CN205934618U - 钢轨绝缘接头胶接加热固化装置 - Google Patents
钢轨绝缘接头胶接加热固化装置 Download PDFInfo
- Publication number
- CN205934618U CN205934618U CN201620844383.5U CN201620844383U CN205934618U CN 205934618 U CN205934618 U CN 205934618U CN 201620844383 U CN201620844383 U CN 201620844383U CN 205934618 U CN205934618 U CN 205934618U
- Authority
- CN
- China
- Prior art keywords
- box
- rail
- electric appliance
- appliance control
- heat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本实用新型涉及一种钢轨绝缘接头胶接加热固化装置。它包括箱体(1)和电器控制箱(2),所述箱体(1)为中空的半圆柱体,电器控制箱(2)设置在箱体(1)的右端,箱体(1)内部中空形成腔体(3),所述箱体(1)由外而内包括外壳(1.1)、保温体(1.2)、加热体(1.3)和内胆(1.4),所述加热体(1.3)与电器控制箱(2)相连,本实用新型的使用包括绝缘夹板和高强度粘结剂A组份胶预热、钢轨预热与涂胶、安装绝缘夹板和保温固化。本实用新型一种钢轨绝缘接头胶接加热固化装置,在低温环境下,缩短了施工时间、提高了现场胶接质量。
Description
技术领域
本实用新型涉及一种钢轨绝缘接头胶接加热固化装置,用于低温环境下铁路线路的钢轨绝缘接头的现场胶接。
背景技术
在低温环境下,尤其是-40℃~10℃时,胶的物理和化学反应性能下降,如此会导致施工时间长,胶接质量差,因此铁路线路的钢轨绝缘接头的现场胶接一直是个难题。
发明内容
本实用新型的目的在于克服上述不足,提供了一种钢轨绝缘接头胶接加热固化装置,此装置利用其生成的热量在相对密闭空间所带来的温度上升,激活了胶接时所使用现场胶的物理和化学反应性能,缩短了施工时间、提高了现场胶接质量。
本实用新型的目的是这样实现的:
一种钢轨绝缘接头胶接加热固化装置,其特点是:它包括箱体和电器控制箱,所述箱体为中空的半圆柱体,电器控制箱设置在箱体的右端,箱体内部中空形成腔体,所述箱体由外而内包括外壳、保温体、加热体和内胆,所述加热体与电器控制箱相连。
与现有技术相比,本实用新型的有益效果是:
1、本实用新型一种钢轨绝缘接头胶接加热固化装置,通过加热固化装置生成的热量在相对密闭空间所带来的温度上升,激活了胶接时所使用现场胶的物理和化学反应性能,缩短了施工时间、提高了现场胶接质量,使得环境温度在零下-40℃~10℃时铁路线路现场胶接钢轨绝缘接头成为了可能;
2、本实用新型一种钢轨绝缘接头胶接加热固化装置,该装置使用操作简便、安全可靠,是低温环境温度下钢轨绝缘接头现场胶接的理想装置。
附图说明
图1为本实用新型一种钢轨绝缘接头胶接加热固化装置的结构示意图。
图2为图1的左视图。
图3为本实用新型与钢轨的配合示意图。
图中:
箱体1,
外壳1.1,
保温体1.2,
加热体1.3,
内胆1.4,
开口1.5,
电器控制箱2,
腔体3。
具体实施方式
参见图1-3,本实用新型涉及一种钢轨绝缘接头胶接加热固化装置,它包括箱体1和电器控制箱2,所述箱体1为中空的半圆柱体,箱体1的两个端面具有与钢轨配合的开口1.5,电器控制箱2设置在箱体1的右端,箱体1内部中空形成腔体3,所述箱体1由外而内包括外壳1.1、保温体1.2、加热体1.3和内胆1.4,所述外壳1.1和内胆1.4均采用不锈钢材料制成,所述加热体1.3与电器控制箱2相连。
本实用新型的使用方法如下:
步骤一、绝缘夹板和高强度粘结剂A组份胶预热,将两块绝缘夹板和粘结剂的罐装A组分胶放入加热固化装置内预热,罐装较不能贴近内胆表面,预热的同时对钢轨轨腰进行打磨除锈;
步骤二、钢轨预热与涂胶,轨腰除锈完毕后钢轨预热,用液化汽火焰在钢轨轨腰胶接处来回扫动,烘烤钢轨,长度范围大约1.5M。当钢轨轨温达到35~45℃时(以手指抚摸钢轨轨腰稍感发烫,但手指能长时间按住为依据),停止预热,用棉布清洁胶接面,准备涂胶;打开预热过的罐装A组份胶,快速搅拌均匀,再将罐装B组份胶倒入A组份胶中混合,最后将混合后的胶搅拌均匀;将混合后的胶直接涂在钢轨轨腰上,即与绝缘夹板结合部位,长度范围0.9M,剩余胶涂在绝缘夹板中间槽口处(若钢轨温度满足不了要求,可以改涂绝缘夹板)。
步骤三、安装绝缘夹板,从加热固化装置内取出绝缘夹板,在钢轨轨腰胶接处合上两块绝缘夹板,在钢轨上套好夹体,拧上螺栓,用直径25mm的圆钢上下拨动绝缘夹板,校正绝缘夹板使其与钢轨轨腹紧密贴合,逐渐拧紧夹体螺栓,夹体凹槽斜面一定要搁在钢轨底部的斜面上,两端螺母同时拧紧,初次扭矩控制在(750—800)N·m左右,在反复拧紧两端螺母过程中,要保持绝缘夹板与钢轨轨腹紧密贴合, 若施工中绝缘夹板与钢轨结合处渗溢粘结剂,将其涂在绝缘夹板槽口处。
步骤四、保温固化,绝缘夹板安装完毕后,用加热固化装置罩在钢轨上加热固化,钢轨底部与道床用硬纸板隔离,调节电器控制箱2的温度至150℃,同时加热固化装置外面覆盖棉以提高加热效率,待粘结剂最终硬化后(大约45—60分钟)。根据环境温度差异、胶接固化实际状况,加热时间作相应调整,之后复紧螺栓,两端螺母同时接近达到额定扭矩800—830N·m左右,放下防松板。
工作原理:
电器控制箱2设置好加热温度后启动,加热体1.3透过内胆1.4,对放置在腔体3内的物体进行加热。
Claims (1)
1.一种钢轨绝缘接头胶接加热固化装置,其特征在于:它包括箱体(1)和电器控制箱(2),所述箱体(1)为中空的半圆柱体,箱体(1)的两个端面具有与钢轨配合的开口(1.5),电器控制箱(2)设置在箱体(1)的右端,箱体(1)内部中空形成腔体(3),所述箱体(1)由外而内包括外壳(1.1)、保温体(1.2)、加热体(1.3)和内胆(1.4),所述加热体(1.3)与电器控制箱(2)相连。