CN204284891U - 横断面无直角连铸板坯 - Google Patents
横断面无直角连铸板坯 Download PDFInfo
- Publication number
- CN204284891U CN204284891U CN201420499822.4U CN201420499822U CN204284891U CN 204284891 U CN204284891 U CN 204284891U CN 201420499822 U CN201420499822 U CN 201420499822U CN 204284891 U CN204284891 U CN 204284891U
- Authority
- CN
- China
- Prior art keywords
- continuous casting
- transverse section
- steel billet
- right angle
- casting steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型专利提出了一种横断面无直角连铸板坯,解决板带生产中,由于连铸坯横断面直角的存在,连铸坯在输送过程中角部温降较其他部位明显偏大,在后续轧制过程中在板带边部形成“黑线”缺陷,影响板带产品的质量,必要时需将边部黑线剪掉,降低了成材率的问题。本实用新型专利提出的横断面无直角连铸板坯,通过对连铸机结晶器形状的改变,使连铸板坯横断面的四个角为圆弧,消除连铸坯横断面的四个直角,减小角部与其他部位的温差,消除“黑线”缺陷,提高板带产品的质量和成材率。
Description
技术领域
本实用新型涉及板带生产领域,特别是指用于板带轧制的横断面无直角连铸板坯。
背景技术
采用连铸板坯生产板带材是一种高效经济的方法,得到了广泛的应用。目前所采用的连铸板坯均为矩形连铸坯,其横断面为长方形,且四个角均为直角。高温的连铸板坯在运输过程中与周围介质的发生热交换,使连铸坯的温度降低。由于四个角部与周围介质的热交换明显大于其他部位,因此连铸板坯在进入轧机轧制时,四个直角处的温度明显低于其他部分。在轧制过程中,由于宽展和立辊的轧制变形,温度较低的角部会逐渐移动到板带的表面,沿板带长度方向产生一条明显的线状缺陷,通常称为“黑线”,尤其是在不锈钢轧制时最为明显,“黑线”与板带边部的距离与轧制工艺和立辊辊型有关。“黑线”的存在影响了板带产品的质量,通常需要将其剪掉,这将降低成材率。
实用新型内容
本实用新型提供横断面无直角连铸板坯,通过将横断面四个角部做成圆弧,解决了断面直角连铸板坯运输过程中,直角处温降大,致使轧制过程中产生“黑线”的问题。
为了实现上述目的,本实用新型采用如下技术方案:
所述的连铸板坯横截面其四个角均采用为圆弧过渡,所述的连铸板坯水平面与角部曲线光滑连接,所述的连铸板坯横截面不存在接近90°的直角。
将连铸机结晶器设计成与图1相适应的形状,生产出横断面无直角连铸板坯。
进一步,所述的横断面无直角连铸板坯直接或经过加热炉加热后进入轧机轧制,生产出无“黑线”板带材。
本实用新型的应用效果:本实用新型提出的横断面无直角连铸板坯,可以大大降低加热后连铸坯在运输过程中产生的温度不均,消除由于角部处温度过低产生的“黑线”问题,适合商业化推广。
附图说明
图1为横断面无直角连铸板坯示意图
具体实施方式
将连铸机结晶器设计成与图1相适应的形状。
Claims (1)
1.横断面无直角连铸板坯,其特征在于:所述的连铸板坯横截面其四个角均采用为圆弧过渡,所述的连铸板坯水平面与角部曲线光滑连接,所述的连铸板坯横截面不存在接近90°的直角。