改进的连铸坯冷却用结晶器 Download PDF

Info

Publication number
CN201603846U
CN201603846U CN2010201072413U CN201020107241U CN201603846U CN 201603846 U CN201603846 U CN 201603846U CN 2010201072413 U CN2010201072413 U CN 2010201072413U CN 201020107241 U CN201020107241 U CN 201020107241U CN 201603846 U CN201603846 U CN 201603846U
Authority
CN
China
Prior art keywords
cooling
continuous casting
casting billet
crystallizer
cooling water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010201072413U
Other languages
English (en)
Inventor
王建新
黄星武
张怀忠
徐逸飞
马国伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xinjiang Bayi Iron and Steel Co Ltd
Original Assignee
Xinjiang Bayi Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xinjiang Bayi Iron and Steel Co Ltd filed Critical Xinjiang Bayi Iron and Steel Co Ltd
Priority to CN2010201072413U priority Critical patent/CN201603846U/zh
Application granted granted Critical
Publication of CN201603846U publication Critical patent/CN201603846U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种改进的连铸坯冷却用结晶器,包括在两侧足辊架上分别相对安装的冷却水喷嘴,冷却水喷嘴喷出的水冷却面呈三角形,与连铸坯外表面相接触的相邻两三角形冷却面一侧部均相互交叉重合,即相邻两喷嘴喷到连铸坯表面上的水呈连续布置。本实用新型改善了铸坯在足辊段的冷却能力,减少了漏钢事故的发生,3#连铸机漏钢率由原来的0.12%减少到0.06%。去掉了足辊后,避免了漏钢钢水粘结足辊、产生冻坯现象,为稳定生产奠定了基础,提高了铸机作业率。

Description

改进的连铸坯冷却用结晶器
技术领域
本实用新型属于连铸坯冷却结晶器结构的改进,特别是改进的连铸坯冷却用结晶器。
背景技术
连铸坯冷却,包括了结晶器冷却和二次冷却两部分。连铸坯在结晶器内仅仅凝固了10~20%的钢水量,约80~90%钢水尚未凝固,离开结晶器后的铸坯凝固成一个较薄的外壳(8~15mm),内部仍是高温钢水。为使连铸坯继续凝固,从结晶器出口到拉矫机长度内设置多段喷水区,即二次冷却区,足辊冷却段是铸坯离开结晶器后进行二次冷却的第一段,漏钢一般发生这一段,因此,足辊段的作用非常重要。但是十几年来的生产实践表明,安装的足辊存在挡水问题,导致连铸坯的冷却面积减小,达不到应有的冷却效果。
发明内容
本实用新型的目的在于提供一种改进的连铸坯冷却用结晶器,其结构简单,造价低廉,能够有效地对连铸坯两侧进行充分连续的冷却,冷却效果好,彻底杜绝漏钢事故的发生。
本实用新型的目的是这样实现的:一种改进的连铸坯冷却用结晶器,包括在两侧足辊架上分别相对安装的冷却水喷嘴,冷却水喷嘴喷出的水冷却面呈三角形,与连铸坯外表面相接触的相邻两三角形冷却面一侧部均相互交叉重合,即相邻两喷嘴喷到连铸坯表面上的水呈连续布置。
所说的冷却水喷嘴的喷射角为102°。
本实用新型优化了冷却喷嘴喷出的水冷面积,使得水冷却面呈连续布置,消除了冷却死角,杜绝了因存在足辊而导致连铸坯有部分区段不能被充分冷却的问题,冷却效果好,彻底杜绝了漏钢事故的发生。本实用新型结构简单,由于没有足辊的阻挡,因而降低了生产成本,还能充分确保生产正常有序进行。
附图说明
下面将结合附图对本实用新型作进一步说明。
附图为本实用新型的主视结构示意图。
具体实施方式
一种改进的连铸坯冷却用结晶器,如附图所示,包括在两侧足辊架3上分别相对安装的冷却水喷嘴2,冷却水喷嘴2喷出的水冷却面呈三角形,与连铸坯1外表面相接触的相邻两三角形冷却面一侧部均相互交叉重合,即相邻两喷嘴喷到连铸坯1表面上的水呈连续布置,这样能够充分消除连铸坯1两侧面上的冷却死角,确保连铸坯1两侧都能够得到充分而连续的冷却。
所说的冷却水喷嘴2的喷射角为102°。
当然,在采用不同角度喷射角的前提下,还可以对所说的冷却水喷嘴2的间距进行调整,以便保证水冷却面侧部的交叉重合。

Claims (2)

1.一种改进的连铸坯冷却用结晶器,包括在两侧足辊架上分别相对安装的冷却水喷嘴,其特征是:冷却水喷嘴喷出的水冷却面呈三角形,与连铸坯外表面相接触的相邻两三角形冷却面一侧部均相互交叉重合,即相邻两喷嘴喷到连铸坯表面上的水呈连续布置。
2.根据权利要求1所述的改进的连铸坯冷却用结晶器,其特征是:所说的冷却水喷嘴的喷射角为102°。
CN2010201072413U 2010-02-03 2010-02-03 改进的连铸坯冷却用结晶器 Expired - Fee Related CN201603846U (zh)