CN202989202U - 一种改进的aod炉供气枪 - Google Patents
一种改进的aod炉供气枪 Download PDFInfo
- Publication number
- CN202989202U CN202989202U CN 201220669888 CN201220669888U CN202989202U CN 202989202 U CN202989202 U CN 202989202U CN 201220669888 CN201220669888 CN 201220669888 CN 201220669888 U CN201220669888 U CN 201220669888U CN 202989202 U CN202989202 U CN 202989202U
- Authority
- CN
- China
- Prior art keywords
- steel
- gas supply
- spray guns
- furnace
- furnace body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及AOD炉技术领域,特别涉及一种改进的AOD炉供气枪,它包括炉体,所述炉体主要由炉壳和保温装置组成,所述炉体底部的一侧设置有两个喷枪,两个喷枪以炉体的轴心线对称设置,所述两个喷枪之间的夹角为42°~48°,所述喷枪的管径为14~18cm。使用本实用新型时,通过减小两个喷枪之间的夹角的度数,极大地分散了供气气体,能够让熔炉内的钢液得到均匀的气体,从而提高炼钢质量;通过增大喷枪的管径,有效增加了供气量,能够有效缩短炼钢时间,提高炼钢产量。另外,还可延长炉体的使用寿命,炉体炼钢的次数由原来30多炉提高到近50炉。本实用新型具有结构简单,设置合理,制作成本低等优点。
Description
技术领域
本实用新型涉及AOD炉技术领域,特别涉及一种改进的AOD炉供气枪。
背景技术
AOD炉又叫做氩氧精炼炉,是一种炉外精炼钢液的方法,主要的任务是脱碳保铬,并且能够很好的搅拌钢液,可以生产低碳钢,乃至超低碳钢。在AOD炉的底侧部装有向熔池水平方向吹入气体的喷枪,喷枪的数量一般为两支,喷枪延长线的会合点与炉子的竖轴重合。通常两支喷枪的夹角为600,而这样的角度不易使供气分散,进而影响炼钢质量。另外,现有喷枪的管径常采用12cm规格,喷枪供气量相对较小,不利于加快钢材熔化速度。因此,如何调整喷枪之间的夹角大小,保证炼钢质量;如何调整喷枪管径,保证炼钢速度等问题已成为业内研究的热点。
实用新型内容
本实用新型的目的在于针对现有技术的缺陷和不足,提供一种结构简单,设计合理、使用方便的改进的AOD炉供气枪。
为实现上述目的,本实用新型采用的技术方案是:本实用新型所述的一种改进的AOD炉供气枪,包括炉体,所述炉体主要由炉壳和保温装置组成,所述炉体底部的一侧设置有两个喷枪,两个喷枪以炉体的轴心线对称设置,所述炉体底部的另一侧设置有出钢口,所述两个喷枪之间的夹角为420~480,所述喷枪的管径为14~18cm。
进一步地,所述两个喷枪之间的夹角为450。
进一步地,所述喷枪的管径为16cm。
采用上述结构后,本实用新型有益效果为:本实用新型所述的一种改进的AOD炉供气枪,包括炉体,所述炉体主要由炉壳和保温装置组成,所述炉体底部的一侧设置有两个喷枪,两个喷枪以炉体的轴心线对称设置,所述炉体底部的另一侧设置有出钢口,所述两个喷枪之间的夹角为420~480,所述喷枪的管径为14~18cm。使用本实用新型时,通过减小两个喷枪之间的夹角的度数,极大地分散了供气气体,能够让熔炉内的钢液得到均匀的气体,从而提高炼钢质量;通过增大喷枪的管径,有效增加了供气量,能够有效缩短炼钢时间,提高炼钢产量。另外,还可延长炉体的使用寿命,每个炉体炼钢的次数由原来30多炉提高到近50炉。本实用新型具有结构简单,设置合理,制作成本低等优点。
附图说明
图1是本实用新型的结构示意图。
附图标记说明:1、炉体;2、炉壳;3、保温装置;4、喷枪;5、出钢口;D、管径;α、夹角。
具体实施方式
下面结合附图对本实用新型作进一步的说明。
如图1所示,本实用新型所述的一种改进的AOD炉供气枪,包括炉体1,所述炉体1主要由炉壳2和保温装置3组成,所述炉体1底部的一侧设置有两个喷枪4,两个喷枪4以炉体1的轴心线对称设置,所述炉体1底部的另一侧设置有出钢口5,所述两个喷枪4之间的夹角α为420~480,所述喷枪4的管径D为14~18cm。
作为本实用新型的一种优选方式,所述两个喷枪4之间的夹角α为450。
作为本实用新型的一种优选方式,所述喷枪4的管径D为16cm。这样可以使每炉的炼钢时间从80分钟缩短到60分钟以内,从而提高炼钢速度。
用本实用新型炼钢时,不仅能够分散供气气体,使熔炉内的钢液能够均匀地与气体混合,从而提高炼钢质量;而且能够增加供气量,有效缩短炼钢时间,提高炼钢产量。另外,该结构简单、设计合理,制造成本低。
以上所述仅是本实用新型的较佳实施方式,故凡依本实用新型专利申请范围所述的构造、特征及原理所做的等效变化或修饰,均包括于本实用新型专利申请范围内。
Claims (3)
1.一种改进的AOD炉供气枪,包括炉体(1),所述炉体(1)主要由炉壳(2)和保温装置(3)组成,所述炉体(1)底部的一侧设置有两个喷枪(4),两个喷枪(4)以炉体(1)的轴心线对称设置,所述炉体(1)底部的另一侧设置有出钢口(5),其特征在于:所述两个喷枪(4)之间的夹角(α)为420~480,所述喷枪(4)的管径(D)为14~18cm。
2.根据权利要求1所述的改进的AOD炉供气枪,其特征在于:所述两个喷枪(4)之间的夹角(α)为450。
3.根据权利要求2所述的改进的AOD炉供气枪,其特征在于:所述喷枪(4)的管径(D)为16cm。