CN201913185U - 铜镍合金铸锭用石墨模具 - Google Patents
铜镍合金铸锭用石墨模具 Download PDFInfo
- Publication number
- CN201913185U CN201913185U CN2011200032131U CN201120003213U CN201913185U CN 201913185 U CN201913185 U CN 201913185U CN 2011200032131 U CN2011200032131 U CN 2011200032131U CN 201120003213 U CN201120003213 U CN 201120003213U CN 201913185 U CN201913185 U CN 201913185U
- Authority
- CN
- China
- Prior art keywords
- die
- ingot casting
- corronil
- copper
- nickel alloy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种铜镍合金铸锭用石墨模具,涉及一种模具,包括模体和模盖,模体和模盖紧贴内壁设有氧化铝复合陶瓷内涂层,模盖上表面设有手柄,还包括通气孔,所述通气孔贯穿整个模盖及手柄。本实用新型结构简单,实用,方便,性能优异,保证了铜镍合金的性能。
Description
技术领域
本实用新型涉及一种模具,特别涉及一种铜镍合金铸锭用石墨模具。
背景技术
铜镍合金具有强韧、耐腐蚀等性能,是一种用量大、用途广、综合性能极佳的耐腐蚀合金,广泛用于化学、机械、核工业等领域。石墨材料集耐热性、抗震性、易于加工性、价格便宜等优点于一体,是冶金行业坩埚和模具制造的重要结构材料,受到业内人士的广泛关注。但是碳在高温下具有较高的反应活性,高温下与铜镍合金反应强烈,增加了铜镍合金的碳含量,影响铜镍合金性能。
发明内容
本实用新型的目的就在于提供一种铜镍合金铸锭用石墨模具,结构简单,实用,方便,性能优异,保证了铜镍合金的性能。
本实用新型的技术方案是:一种铜镍合金铸锭用石墨模具,包括模体和模盖,模体和模盖紧贴内壁设有氧化铝复合陶瓷内涂层,模盖上表面设有手柄,还包括通气孔,所述通气孔贯穿整个模盖及手柄。
作为优选,氧化铝复合陶瓷内涂层的厚度为150~200μm。
作为优选,模体内底面四个角上设有倒角。
与现有技术相比,本实用新型的有益效果在于:氧化铝复合陶瓷内涂层能够有效地把铜镍合金熔料和石墨体隔绝开来,避免铜镍合金与石墨发生反应,提高了合金熔体的纯度,保护了石墨模具,增加了石墨模具的使用寿命。在模体上加上模盖能够使铜镍合金铸锭四周热场均匀,避免铜镍合金组织不均匀而影响其使用性能。模盖上的通气孔,能够使模体内合金熔料引起的热气顺畅排出,利于铸锭的冷却。模体内底面的倒角便于取出成型的铸锭。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
下面将结合附图对本实用新型作进一步说明。
如图1所示一种铜镍合金铸锭用石墨模具,包括模体1和模盖2,模体1和模盖2紧贴内壁设有氧化铝复合陶瓷内涂层3,模盖2上表面设有手柄4,还包括通气孔,所述通气孔贯穿整个模盖2及手柄4。作为优选,氧化铝复合陶瓷内涂层3的厚度为150~200μm;模体1内底面四个角上设有倒角。
冶炼时,首先将模体1和模盖2放在箱式电路内预热,预热温度为300~400℃,保温半小时,将熔炼好的铜镍合金液体倒入模体1中,盖上石墨的模盖2,待合金冷却时取下模盖2,倒出铜镍合金铸锭。
Claims (3)
1.一种铜镍合金铸锭用石墨模具,其特征在于:包括模体和模盖,模体和模盖紧贴内壁设有氧化铝复合陶瓷内涂层,模盖上表面设有手柄,还包括通气孔,所述通气孔贯穿整个模盖及手柄。
2.根据权利要求1所述的铜镍合金铸锭用石墨模具,其特征在于:氧化铝复合陶瓷内涂层的厚度为150~200μm。
3.根据权利要求1或2所述的铜镍合金铸锭用石墨模具,其特征在于:模体内底面四个角上设有倒角。