CN203240887U - 一种加热炉坯料跑偏纠正装置 - Google Patents
一种加热炉坯料跑偏纠正装置 Download PDFInfo
- Publication number
- CN203240887U CN203240887U CN 201320243003 CN201320243003U CN203240887U CN 203240887 U CN203240887 U CN 203240887U CN 201320243003 CN201320243003 CN 201320243003 CN 201320243003 U CN201320243003 U CN 201320243003U CN 203240887 U CN203240887 U CN 203240887U
- Authority
- CN
- China
- Prior art keywords
- deviation correcting
- furnace
- correcting device
- blank
- buffer board
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
加热炉坯料跑偏纠正装置,包括炉墙缓冲板(1)和纠偏装置(2)。炉墙缓冲板(1)和纠偏装置(2)分体制作,炉墙缓冲板(1)设置在正对坯料进料口的炉体侧墙(4)上,纠偏装置(2)数量为两件,分别布置于炉体侧墙(4)的两侧。炉墙缓冲板(1)能够避免坯料撞击侧墙(4),进而避免炉墙损坏。纠偏装置(2)能够使跑偏的坯料(3)得到纠正,防止刮蹭炉体侧墙(4)或坯料(3)掉道,从而保证炉子能够长期生产运行。
Description
技术领域
本实用新型属于冶金及机械行业的加热炉或热处理炉领域,具体涉及一种用于加热炉的坯料跑偏纠正装置。
背景技术
目前,国内钢铁行业和机械制造业中,普遍使用加热炉或热处理炉加热钢坯等坯料,坯料在加热炉中输送加热。加热炉在长期的生产运行过程中,由于进料方向存在偏差,钢坯与支撑架摩擦等原因,坯料在输送的过程中会出现横向跑偏以及在炉内前进时向炉侧跑偏。横向跑偏过大时会损坏炉墙,有时还会使坯料从水梁脱落造成停产事故。向炉侧跑偏过多时会刮炉体侧墙,使炉体侧墙发生损毁,严重时最终会导致加热炉不能正常生产。为了保证加热炉能够长期正常生产,需要设计一种可纠正坯料跑偏的装置,保证炉子能够长期生产运行。
发明内容
本实用新型的目的在于克服上述技术的不足,提供一种加热炉坯料跑偏纠正装置。该装置包括炉墙缓冲板和纠偏装置,炉墙缓冲板和纠偏装置分体制作,炉墙缓冲板设置在正对坯料进料口的炉体侧墙上,纠偏装置数量为两个,分别布置于炉体侧墙的两侧。炉墙缓冲板能够避免坯料撞击侧墙,纠偏装置能够使跑偏的坯料得到纠正,使坯料不至于刮蹭炉体侧墙,从而保证炉子能够长期运行。纠偏装置制作成弧形,便于平稳推动钢坯。炉墙缓冲板使用耐热钢或耐热铸钢制作,也可用普通钢材制作但需要水冷却,保证炉墙缓冲板在高温环境中具有足够的强度。纠偏装置使用耐热钢或耐热铸钢制作,也可用普通钢材制作但需要水冷却,还可以使用高强耐火材料制作,保证纠偏装置在高温环境中具有足够的强度。
附图说明
图1为本实用新型的示意图。
其中:1、炉墙缓冲板;2、纠偏装置;3、坯料;4、炉体侧墙。
具体实施方式
下面结合附图,对本实用新型作进一步描述。
加热炉坯料跑偏纠正装置,包括炉墙缓冲板1和纠偏装置2。炉墙缓冲板1和纠偏装置2分体制作,炉墙缓冲板1设置在正对坯料进料口的炉体侧墙4上,纠偏装置2数量为两个,分别布置于炉体侧墙4的两侧。炉墙缓冲板1能够避免坯料撞击侧墙4,纠偏装置2能够使跑偏的坯料3得到纠正,使坯料3不至于刮蹭炉体侧墙4,从而保证炉子能够长期运行。纠偏装置2制作成弧形,便于平稳推动钢坯3。炉墙缓冲板1使用耐热钢或耐热铸钢制作,也可用普通钢材制作但需要水冷却,保证炉墙缓冲板1在高温环境中具有足够的强度。纠偏装置2使用耐热钢或耐热铸钢制作,也可用普通钢材制作但需要水冷却,还可以使用高强 耐火材料制作,保证纠偏装置2在高温环境中具有足够的强度。当进炉坯料3因惯性等原因没有在适当的位置停下时,炉墙缓冲板1可以避免坯料撞击炉体侧墙4,进而避免炉墙损坏。当坯料3偏离前进方向接触到弧形纠偏装置2时,纠偏装置通过侧向推力将坯料向炉体中心推动,防止刮蹭炉体侧墙4或坯料3掉道,从而保证炉子能够长期生产运行。
Claims (3)
1.一种加热炉坯料跑偏纠正装置,其特征在于:包括设置在正对坯料进料口的炉体侧墙(4)上的炉墙缓冲板(1)和设置在炉体侧墙(4)两侧的纠偏装置(2)。
2.根据权利要求1所述的加热炉坯料跑偏纠正装置,其特征在于:纠偏装置(2)数量为两个。
3.根据权利要求1所述的加热炉坯料跑偏纠正装置,其特征在于:纠偏装置(2)制作成弧形。