CN203403163U - 一种新型电解锰阴极板 - Google Patents
一种新型电解锰阴极板 Download PDFInfo
- Publication number
- CN203403163U CN203403163U CN201320396563.8U CN201320396563U CN203403163U CN 203403163 U CN203403163 U CN 203403163U CN 201320396563 U CN201320396563 U CN 201320396563U CN 203403163 U CN203403163 U CN 203403163U
- Authority
- CN
- China
- Prior art keywords
- hollow tube
- electrolytic manganese
- stainless steel
- novel electrolytic
- cathode plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种新型电解锰阴极板,由不锈钢板和具导电性的中空管组成,该中空管与所述不锈钢板一体设置,该中空管内铸入有紫铜。由于中空管中是直接铸入熔融的紫铜液,因此不需要成型的铜材,成本低,且制造方便;同时,紫铜液铸入具导电性的中空管,凝固后与中空管紧密接触,不易松动,导电性能良好。
Description
技术领域
本实用新型涉及一种用于电解锰的阴极板。
背景技术
目前,电解锰时使用的阴极板,最常见的是采用螺栓将两片紫铜排与不锈钢板连接成一体。虽然,紫铜排具有良好的导电性,但使用一段时间后,由于螺栓的松动,铜排与不锈钢板间会产生间隙,导致导电不理想,影响锰的产量。
于是,相关人士将紫铜排与不锈钢板焊接成一体,使阴极板的导电性能增强,但该种阴极板与前述阴极板都需要使用成型的铜材作为原材料,成本不低,有待改进。
发明内容
本实用新型所要解决的技术问题是:针对上述现有技术的不足,提供一种制作方便、成本低的新型电解锰阴极板。
为了解决上述技术问题,本实用新型所采用的技术方案是:一种新型电解锰阴极板,包括不锈钢板,其特点是,还包括具导电性的中空管,该中空管与所述不锈钢板一体设置,该中空管内铸入有紫铜。
较佳的,所述中空管与该不锈钢板焊接成一体。
较佳的,所述中空管为不锈钢管。
与现有技术相比,本实用新型的有益效果是:由于中空管中是直接铸入熔融的紫铜液,因此不需要成型的铜材,成本低,且制造方便;同时,紫铜液铸入具导电性的中空管,凝固后与中空管紧密接触,不易松动,导电性能良好。
附图说明
图1是本实用新型的结构示意图。
具体实施方式
参见图1,本实用新型为一种新型电解锰阴极板,由不锈钢板1与中空管2组成。该不锈钢板1与中空管2一体设置,在本实施例中,采用焊接成为一体。该中空管2具有良好的导电性,其内部铸入有紫铜3,该紫铜以熔融的紫铜液的形式铸入,凝固后会与中空管紧密接触。在本实施例中,该中空管2采用不锈钢管制成。
Claims (3)
1.一种新型电解锰阴极板,包括不锈钢板(1),其特征在于,还包括具导电性的中空管(2),该中空管(2)与所述不锈钢板(1)一体设置,该中空管(2)内铸入有紫铜(3)。
2.如权利要求1所述的一种新型电解锰阴极板,其特征在于,所述中空管(2)与该不锈钢板(1)焊接成一体。
3.如权利要求1或2所述的一种新型电解锰阴极板,其特征在于,所述中空管(2)为不锈钢管。