CN201565485U - 一种高效冷却铝型材热挤压模具结构 - Google Patents

一种高效冷却铝型材热挤压模具结构 Download PDF

Info

Publication number
CN201565485U
CN201565485U CN2009202736870U CN200920273687U CN201565485U CN 201565485 U CN201565485 U CN 201565485U CN 2009202736870 U CN2009202736870 U CN 2009202736870U CN 200920273687 U CN200920273687 U CN 200920273687U CN 201565485 U CN201565485 U CN 201565485U
Authority
CN
China
Prior art keywords
liquid nitrogen
mold
die
mould
cushion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009202736870U
Other languages
English (en)
Inventor
严荣庆
郑晓军
陈纪欢
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Ruisile Composite Metal Materials Co., Ltd.
Shanghai Zhenxing Aluminium Industry Co., Ltd.
Xinshi Aluminum (Shanghai) Co., Ltd.
Original Assignee
SHANGHAI ZHENXING ALUMINIUM INDUSTRY Co Ltd
XINSHI ALUMINUM (SHANGHAI) CO Ltd
SHANGHAI RUISILE DOORS AND WINDOWS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI ZHENXING ALUMINIUM INDUSTRY Co Ltd, XINSHI ALUMINUM (SHANGHAI) CO Ltd, SHANGHAI RUISILE DOORS AND WINDOWS CO Ltd filed Critical SHANGHAI ZHENXING ALUMINIUM INDUSTRY Co Ltd
Priority to CN2009202736870U priority Critical patent/CN201565485U/zh
Application granted granted Critical
Publication of CN201565485U publication Critical patent/CN201565485U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供一种高效冷却铝型材热挤压模具结构,它包括模具、模垫,在模垫的外沿上设置有液氮入口,在模垫与模具的接触面上设置有液氮通道,液氮通道与液氮入口连通;液氮通道的出口导入模具,在模具上与液氮通道出口对应的位置设计有液氮导入孔,液氮导入孔通向模具的工作带。本实用新型结构直接冷却到模具工作带处,可实现对模具工作带和模具出口型材的直接冷却,冷却效果更佳。

Description

一种高效冷却铝型材热挤压模具结构
技术领域
本实用新型涉及一种铝型材加工模具结构,尤其是一种高效冷却的铝型材热挤压模具结构。
背景技术
在铝型材热挤压生产过程中,铝锭在挤压筒内被挤压通过模具后,挤出的铝型材和模具温度均会升高,并且由于挤出的高温型材和模具都暴露在空气中,会出现如下缺陷:1.在铝型材表面产生坚硬的氧化铝颗粒,并且部分黏附在模具出口,对后续的型材表面会产生划痕,模具表面也会造成拉伤;2.持续升高的模具温度将导致模具表面退氮并降低硬度,从而缩短模具使用寿命;3.挤出的铝型材温度不断升高也将导致型材无规律变形甚至报废。基于上述技术问题,铝型材热挤压过程中,保持恒定的温度,既可以避免型材表面过早氧化,也能够显著提高基础型材的表面质量,也可延长模具使用寿命,提高铝型材挤出速度。为了解决上述问题,近年来液氮冷却模具技术得到了逐步推广应用。
现有技术液氮冷却方式和结构如图1、图2和图3所示,即在模具或模垫上加工出液氮通道,在挤压过程中把液氮从分布在模垫上的通道喷向模具,使模具冷却,同时液氮吸热蒸发后形成氮气,可排除模具出口的空气,对型材形成气体保护,防止氧化。现有技术液氮冷却的液氮通道都是在模垫上,并且液氮通道与模具工作带有一定得距离,一般不小于40mm~50mm,这样造成冷却效果不理想。
发明内容
本实用新型为解决现有技术铝型材热挤压加工过程中,液氮冷却效果不好的技术问题,提供一种高效冷却铝型材热挤压模具结构,该结构的液氮冷却通道直接冷却到模具工作带处,可实现对模具工作带和模具出口型材的直接冷却,效果更佳。
为了达到上述目的,本实用新型所采用的技术方案是,提供一种高效冷却铝型材热挤压模具结构,它包括模具、模垫,在所述模垫的外沿上设置有液氮入口,在所述模垫与模具的接触面上设置有液氮通道,所述的液氮通道与所述的液氮入口连通;所述液氮通道的出口导入所述的模具;在所述模具上与液氮通道出口对应的位置设计有液氮导入孔,所述液氮导入孔通向所述模具的工作带。
进一步的,所述液氮通道在模垫与模具接触面部分为螺旋形。
进一步的,所述模具上的液氮导入孔与模具工作带的距离为10mm~20mm。
本实用新型与现有技术相比较,其效果是积极和明显的。首先通过在模具上的液氮导入孔,将液氮导入模具工作带附近,更充分的完成对模具工作带和模具出口型材的冷却;另外本实用新型中的液氮冷却通道为螺旋形,增加了液氮与模垫和模具的接触面积,使液氮更好的在模垫和模具接触面之间流动,更充分的实现了对模具的冷却,增加了模具的强度,提高了模具的寿命。
附图说明
图1是现有技术铝型材热挤压模具的模垫结构示意图;
图2是现有技术铝型材热挤压模具的模具结构示意图;
图3是现有技术铝型材热挤压模具与模垫的装配图;
图4是本实用新型高效冷却铝型材热挤压模具的模垫结构示意图;
图5是本实用新型高效冷却铝型材热挤压模具的模具结构示意图;
图6是本实用新型高效冷却铝型材热挤压模具与模垫的装配图。
具体实施方式
下面结合附图对本实用新型做进一步的说明。
如图1、图2所示,现有技术铝型材热挤压模具在模垫1上设置液氮入口3,液氮通道4设置在模垫1上,并通向模垫1与模具2的接触面。如图3所示,液氮通道4的出口与模具工作带5有一定距离,不利于冷却。
如图4、图5所示,本实用新型在模垫11的外沿上设置有液氮入口13,液氮通道14和液氮入口13连通;液氮通道14在模垫11和模具12的接触面部分设计为螺旋形;液氮通道14的出口17导入模具12;模具12上与液氮通道14的出口17对应的位置设计有液氮导入孔16。
如图5、图6所示,液氮导入孔16通向模具的工作带15;液氮导入口16距离模具工作带15的距离为10mm~20mm。

Claims (3)

1.一种高效冷却铝型材热挤压模具结构,它包括模具、模垫,其特征在于:在所述模垫的外沿上设置有液氮入口,在所述模垫与模具的接触面上设置有液氮通道,所述的液氮通道与所述的液氮入口连通;所述液氮通道的出口导入所述的模具;在所述模具上与液氮通道出口对应的位置设计有液氮导入孔,所述液氮导入孔通向所述模具的工作带。
2.如权利要求1所述的一种高效冷却铝型材热挤压模具结构,其特征在于:所述液氮通道在模垫与模具接触面部分为螺旋形。
3.如权利要求1或2所述的一种高效冷却铝型材热挤压模具结构,其特征在于:所述模具上的液氮导入孔与模具工作带的距离为10mm~20mm。
CN2009202736870U 2009-11-24 2009-11-24 一种高效冷却铝型材热挤压模具结构 Expired - Fee Related CN201565485U (zh)