CN201322613Y - 连铸结晶器保护渣渣层厚度测量装置 - Google Patents

连铸结晶器保护渣渣层厚度测量装置 Download PDF

Info

Publication number
CN201322613Y
CN201322613Y CNU2008202146347U CN200820214634U CN201322613Y CN 201322613 Y CN201322613 Y CN 201322613Y CN U2008202146347 U CNU2008202146347 U CN U2008202146347U CN 200820214634 U CN200820214634 U CN 200820214634U CN 201322613 Y CN201322613 Y CN 201322613Y
Authority
CN
China
Prior art keywords
slag
stainless
longest
steel pipe
measuring device
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008202146347U
Other languages
English (en)
Inventor
吴建永
朱定华
董�成
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanjing Iron and Steel United Co Ltd
Original Assignee
Nanjing Iron and Steel United Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing Iron and Steel United Co Ltd filed Critical Nanjing Iron and Steel United Co Ltd
Priority to CNU2008202146347U priority Critical patent/CN201322613Y/zh
Application granted granted Critical
Publication of CN201322613Y publication Critical patent/CN201322613Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种渣层厚度测量装置,是连铸结晶器保护渣渣层厚度测量装置,包括一个由三根不锈钢管焊接成的直角支架和镀铜的铁丝,第二长的不锈钢钢管位于最长的不锈钢钢管的中间,最短的不锈钢钢管位于最长的不锈钢钢管的中上方。铁丝穿过直角支架中最长的不锈钢钢管,然后插入结晶器中钢水内。等铁丝头熔断后,撤除测量装置,用卷尺量出测量距离。本实用新型结构简单,使用方便,采用本实用新型的测量装置,随时都能够精确掌握保护渣渣层的厚度和钢液面的稳定性。

Description

连铸结晶器保护渣渣层厚度测量装置
技术领域
本实用新型涉及一种渣层厚度测量装置,具体的说是连铸结晶器保护渣渣层厚度测量装置。
背景技术
连铸是钢铁企业质量控制的关键过程之一,高效、低耗生产无缺陷的铸坯是连铸的最高目标。在连铸生产过程中,除了配备相应的工艺设备及合适的工艺参数外,还要在生产过程中时刻对水口等耐材使用状况进行监控,尤其是结晶器保护渣渣层厚度保持在一个合适的范围内,否则会引起铸坯洁净度降低及表面质量和内部质量恶化,甚至在生产过程中造成漏钢事故。连铸一般采用浸入式水口(内装水口)加保护渣浇铸来提高铸坯的质量,水口和保护渣对液面测量有影响,保护渣厚度的精确测量一直是一个难题。在生产过程中由于侵入式水口摆放不正或保护渣添加过多等原因都会直接影响结晶器内的钢水液面高度。现有技术中通常都是通过目测或用捞渣棒探钢水液面高度,但是无法准确的判断出保护渣的添加厚度。水口插入过深,造成结晶器内热区下移,影响钢的内部质量而且造成化渣不良影响铸坯的表面质量。以及钢水超过水口内含锆层会加快钢水对侵入式水口的侵蚀,这样会造成水口过早熔断,易卷渣造成漏钢同时也严重影响了连铸的连浇炉数和铸坯的内部质量。保护渣添加过多会造成水口插入过浅,易卷渣,造成铸坯洁净度降低。保护渣添加过少,会造成钢水二次氧化,产生氧化渣,易造成漏钢同时也严重影响了连铸的连浇炉数和铸坯的内部质量。因些,现有技术中没有一种精确测量结晶器内保护渣渣层厚度的装置。
发明内容
本实用新型所要解决的技术问题是:针对以上现有技术存在的缺点,提出一种可精确测量结晶器内保护渣渣层厚度的测量装置。
本实用新型解决以上技术问题的技术方案是:连铸结晶器保护渣渣层厚度测量装置,包括一个由三根不锈钢管焊接成的直角支架和镀铜的铁丝,直角支架中最长的一根不锈钢钢管竖直设置,两根短的不锈钢钢管水平设置,分别位于最长的不锈钢钢管的两边,铁丝穿过直角支架中最长的一根不锈钢钢管。
第二长的不锈钢钢管位于最长的不锈钢钢管的中间,最短的不锈钢钢管位于最长的不锈钢钢管的中上方。铁丝表面镀有铜。
本实用新型的优点是:本实用新型结构简单,使用方便,采用本实用新型的测量装置,随时都能够精确掌握保护渣渣层的厚度和钢液面的稳定性。
附图说明
图1是本实用新型的结构示意图。
图2是本实用新型的使用状态图。
具体实施方式
实施例一
本实施例是一种连铸结晶器保护渣渣层厚度测量装置,其结构如图1所示,包括一个由三根不锈钢管焊接成的直角支架和镀铜的铁丝4,第二长的不锈钢钢管2位于最长的不锈钢钢管1的中间,最短的不锈钢钢管3位于最长的不锈钢钢管的1中上方。铁丝4穿过直角支架中最长的不锈钢钢管1,然后插入结晶器中钢水内。等铁丝4头熔断后,撤除测量装置,用卷尺量出测量距离。
本实用新型的使用状态如图2所示,本实施新型在具体测量时,第一步必须将结晶器内的保护渣渣带捞取干净,在捞取结晶器内的保护渣渣带的过程中,顺便用捞渣棒大概探一下保护渣的厚度;第二步将镀铜的细铁丝4穿过直角支架中最长的一根不锈钢钢管1,测算好铁丝4的长度;第三步将测量装置中最短的一根不锈钢管3搭在正在浇注的浸入式水口碗口边缘,将最长的一根不锈钢钢管1内的细铁丝4插入结晶器钢水中。然后取出,根据铁丝4发红的部位,水口的尺寸和铁丝4的长度,用卷尺测量其长度就能够精确的测算出保护渣渣层的厚度,及时做出调整,否则会引起铸坯洁净度降低及表面质量和内部质量恶化,甚至在生产过程中造成漏钢事故。
本实用新型还可以有其它实施方式,凡采用同等替换或等效变换形成的技术方案,均落在本实用新型要求保护的范围之内。

Claims (3)

1.连铸结晶器保护渣渣层厚度测量装置,其特征在于:包括一个由三根不锈钢管焊接成的直角支架和镀铜的铁丝,所述直角支架中最长的一根不锈钢钢管竖直设置,两根短的不锈钢钢管水平设置,分别位于最长的不锈钢钢管的两边,所述铁丝穿过直角支架中最长的一根不锈钢钢管。
2.如权利要求1所述的连铸结晶器保护渣渣层厚度测量装置,其特征在于:所述第二长的不锈钢钢管位于最长的不锈钢钢管的中间,所述最短的不锈钢钢管位于最长的不锈钢钢管的中上方。
3.如权利要求1所述的连铸结晶器保护渣渣层厚度测量装置,其特征在于:所述铁丝是表面镀铜的铁丝。
CNU2008202146347U 2008-12-23 2008-12-23 连铸结晶器保护渣渣层厚度测量装置 Expired - Fee Related CN201322613Y (zh)