
3.根据权利要求1所述的带喷嘴的结晶器铜管,其特征是:所述喷嘴(4)的进水方向与出水方向成75°偏转。
4.根据权利要求1所述的带喷嘴的结晶器铜管,其特征是:所述的进水槽(2)为方形截面槽。
CN201820738744.7U 2018-05-18 2018-05-18 带喷嘴的结晶器铜管 Active CN208230812U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201820738744.7U CN208230812U (zh) 2018-05-18 2018-05-18 带喷嘴的结晶器铜管

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201820738744.7U CN208230812U (zh) 2018-05-18 2018-05-18 带喷嘴的结晶器铜管

Publications (1)

Publication Number Publication Date
CN208230812U true CN208230812U (zh) 2018-12-14

Family

ID=64579666

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201820738744.7U Active CN208230812U (zh) 2018-05-18 2018-05-18 带喷嘴的结晶器铜管

Country Status (1)

Country Link
CN (1) CN208230812U (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110548839A (zh) * 2019-09-04 2019-12-10 中冶南方连铸技术工程有限责任公司 板坯连铸强制冷却结晶器
CN111545715A (zh) * 2019-02-12 2020-08-18 株式会社神户制钢所 连续铸造用铸模、连续铸造装置以及连续铸造方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111545715A (zh) * 2019-02-12 2020-08-18 株式会社神户制钢所 连续铸造用铸模、连续铸造装置以及连续铸造方法
CN110548839A (zh) * 2019-09-04 2019-12-10 中冶南方连铸技术工程有限责任公司 板坯连铸强制冷却结晶器

Similar Documents

Publication Publication Date Title
CN208230812U (zh) 带喷嘴的结晶器铜管
CN211218589U (zh) 紫铜锭大规格水平连铸用结晶器
WO2017193704A1 (zh) 冶金炉
CN110842162A (zh) 紫铜锭大规格水平连铸用结晶器
CN207272114U (zh) 一种水冷浇注锭模
CN104511578A (zh) 一种立式半连续铸造机结晶器冷却装置
CN203281828U (zh) 铝杆连铸机的无盲区冷却水系统
CN103894565A (zh) 一种改进冷却通道的结晶器
CN214735912U (zh) 一种落料结构及淬火冷却机构
CN102554150A (zh) 用于连续铸钢的结晶器
CN212884840U (zh) 一种消失模铸造用砂库的降温装置
CN107716882A (zh) 一种带有冲击冷却结构的结晶器
CN203411593U (zh) 电渣重熔结晶器
CN205217965U (zh) 连铸结晶器内环面的可分段冷却结构
CN209584338U (zh) 一种椭圆形扁锭结晶器
CN201220269Y (zh) 铸造用结晶器
CN207127226U (zh) 导流喷淋式冷却结晶器
CN203109200U (zh) 水冷金属型离心铸管机喷淋式冷却装置
CN208067267U (zh) 一种带有冲击冷却结构的结晶器
CN203155963U (zh) 一种浇注方坯的新型结晶器
CN211679912U (zh) 铸机循环水池自冷降温系统
CN203184640U (zh) 一种连铸用电磁旋流水口
CN105537542A (zh) 一种雾冷环悬吊式连铸机结晶器
CN205414350U (zh) 一种连铸结晶器内环面具有折流的可分段冷却结构
CN213104380U (zh) 一种强制冷却制造空心钢锭的浇注模具

Legal Events

Date Code Title Description
GR01 Patent grant
GR01 Patent grant
PE01 Entry into force of the registration of the contract for pledge of patent right

Denomination of utility model: Mould copper tube with nozzle

Effective date of registration: 20210423

Granted publication date: 20181214

Pledgee: Changjiang Technology sub branch of Qinhuangdao Bank Co.,Ltd.

Pledgor: QINHUANGDAO HANFENG CHANGBAI CRYSTALLIZER Co.,Ltd.

Registration number: Y2021980002952

PE01 Entry into force of the registration of the contract for pledge of patent right
PC01 Cancellation of the registration of the contract for pledge of patent right

Granted publication date: 20181214

Pledgee: Changjiang Technology sub branch of Qinhuangdao Bank Co.,Ltd.

Pledgor: QINHUANGDAO HANFENG CHANGBAI CRYSTALLIZER Co.,Ltd.

Registration number: Y2021980002952

PC01 Cancellation of the registration of the contract for pledge of patent right
PE01 Entry into force of the registration of the contract for pledge of patent right

Denomination of utility model: Crystallizer copper tube with nozzle

Granted publication date: 20181214

Pledgee: Changjiang Technology sub branch of Qinhuangdao Bank Co.,Ltd.

Pledgor: QINHUANGDAO HANFENG CHANGBAI CRYSTALLIZER Co.,Ltd.

Registration number: Y2024990000106

PE01 Entry into force of the registration of the contract for pledge of patent right