CN205893362U - 用于生产空心电渣锭的扇形电极 - Google Patents
用于生产空心电渣锭的扇形电极 Download PDFInfo
- Publication number
- CN205893362U CN205893362U CN201620678169.7U CN201620678169U CN205893362U CN 205893362 U CN205893362 U CN 205893362U CN 201620678169 U CN201620678169 U CN 201620678169U CN 205893362 U CN205893362 U CN 205893362U
- Authority
- CN
- China
- Prior art keywords
- electrode
- sector
- fan
- electroslag
- consutrodes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
用于生产空心电渣锭的扇形电极,属于电渣熔铸技术领域,解决了现有技术中存在的无法保证大的填充比,自耗电极易变形的技术问题;本实用新型包括假电极和扇形自耗电极;所述扇形自耗电极包括多个扇形钢棒;多个扇形钢棒圆周均布并联焊接在假电极上;本实用新型具有电渣重熔的充填比高、熔化速度快;生产电渣锭绿色环保、节能高效、成本低、质量高的优点。
Description
技术领域
本实用新型属于电渣熔铸技术领域,具体涉及一种用于生产空心电渣锭的扇形电极。
背景技术
电渣锭的生产过程为:在铜制水冷结晶器内盛有熔融的炉渣,自耗电极一端插入熔渣内;自耗电极、渣池、金属熔池、钢锭、底水箱通过短网导线和变压器形成回路;在通电过程中,渣池放出焦耳热,将自耗电极端头逐渐熔化,熔融金属汇聚成液滴,穿过渣池,落入结晶器,形成金属熔池,受水冷作用,迅速凝固形成钢锭。
电渣重熔工艺参数中充填比对电渣锭的质量影响很大,在相同定型和一定的工艺参数下,大充填比在电渣重熔过程中,熔滴在结晶器内分布面积较大,且温度场比较均匀,熔池趋向为“U”型和“浅平”,熔炼出的电渣锭性能较好;同一锭型采用大充填比可以提高熔化速度,降低电耗。
目前,用于生产空心电渣锭的电极包括自耗电极1和假电极2,自耗电极1为由多个小直径圆棒101并联焊接成的圆环形。但现有技术中的自耗电极存在以下技术缺陷:由于小直径圆棒101的横截面积小,焊接出的自耗电极1在重熔过程中无法保证大的充填比;由于小直径圆棒101较细而且较长,焊接成的圆环形自耗电极容易变形,影响自耗电极与结晶器内壁的平行度。
本实用新型内容
本实用新型的目的是提供用于生产空心电渣锭的扇形电极,解决现有技术中存在的无法保证大的填充比,自耗电极易变形的技术问题。
本实用新型用于生产空心电渣锭的扇形电极包括假电极和扇形自耗电极;所述扇形自耗电极包括多个扇形钢棒;多个扇形钢棒圆周均布并联焊接在假电极上。
所述扇形钢棒的横截面积为扇形。
本实用新型的有益技术效果:本实用新型的扇形自耗电极由多个扇形电极并联焊接而成的圆环型,在内外结晶器尺寸相同的情况下,电渣重熔的充填比提高了,进而提高了熔化速度,提高了生产效率;降低了电耗,节省能源,降低了熔炼成本;生产同一锭型的空心电渣锭情况下,采用横截面积为扇形的钢棒的长度比采用小直径圆钢棒的长度短,进而降低了电极的整体高度,便于电极的安装;横截面积为扇形的钢棒与假电极的焊接工艺简单,绿色环保,能够保证电极的垂直度,进而提高了电渣锭的质量。
附图说明
图1为现有技术中用于生产空心电渣锭的电极的结构示意图;
图2为现有技术中用于生产空心电渣锭的电极的主视图;
图3为现有技术中用于生产空心电渣锭的电极的仰视图;
图4为本实用新型用于生产空心电渣锭的扇形电极的三维结构示意图;
图5为本实用新型用于生产空心电渣锭的扇形电极的主视图;
图6为本实用新型用于生产空心电渣锭的扇形电极的仰视图;
其中,1、自耗电极,101、小直径圆棒,2、假电极,3、扇形自耗电极,301、扇形钢棒。
具体实施方式
下面结合附图对本实用新型做进一步阐述。
参见附图3和附图4,本实用新型用于生产空心电渣锭的扇形电极包括假电极2和扇形自耗电极3;所述扇形自耗电极3包括多个扇形钢棒301;多个扇形钢棒301圆周均布并联焊接在假电极2上。
所述扇形钢棒301的横截面积为扇形。
Claims (2)
1.用于生产空心电渣锭的扇形电极,其特征在于,包括假电极(2)和扇形自耗电极(3);所述扇形自耗电极(3)包括多个扇形钢棒(301);多个扇形钢棒(301)圆周均布并联焊接在假电极(2)上。
2.根据权利要求1所述的用于生产空心电渣锭的扇形电极,其特征在于,所述扇形钢棒(301)的横截面积为扇形。