Prior art keywords
waste heat
heat boiler
heating surface
temperature composite
alloy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201320180058
Other languages
English (en)
Inventor
陈明
翟文杰
陈昭芳
强学才
王军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
703th Research Institute of CSIC
Original Assignee
703th Research Institute of CSIC
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 703th Research Institute of CSIC filed Critical 703th Research Institute of CSIC
Priority to CN 201320180058 priority Critical patent/CN203144516U/zh
Application granted granted Critical
Publication of CN203144516U publication Critical patent/CN203144516U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Coating By Spraying Or Casting (AREA)

Abstract

本实用新型公开了一种余热锅炉受热面高温复合耐磨涂层,其技术要点在于:在以合金钢板制成的基体表面喷涂Ni-Cr合金涂层作为功能层,在Ni-Cr合金涂层与基体之间涂有过渡层,在Ni-Cr合金涂层外涂有封孔层。本实用新型提高了余热锅炉受热面的抗氧化、抗腐蚀、耐磨损等性能,同时可极大地缩短余热锅炉的检修周期,从而创造出更为可观的经济效益。

Description

一种余热锅炉受热面高温复合耐磨涂层
技术领域:
本实用新型涉及余热锅炉受热面的耐磨涂层,具体涉及一种余热锅炉受热面高温复合耐磨涂层。
背景技术:
随着我国节能减排工作的不断深入,余热利用技术得到广泛应用,特别是在钢铁、化工、焦炭等行业,余热利用发电已经成为发展循环经济的关键技术。但是在这些行业中,大多数余热载体温度较高、含尘量较大,对余热锅炉受热面(特别是过热器)磨损严重,不但影响余热锅炉使用寿命,而且也威胁到余热锅炉的安全运行,同时增加了检修维护成本,所以提高余热锅炉受热面(特别是过热器,此处烟气温度在1100℃左右)在高温下的强度和耐磨性能,对于延长余热锅炉的使用寿命,提高余热锅炉运行的安全性致关重要。
实用新型内容:
本实用新型的目的是提供一种余热锅炉受热面高温复合耐磨涂层,它可使复合耐磨涂层附着在余热锅炉的高温受热面上,提高了余热锅炉高温受热面的抗氧化、抗腐蚀、耐磨损等性能。
本实用新型的目的是通过以下方式实现的:该余热锅炉受热面高温复合耐磨涂层,其特征在于:在以合金钢板制成的基体表面喷涂有Ni-Cr合金涂层,Ni-Cr合金涂层与基体之间设有过渡层,Ni-Cr合金涂层外设有封孔层。
本实用新型的有益效果是:该余热锅炉受热面高温复合耐磨涂层,在以合金钢板制成的基体表面喷涂Ni-Cr合金涂层作为功能层,在Ni-Cr合金涂层与基体之间涂有过渡层,在Ni-Cr合金涂层外涂有封孔层,提高余热锅炉受热面的抗氧化、抗腐蚀、耐磨损等性能,同时可极大地缩短余热锅炉的检修周期,从而创造出更为可观的经济效益。
附图说明:
图1是本实用新型的结构示意图。
具体实施方式
参照图1,该余热锅炉受热面高温复合耐磨涂层,在以合金钢板制成的基体1表面喷涂有Ni-Cr合金涂层3。Ni-Cr合金涂层3与基体1之间涂有由纳米稀土钇和Ni-Al粉制成的过渡层2。Ni-Cr合金涂层外涂有由Cr3C2、稀土元素及有机树脂混合而成的封孔层3。制作时,先将纳米稀土钇与Ni-A1粉的高温自反应型耐磨涂料通过压力喷射方式喷涂至基体表面形成过渡层2,并将过渡层2加热至500℃进行高温固化;再将Ni-Cr合金通过超音速电弧热喷涂的方式喷涂至过渡层上形成Ni-Cr合金涂层3;最后将Cr3C2、稀土元素及有机树脂的混合物喷涂至Ni-Cr合金涂层上形成封孔层4。

Claims (1)

1.一种余热锅炉受热面高温复合耐磨涂层,其特征在于:在以合金钢板制成的基体表面喷涂有Ni-Cr合金涂层,Ni-Cr合金涂层与基体之间设有过渡层,Ni-Cr合金涂层外设有封孔层。
CN 201320180058 2013-04-11 2013-04-11 一种余热锅炉受热面高温复合耐磨涂层 Expired - Fee Related CN203144516U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201320180058 CN203144516U (zh) 2013-04-11 2013-04-11 一种余热锅炉受热面高温复合耐磨涂层

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201320180058 CN203144516U (zh) 2013-04-11 2013-04-11 一种余热锅炉受热面高温复合耐磨涂层

Publications (1)

Publication Number Publication Date
CN203144516U true CN203144516U (zh) 2013-08-21

Family

ID=48972059

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201320180058 Expired - Fee Related CN203144516U (zh) 2013-04-11 2013-04-11 一种余热锅炉受热面高温复合耐磨涂层

Country Status (1)

Country Link
CN (1) CN203144516U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109136815A (zh) * 2018-07-23 2019-01-04 翟恩荣 一种等离子表面熔覆工艺

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109136815A (zh) * 2018-07-23 2019-01-04 翟恩荣 一种等离子表面熔覆工艺

Similar Documents

Publication Publication Date Title
CN103160827B (zh) 一种余热锅炉受热面高温复合耐磨涂层及其制作方法
CN104264133B (zh) 面向生物油应用的内燃机活塞环摩擦表面涂层及其制备方法
CN102912277B (zh) 一种电弧喷涂粉芯线材
CN203144516U (zh) 一种余热锅炉受热面高温复合耐磨涂层
CN101985119A (zh) 新型金属表面复合涂层的制备工艺
CN104962177A (zh) 一种电厂锅炉管道用耐高温腐蚀耐磨涂料及其制备方法
CN103912738B (zh) 一种用于磁化煤粉的耐磨软管
CN204474703U (zh) 高炉封炉风口密封结构
CN202073766U (zh) 耐磨陶瓷泵套
CN202598531U (zh) 陶瓷内衬复合喷嘴
CN203518222U (zh) 一种热风炉
CN203695285U (zh) 一种利用天然气供能的自动喷淋涂装装置
CN107541693A (zh) 沉没辊耐腐蚀涂层制备工艺
CN104195500A (zh) 一种新型汽车电弧喷涂方法
CN201874833U (zh) 沉淀池专用泵
CN202108765U (zh) 高硬度耐磨合金泵轴
CN205887266U (zh) 一种铝锭专用的喷涂枪炬
CN203540863U (zh) 喷涂生产线预热装置
CN205331043U (zh) 用于潜水泵的新型叶轮
CN103350059A (zh) 钢管的生产方法
CN204693399U (zh) 循环流化床锅炉水冷壁管多重组合式防磨装置
CN205245814U (zh) 一种冶炼炉
CN206009056U (zh) 自动加温喷油装置
CN203757211U (zh) 一种用于磁化煤粉的耐磨软管
CN203175865U (zh) 一种具有防腐蚀层的罗茨泵

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C17 Cessation of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20130821

Termination date: 20140411