CN204208901U - 一种耐高温磨蚀传送辊 - Google Patents
一种耐高温磨蚀传送辊 Download PDFInfo
- Publication number
- CN204208901U CN204208901U CN201420675659.2U CN201420675659U CN204208901U CN 204208901 U CN204208901 U CN 204208901U CN 201420675659 U CN201420675659 U CN 201420675659U CN 204208901 U CN204208901 U CN 204208901U
- Authority
- CN
- China
- Prior art keywords
- roller
- transfer roller
- working face
- core
- high temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种耐高温磨蚀传送辊,属于热轧型钢传送辊。传送辊包括:中碳钢空心辊子、辊芯和金属陶瓷工作面;在中碳钢空心辊子的轴芯位置连接有辊芯,中碳钢空心辊子辊芯焊接成一体构成传送辊本体,辊芯中心有轴孔,在传送辊本体外侧的两端头连接有金属陶瓷工作面。这种由两种材料制造成型的传送辊具有优良的耐高温腐蚀和耐磨损性能,其使用寿命明显优于高铬铸铁、镍铬硼硅自熔合金堆焊辊。由传送辊本体提供转动和热轧型钢传送支撑功能,NiCrMo-WC金属陶瓷工作面提供传送辊耐高温和耐磨损使用性能,传送辊工作面分布在辊子的两个端头,方便辊子一端失效后更换另外一端继续使用,延长传送辊的使用寿命,广泛应用于热轧、冷轧型钢用传送辊,及其它相关传送辊。
Description
技术领域
本实用新型涉及一种热轧型钢传送辊,尤其是一种耐高温磨蚀传送辊。
背景技术
传送辊品质优劣正在成为热轧钢型材表面质量的主要影响因素,由于高温磨损和腐蚀使传送辊表面出现矩形沟槽或“V”型沟槽或腐蚀麻坑等缺陷,使其在传送热轧型钢时,导致型钢表面出现微凸起、裂纹、单位长度质量增加等质量缺陷。传送辊转动时其工作面与热轧型钢接触,依靠摩擦力输送型钢,传送辊工作面常常因表面腐蚀、磨损出现过早局部损坏而引起失效或报废,不仅影响型钢的输送效率,同时影响型钢的表面质量,严重时整台套设备生产线停产检修。
公开号为203679431的中国发明专利申请给出的《一种具有传动及压料支撑作用的辊道辊子》,该方法是由棍身和辊轴组成的结构,棍身端部安装链轮带动辊子转动。
公开号为203532511的中国发明专利申请给出的《金属和异形陶瓷组合辊子》,该方法是金属辊子本体外套装异形陶瓷,金属本体和异形陶瓷之间填充柔性填充层。
在多处公开资料和专利均有采用镍基自熔合金堆焊强化的轧辊或输送辊报道,基于堆焊层表面裂纹存在对热轧型钢表面质量的影响是严重的;也有文献报道钴基自熔合金堆焊强化,由于钴基自熔合金堆焊层表面耐高温磨损性能有限应用受限。此外,关于超音速火焰喷涂或等离子喷涂金属金属陶瓷涂层对输送辊进行强化,所用金属陶瓷主要由镍基自熔合金或钴基自熔合金加WC组成,涂层的结合性能还是影响高温腐蚀和磨损环境下的轧辊或输送辊的关键。
发明内容
本实用新型的目的是克服已有技术中的不足,提供一种结构简单、性能优良,稳定好、操作简便、耐高温腐蚀、耐高温磨损的传送辊。
为实现上述目的,本实用新型耐高温磨蚀传送辊结构包括:中碳钢空心辊子、辊芯和金属陶瓷工作面;在中碳钢空心辊子的轴芯位置连接有辊芯,中碳钢空心辊子辊芯焊接成一体构成传送辊本体,辊芯中心有轴孔,在传送辊本体外侧的两端头连接有金属陶瓷工作面。
所述的金属陶瓷工作面是由超音速火焰或超音速等离子喷涂成型的NiCrMo-WC传送辊金属陶瓷工作面。
有益效果:本发明的耐高温磨蚀传送辊结构与辊身辊轴结构辊子相比较,辊子结构紧凑、传送简单。辊体和辊芯设计为一体,有效实现自身滚动、传动和支撑功能。NiCrMo-WC金属陶瓷具有优良的耐高温磨损和耐高温腐蚀性能,工作面成型应力低,保证工作面与辊子本体结合性能优良。传送辊工作面分布在辊子的两个端头,方便辊子一端失效后更换另外一端继续使用,延长传送辊的使用寿命,避免更换安装麻烦,应用范围广泛,可以应用于热轧、冷轧型钢用传送辊,及其它相关传送辊。
附图说明
图1是本实用新型的结构示意图。
图2为图1的侧视结构图。
图中:1、中碳钢空心辊子;2、辊芯;3、金属陶瓷工作面。
具体实施方式
下面结合附图对本实用新型的一个实施例作进一步的描述:
耐高温磨蚀传送辊结构包括:中碳钢空心辊子1、辊芯2和金属陶瓷工作面3;在中碳钢空心辊子1的轴芯位置连接有辊芯2,中碳钢空心辊子辊芯焊接成一体构成传送辊本体,辊芯中心有轴孔,在传送辊本体外侧的两端头连接有金属陶瓷工作面。
所述的金属陶瓷工作面是由超音速火焰或超音速等离子喷涂成型的NiCrMo-WC传送辊金属陶瓷工作面。
具体的:耐高温磨蚀传送辊结构,由中碳钢空心辊子1,与空心辊子1焊接成一体的辊芯2组成传送辊本体,焊接方式为CO2气体保护焊实施的,辊子本体两个端头预先车削半径方向向内2~3mm,对工作面毛坯进行毛化,获得表面清洁度Sa3级基础上再继续毛化25%时间,获得粗糙度Rz30~65μm,几何棱角的毛化表面,超音速喷涂成型NiCrMo-WC合金工作面3,采用立方氮化硼砂轮对工作面3进行精加工完成传送辊制造。
所述的传送辊NiCrMo-WC金属陶瓷工作面(3)成分为4.0~5.5%C、10.5~15.5%Ni、1.5~15.0%Cr、1.0~2.0%Mo、0.5~1.5%Fe、余为W。
Claims (2)
1.一种耐高温磨蚀传送辊,其特征是:耐高温磨蚀传送辊包括:中碳钢空心辊子(1)、辊芯(2)和金属陶瓷工作面(3);在中碳钢空心辊子(1)的轴芯位置连接有辊芯(2),中碳钢空心辊子辊芯焊接成一体构成传送辊本体,辊芯中心有轴孔,在传送辊本体外侧的两端头连接有金属陶瓷工作面。
2.根据权利要求1所述的一种耐高温磨蚀传送辊,其特征在于:所述的金属陶瓷工作面是由超音速火焰或超音速等离子喷涂成型的NiCrMo-WC传送辊金属陶瓷工作面。