CN201738029U - 电镀锌彩涂连续生产线 - Google Patents
电镀锌彩涂连续生产线 Download PDFInfo
- Publication number
- CN201738029U CN201738029U CN2010202298101U CN201020229810U CN201738029U CN 201738029 U CN201738029 U CN 201738029U CN 2010202298101 U CN2010202298101 U CN 2010202298101U CN 201020229810 U CN201020229810 U CN 201020229810U CN 201738029 U CN201738029 U CN 201738029U
- Authority
- CN
- China
- Prior art keywords
- coating
- roll
- tensioner
- deviation correcting
- machine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种电镀锌彩涂连续生产线,由下列设备依次连接:上卷小车→开卷机→开卷夹送辊→入口剪板机→缝合机→去毛刺辊→1#张力器→入口活套→预清洗装置→刷洗装置→碱水清洗装置→水洗装置→热风干燥器→镀前酸洗装置→镀前水洗装置→纠偏装置→电镀段→化学辊涂装置→化涂干燥炉→2#张力器→纠偏装置→初涂辊涂装置→初涂固化炉→水淬冷却装置→冷风干燥装置→3#张力器→支撑辊组→纠偏装置→精涂辊涂装置→精涂固化炉→水淬冷却装置→冷风干燥装置→4#张力器→出口活套装置→5#张力器→夹送辊装置→出口剪板机→出口夹送辊→卷取机→卸卷小车。所述生产线将电镀和彩涂整合在同一生产线上,能源消耗低,灵活性和独创性强。
Description
技术领域
本实用新型涉及一种生产线,特别是涉及一种以镀锌带钢和冷轧钢为原料,采用两涂两烘的生产工艺,连续生产彩涂板卷的电镀锌彩涂连续生产线。
背景技术
带材图层产生于19世纪30年代,由于它不仅加工性能和防腐性能优良,而且外表美观,因此在现代建筑业、汽车制造业、造船业、电器工业等各领域被广泛地应用。然而,现有的彩涂板卷生产线都是电镀和彩涂不在同一生产线上,工艺布置能源消耗大,单一机组的生产品种的灵活性和独创性弱,因此,需要对其进行改进。
发明内容
本实用新型彩涂板卷生产线旨在提供一种以镀锌带钢和冷轧带钢为原料,将电镀和彩涂整合在同一生产线上,可以十分方便地改为镀锌彩涂生产线或电镀锌生产线,同时有效地减少能源消耗,更增强了单一机组的生产品种的灵活性和独创性的电镀锌彩涂连续生产线。
本实用新型电镀锌彩涂连续生产线的技术方案如下:
本实用新型电镀锌彩涂连续生产线由下列设备依次连接:上卷小车→开卷机→开卷夹送辊→入口剪板机→缝合机→去毛刺辊→1#张力器→入口活套→预清洗装置→刷洗装置→碱水清洗装置→水洗装置→热风干燥器→镀前酸洗装置→镀前水洗装置→纠偏装置→电镀段→化学辊涂装置→化涂干燥炉→2#张力器→纠偏装置→初涂辊涂装置→初涂固化炉→水淬冷却装置→冷风干燥装置→3#张力器→支撑辊组→纠偏装置→精涂辊涂装置→精涂固化炉→水淬冷却装置→冷风干燥装置→4#张力器→出口活套装置→5#张力器→夹送辊装置→出口剪板机→出口夹送辊→卷取机→卸卷小车。
本实用新型电镀锌彩涂连续生产线的有益效果在于:本实用新型电镀锌彩涂连续生产线将电镀和彩涂整合在同一生产线上,同时,可以十分方便地改为镀锌彩涂生产线或电镀锌生产线,这种工艺布置有效地减少了能源消耗,更增强了单一机组的生产品种的灵活性和独创性。
附图说明
图1是本实用新型电镀锌彩涂连续生产线的构成示意图;
其中,1、上卷小车,2、开卷机,3、开卷夹送辊,4、入口剪板机,5、缝合机,6、去毛刺辊,7、1#张力器,8、入口活套,9、预清洗装置,10、刷洗装置,11、碱水清洗装置,12、水洗装置,13、热风干燥器,14、镀前酸洗装置,15、镀前水洗装置,16、纠偏装置,17、电镀段,18、化学辊涂装置,19、化涂干燥炉,20、2#张力器,21、纠偏装置,22、初涂辊涂装置,23、初涂固化炉,24、水淬冷却装置,25、冷风干燥装置,26、3#张力器,27、支撑辊组,28、纠偏装置,29、精涂辊涂装置,30、精涂固化炉,31、水淬冷却装置,32、冷风干燥装置,33、4#张力器,34、出口活套装置,35、5#张力器,36、夹送辊装置,37、出口剪板机,38、出口夹送辊,39、卷取机,40、卸卷小车。
具体实施方式
参见附图1,本实用新型电镀锌彩涂连续生产线由下列设备依次连接:上卷小车1→开卷机2→开卷夹送辊3→入口剪板机4→缝合机5→去毛刺辊6→1#张力器7→入口活套8→预清洗装置9→刷洗装置10→碱水清洗装置11→水洗装置12→热风干燥器13→镀前酸洗装置14→镀前水洗装置15→纠偏装置16→电镀段17→化学辊涂装置18→化涂干燥炉19→2#张力器20→纠偏装置21→初涂辊涂装置22→初涂固化炉23→水淬冷却装置24→冷风干燥装置25→3#张力器26→支撑辊组27→纠偏装置28→精涂辊涂装置29→精涂固化炉30→水淬冷却装置31→冷风干燥装置32→4#张力器33→出口活套装置34→5#张力器35→夹送辊装置36→出口剪板机37→出口夹送辊38→卷取机39→卸卷小车40。
Claims (1)
1.电镀锌彩涂连续生产线,其特征在于:由下列设备依次连接:上卷小车→开卷机→开卷夹送辊→入口剪板机→缝合机→去毛刺辊→1#张力器→入口活套→预清洗装置→刷洗装置→碱水清洗装置→水洗装置→热风干燥器→镀前酸洗装置→镀前水洗装置→纠偏装置→电镀段→化学辊涂装置→化涂干燥炉→2#张力器→纠偏装置→初涂辊涂装置→初涂固化炉→水淬冷却装置→冷风干燥装置→3#张力器→支撑辊组→纠偏装置→精涂辊涂装置→精涂固化炉→水淬冷却装置→冷风干燥装置→4#张力器→出口活套装置→5#张力器→夹送辊装置→出口剪板机→出口夹送辊→卷取机→卸卷小车。