CN207367639U - 聚酰胺复合聚酯漆包铜圆线 - Google Patents

聚酰胺复合聚酯漆包铜圆线 Download PDF

Info

Publication number
CN207367639U
CN207367639U CN201721391674.4U CN201721391674U CN207367639U CN 207367639 U CN207367639 U CN 207367639U CN 201721391674 U CN201721391674 U CN 201721391674U CN 207367639 U CN207367639 U CN 207367639U
Authority
CN
China
Prior art keywords
layer
polyamide
round line
copper powder
enamelling cuprum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201721391674.4U
Other languages
English (en)
Inventor
冯海祥
章利明
高利泉
郭利吉
冯利忠
高小峰
沈华梁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Three Line Electrical Technology Co Ltd
Original Assignee
Zhejiang Three Line Electrical Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Three Line Electrical Technology Co Ltd filed Critical Zhejiang Three Line Electrical Technology Co Ltd
Priority to CN201721391674.4U priority Critical patent/CN207367639U/zh
Application granted granted Critical
Publication of CN207367639U publication Critical patent/CN207367639U/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型提供一种聚酰胺复合聚酯漆包铜圆线,包括有截面呈圆形的芯体,芯体表面包覆有聚酰胺漆层,聚酰胺漆层厚度为0.01‑0.02mm,聚酰胺漆层表面设有玻璃纤维层,玻璃纤维层厚度为0.02mm,玻璃纤维层表面设有聚酯纤维层,聚酯纤维层表面设有铜粉层,铜粉层表面设有绝缘层;绝缘层表面设有防氧化层。采用本方案后的漆包铜圆线具有强度高、绝缘性好、防氧化的优点。

Description

聚酰胺复合聚酯漆包铜圆线
技术领域
本实用新型涉及包铜圆线技术领域,尤其是指聚酰胺复合聚酯漆包铜圆线。
背景技术
漆包线是绕组线的一个主要品种,由导体和绝缘层两部组成,裸线经退火软化后,再经过多次涂漆,烘焙而成。但要生产出既符合标准要求,又满足客户要求的产品并不容易,它受原材料质量,工艺参数,生产设备,环境等因素影响,因此,各种漆包线的质量特性各不相同,现有的漆包线易氧化、强度低、绝缘性不佳。
发明内容
本实用新型的目的在于克服现有技术的不足,提供一种强度高、绝缘性好、防氧化的聚酰胺复合聚酯漆包铜圆线。
为实现上述目的,本实用新型所提供的技术方案为:聚酰胺复合聚酯漆包铜圆线,它包括有截面呈圆形的芯体,芯体表面包覆有聚酰胺漆层,聚酰胺漆层厚度为0.01-0.02mm,聚酰胺漆层表面设有玻璃纤维层,玻璃纤维层厚度为0.02mm,玻璃纤维层表面设有聚酯纤维层,聚酯纤维层表面设有铜粉层,铜粉层表面设有绝缘层;绝缘层表面设有防氧化层。
所述的铜粉层采用80目铜粉颗粒分布在聚酯纤维层表面形成。
所述的玻璃纤维层、聚酯纤维层、绝缘层之间通过聚酰胺漆浸渍复合形成一体。
所述的防氧化层采用Ni-Cr合金镀层,防氧化层厚度为0.02-0.05mm。
本实用新型在采用上述方案后,通过反复实验,限定各层次最佳厚度,使漆包铜圆线具有强度高、绝缘性好、防氧化的优点。
附图说明
图1为本实用新型的整体结构示意图。
具体实施方式
下面结合所有附图对本实用新型作进一步说明实用新型的较佳实施例为:参见附图1,本实施例所述的聚酰胺复合聚酯漆包铜圆线包括有截面呈圆形的芯体1,芯体1表面包覆有聚酰胺漆层2,聚酰胺漆层2厚度为0.01mm,聚酰胺漆层2表面设有玻璃纤维层3,玻璃纤维层3厚度为0.02mm,玻璃纤维层3表面设有聚酯纤维层4,聚酯纤维层4表面设有铜粉层5,铜粉层5采用80目铜粉颗粒分布在聚酯纤维层4表面形成,铜粉层5表面设有绝缘层6,玻璃纤维层3、聚酯纤维层4、绝缘层6之间通过聚酰胺漆浸渍复合形成一体;绝缘层6表面设有防氧化层7,防氧化层7采用Ni-Cr合金镀层,防氧化层7厚度为0.02mm。本实施例通过反复实验,限定各层次最佳厚度,使漆包铜圆线具有强度高、绝缘性好、防氧化的优点。
以上所述之实施例只为本实用新型之较佳实施例,并非以此限制本实用新型的实施范围,故凡依本实用新型之形状、原理所作的变化,均应涵盖在本实用新型的保护范围内。

Claims (4)

1.聚酰胺复合聚酯漆包铜圆线,其特征在于:它包括有截面呈圆形的芯体(1),芯体(1)表面包覆有聚酰胺漆层(2),聚酰胺漆层(2)厚度为0.01-0.02mm,聚酰胺漆层(2)表面设有玻璃纤维层(3),玻璃纤维层(3)厚度为0.02mm,玻璃纤维层(3)表面设有聚酯纤维层(4),聚酯纤维层(4)表面设有铜粉层(5),铜粉层(5)表面设有绝缘层(6);绝缘层(6)表面设有防氧化层(7)。
2.根据权利要求1所述的聚酰胺复合聚酯漆包铜圆线,其特征在于:铜粉层(5)采用80目铜粉颗粒分布在聚酯纤维层(4)表面形成。
3.根据权利要求1所述的聚酰胺复合聚酯漆包铜圆线,其特征在于:玻璃纤维层(3)、聚酯纤维层(4)、绝缘层(6)之间通过聚酰胺漆浸渍复合形成一体。
4.根据权利要求1所述的聚酰胺复合聚酯漆包铜圆线,其特征在于:防氧化层(7)采用Ni-Cr合金镀层,防氧化层(7)厚度为0.02-0.05mm。
CN201721391674.4U 2017-10-26 2017-10-26 聚酰胺复合聚酯漆包铜圆线 Active CN207367639U (zh)