CN202215891U - 一种耐高温防磨型正压膨胀节 - Google Patents

一种耐高温防磨型正压膨胀节 Download PDF

Info

Publication number
CN202215891U
CN202215891U CN201120326172XU CN201120326172U CN202215891U CN 202215891 U CN202215891 U CN 202215891U CN 201120326172X U CN201120326172X U CN 201120326172XU CN 201120326172 U CN201120326172 U CN 201120326172U CN 202215891 U CN202215891 U CN 202215891U
Authority
CN
China
Prior art keywords
sleeve pipe
expansion joint
lower sleeve
sleeve
insulating material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201120326172XU
Other languages
English (en)
Inventor
黄长军
丁乾彬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU SUNCO BOILER CO Ltd
Original Assignee
JIANGSU SUNCO BOILER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU SUNCO BOILER CO Ltd filed Critical JIANGSU SUNCO BOILER CO Ltd
Priority to CN201120326172XU priority Critical patent/CN202215891U/zh
Application granted granted Critical
Publication of CN202215891U publication Critical patent/CN202215891U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种耐高温防磨型正压膨胀节,其包括:与法兰相焊接的上套管、放置于法兰上的下套管及设置于上、下套管外侧的金属波纹管,所述上、下套管与金属波纹管之间设有保温材料,所述上、下套管的外壁设有数个挂钩,所述保温材料由钢丝网包裹并用挂钩固定在上、下套管上,在下套管的周围设有限位卡板,所述限位卡板和下套管之间留有径向膨胀间隙,所述上、下套管的内壁焊接有数个抓钉并敷设有防磨材料。从而可防止膨胀节泄漏、拉裂和磨损。

Description

一种耐高温防磨型正压膨胀节
技术领域
本实用新型涉及一种膨胀节,尤其涉及一种耐高温防磨型正压膨胀节。
背景技术
在锅炉、冶炼及化工行业,有的烟风道工作于高温、正压环境,且具有气流中粉尘浓度大、速度高、磨损性强的特点,由于存在膨胀差,通常在这些部位安装膨胀节,以吸收膨胀。目前使用的膨胀节,由于结构设计不合理,主要存在以下问题:1、运行中不能吸收径向膨胀而被拉裂;2、内部套管不能密封导致高温烟气泄露烧坏波纹管;3、在经过冷态、热态后,保温材料不能复原导致波纹管烧坏;4、内套管没有防磨材料而磨损。
因此,有必要提供一种解决上述技术问题的膨胀节。
实用新型内容
本实用新型所要解决的技术问题是:提供一种可防止泄漏、拉裂和磨损的膨胀节。
为解决上述技术问题,本实用新型采用的技术方案为:一种耐高温防磨型正压膨胀节,其包括:与法兰相焊接的上套管、放置于法兰上的下套管及设置于上、下套管外侧的金属波纹管,所述上、下套管与金属波纹管之间设有保温材料,所述上、下套管的外壁设有数个挂钩,所述保温材料由钢丝网包裹并用挂钩固定在上、下套管上,在下套管的周围设有限位卡板,所述限位卡板和下套管之间留有径向膨胀间隙,所述上、下套管的内壁焊接有数个抓钉并敷设有防磨材料。
作为一种优选的方案,所述膨胀节的上套管与下套管紧密贴合。
作为一种优选的方案,所述挂钩与上、下套管的外壁相焊接。
本实用新型的有益效果是:通过上、下套管紧密贴合,在下套管与卡板之间留有径向膨胀间隙,在运行中不论发生轴向膨胀,还是径向膨胀,上、下套管始终保持密封状态,防止高温烟气泄露。保温材料以钢丝网包裹,并用挂钩固定在上、下套管上,在运行中无论膨胀节如何膨胀,挂钩均会让保温材料和套管同步移动,防止出现保温材料不能复原,从而发生烟气泄露。在上、下套管的内侧,设有抓钉,并敷设防磨材料,可防止内套管磨损。
附图说明
图1为耐高温防磨型正压膨胀节的结构示意图。
图1中:1、上套管,100、耐高温防磨型正压膨胀节,2、下套管,3、金属波纹管,4、保温材料,5、挂钩,6、钢丝网,7、限位卡板,8、径向膨胀间隙,9、抓钉,90、防磨材料。
具体实施方式
请参阅图1,一种耐高温防磨型正压膨胀节100,其包括:与法兰相焊接的上套管1、放置于法兰上的下套管2及设置于上、下套管外侧的金属波纹管3,所述上、下套管与金属波纹管3之间设有保温材料4,所述上、下套管的外壁设有数个挂钩5,所述保温材料4由钢丝网6包裹并用挂钩5固定在上、下套管1、2上,在下套管2的周围设有限位卡板7,所述限位卡板7和下套管2之间留有径向膨胀间隙8,所述上、下套管的内壁焊接有数个抓钉9并敷设有防磨材料90。所述膨胀节100的上套管1与下套管2紧密贴合。所述挂钩5与上、下套管1、2的外壁相焊接。
本实用新型通过上、下套管1、2紧密贴合,在下套管2与限位卡板7之间留有径向膨胀间隙8,在运行中不论发生轴向膨胀,还是径向膨胀,上、下套管始终保持密封状态,防止高温烟气泄露。保温材料4以钢丝网6包裹,并用挂钩5固定在上、下套管1、2上,在运行中无论膨胀节如何膨胀,挂钩5均会让保温材料4和套管同步移动,防止出现保温材料4不能复原,从而发生烟气泄露。在上、下套管的内侧,设有抓钉9,并敷设防磨材料90,从而可防止内套管磨损。

Claims (3)

1.一种耐高温防磨型正压膨胀节,其特征在于:该耐高温防磨型正压膨胀节包括:与法兰相焊接的上套管、放置于法兰上的下套管及设置于上、下套管外侧的金属波纹管,所述上、下套管与金属波纹管之间设有保温材料,所述上、下套管的外壁设有数个挂钩,所述保温材料由钢丝网包裹并用挂钩固定在上、下套管上,在下套管的周围设有限位卡板,所述限位卡板和下套管之间留有径向膨胀间隙,所述上、下套管的内壁焊接有数个抓钉并敷设有防磨材料。
2.如权利要求1所述的一种耐高温防磨型正压膨胀节,其特征在于:所述膨胀节的上套管与下套管紧密贴合。
3.如权利要求2所述的一种耐高温防磨型正压膨胀节,其特征在于:所述挂钩与上、下套管的外壁相焊接。
CN201120326172XU 2011-09-02 2011-09-02 一种耐高温防磨型正压膨胀节 Expired - Fee Related CN202215891U (zh)