CN202214417U - 一种金属管钝化装置 - Google Patents

一种金属管钝化装置 Download PDF

Info

Publication number
CN202214417U
CN202214417U CN2011202627620U CN201120262762U CN202214417U CN 202214417 U CN202214417 U CN 202214417U CN 2011202627620 U CN2011202627620 U CN 2011202627620U CN 201120262762 U CN201120262762 U CN 201120262762U CN 202214417 U CN202214417 U CN 202214417U
Authority
CN
China
Prior art keywords
tube
passivation
pipe
passivating
oven dry
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011202627620U
Other languages
English (en)
Inventor
陈青明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TIANJIN SHIJI METAL PRODUCT CO Ltd
Original Assignee
TIANJIN SHIJI METAL PRODUCT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TIANJIN SHIJI METAL PRODUCT CO Ltd filed Critical TIANJIN SHIJI METAL PRODUCT CO Ltd
Priority to CN2011202627620U priority Critical patent/CN202214417U/zh
Application granted granted Critical
Publication of CN202214417U publication Critical patent/CN202214417U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种金属管钝化装置,包括清洗管、钝化管、烘干管和传输管;所述清洗管、钝化管和烘干管通过传输管依次连接,所述钝化管内壁设有加热层,钝化管外壁设有试剂入口,所述烘干管内壁设有加热层,所述清洗管、钝化管、烘干管内径均大于传输管的外径。本实用新型采用流水线钝化装置,提高了钢管的钝化速率,同时也提高了钝化的效果。

Description

一种金属管钝化装置
技术领域
本实用新型属于金属管加工领域,尤其是涉及一种金属管钝化装置。
背景技术
众所周知,金属管在工业生产过程中担负着举足轻重的作用,由于金属在潮湿的环境中很容易被腐蚀,所以为了保护金属管不被腐蚀,在金属管出厂之前,需要对金属管进行钝化处理,传统的金属管钝化处理的方法分为电钝化和化学钝化,长期的实践经验发现,化学钝化的结果明显要好于电钝化的结果,但是传统的化学钝化流程比较复杂,各个钝化步骤之间缺乏连续性,在降低钝化效率的同时也影响了钝化的结果。
发明内容
本实用新型要解决的技术问题是提供一种自动化程度高,钝化效果好的的金属管钝化装置。
本实用新型是由以下技术方案实现的,一种金属管钝化装置,包括清洗管、钝化管、烘干管和传输管;所述清洗管、钝化管和烘干管通过传输管依次连接,所述钝化管内壁设有加热层,钝化管外壁设有试剂入口,所述烘干管内壁设有加热层,所述清洗管、钝化管、烘干管内径均大于传输管的外径。
所述钝化管内装有水和化学试剂。
作为优选方案:所述清洗管、钝化管、烘干管外径均相同。
本实用新型的有益效果为:由于采用了流水线的钝化方式,提高了钝化的效率,同时,由于金属管刚清洗完成后,直接进入钝化管,避免了再次被污染的可能性,使得钝化结果更好。
附图说明
图1是本实用新型的结构示意图
图中:
1、清洗管    2、钝化管    3、烘干管
4、传输管    5、试剂入口
具体实施方式
如图1所示:一种金属管钝化装置,包括清洗管1、钝化管2、烘干管3和传输管4;所述清洗管1、钝化管2和烘干管3通过传输管4依次连接,所述钝化管2内壁设有加热层,钝化管2外壁设有试剂入口,所述烘干管3内壁设有加热层,所述清洗管1、钝化管2、烘干管3内径均大于传输管4的外径。
所述钝化管2内装有水和化学试剂。
作为优选方案:所述清洗管1、钝化管2、烘干管3外径均相同。
本实例的工作过程为:
1、将钢管放入清洗管1前端的传输管4中,通过钝化管2外壁的试剂入口5将水合化学试剂放入钝化管2内;
2、启动装置,传输管4将待钝化的钢管送入清洗管1中,清洗管1内的清洗液将钢管外壁的杂质洗去,传输管4将清洗后的钢管送入钝化管2中;
3、钝化管2内的加热层对试剂溶液进行加热到50-60度之间,在此温度下钢管和试剂溶液反应20分钟,钢管外壁形成一层1毫米厚的防腐层;
4、传输管4将钝化后的钢管送入烘干管3中,烘干管3内部的加热层对钢管进行加热,将钢管外壁的试剂液体蒸发掉;
5、烘干完成后,传输管4将钝化好的钢管送入仓库保存。
以上对本实用新型的一个实施例进行了详细说明,但所述内容仅为本实用新型的较佳实施例,不能被认为用于限定本实用新型的实施范围。凡依本实用新型申请范围所作的均等变化与改进等,均应仍归属于本实用新型的专利涵盖范围之内。

Claims (3)

1.一种金属管钝化装置,包括清洗管(1)、钝化管(2)、烘干管(3)和传输管(4);其特征在于:所述清洗管(1)、钝化管(2)和烘干管(3)通过传输管(4)依次连接,所述钝化管(2)内壁设有加热层,钝化管(2)外壁设有试剂入口(5),所述烘干管(3)内壁设有加热层,所述清洗管(1)、钝化管(2)、烘干管(3)内径均大于传输管(4)的外径。
2.根据权利要求1所述的一种金属管钝化装置,其特征在于:所述钝化管(2)内装有水和化学试剂。
3.根据权利要求1所述的一种金属管钝化装置,其特征在于:所述清洗管(1)、钝化管(2)、烘干管(3)外径均相同。
CN2011202627620U 2011-07-23 2011-07-23 一种金属管钝化装置 Expired - Fee Related CN202214417U (zh)