CN201288206Y - 钢包喂线枪 - Google Patents

钢包喂线枪 Download PDF

Info

Publication number
CN201288206Y
CN201288206Y CNU2008203014542U CN200820301454U CN201288206Y CN 201288206 Y CN201288206 Y CN 201288206Y CN U2008203014542 U CNU2008203014542 U CN U2008203014542U CN 200820301454 U CN200820301454 U CN 200820301454U CN 201288206 Y CN201288206 Y CN 201288206Y
Authority
CN
China
Prior art keywords
steel
steel pipe
feeding
wire
ladle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008203014542U
Other languages
English (en)
Inventor
王明春
关春立
李林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNU2008203014542U priority Critical patent/CN201288206Y/zh
Application granted granted Critical
Publication of CN201288206Y publication Critical patent/CN201288206Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种冶金工具,即钢包喂线枪。它包括一个钢管,钢管下部一段箍有耐火材料保护层。钢管上部带有进气口,用于通入惰性气体,保持抢孔的畅通并不粘钢。采用本装置把喂线插入离钢液面约2米的深度,喂线枪通入惰性气体(通常是氩气)用于保持抢孔的畅通并不粘钢。采用耐火材料保护插入钢水中的钢管,实现向钢水深部送线,提高使用寿命。具有提高钙的收得率,利于环境保护,提高钢材产品质量的特点。

Description

钢包喂线枪
技术领域
本实用新型涉及一种冶金工具,即钢包喂线枪。
背景技术
在已有技术中,钢包冶金过程中普遍采用喂线机喂线工艺,通过喂线导管在钢水液面上方500mm高度将包芯线以一定的速率喂入钢水中,包芯线在穿过渣层进入钢水的过程中,在渣层以及炉渣空气界面发生强烈的汽化反应,导致合金芯粉烧损一部分,同时产生燃烧粉尘污染空气。在喂入金属钙等易氧化合金时,情况更为严重,钙线在钢水表面剧烈燃烧产生大量白色烟气污染空气,金属钙的收得率仅为7%左右。
实用新型内容
本实用新型的目的是针对上述不足而提供一种把喂线方便插入钢水中并使用可靠的钢包喂线枪。
本实用新型的技术解决方案是:钢包喂线枪包括一个钢管,钢管下部一段箍有耐火材料保护层。钢管上部带有进气口,用于通入惰性气体(通常是氩气),保持抢孔的畅通并不粘钢。喷枪喂线工艺的独特设计可以通过钢包喂线枪(耐火喷枪)把包芯线喂至钢水中钙汽化的临界深度以下的理想区域,在这里包芯线与钢液直接接触而不接触氧化性强的炉渣和空气,避免了包芯线与炉渣和空气之间的直接氧化烧损,使包芯线可以很好地溶解。极大地提高了包芯线收得率,同时不会产生燃烧烟气,减轻了对大气的污染。在液态下,钙珠由于其比重较小而在钢液中上浮。在汽态下,钙则以更快的速度上升。钙的汽化受到温度和压力的影响,当其在钢包内的深度足够时,从理论上说钢水静压力将抑制钙的汽化相变。采用本装置把喂线插入离钢液面约2米的深度,喂线枪通入惰性气体(通常是氩气)用于保持抢孔的畅通并不粘钢。惰性气体从枪孔喷射出,在钢包内形成一种环流状态,然后借助于机械喂线方式把钙线通过喷枪孔射入钢包,直到进入钢液中约1秒后溶解,包芯线在穿过喷枪孔后依靠其驱动速度可以继续向下穿行一段距离,浮力使包芯线下行受阻发生横向位移。由于喷枪将钙线喂至钢水中钙汽化临界深度以下的理想区域,在这里钙可以很好地溶解到钢液里。钙的使用效率平均提高了180%。
本实用新型的优点是:1、采用耐火材料保护插入钢水中的钢管,实现向钢水深部送线,提高使用寿命。2、送线同时采用通入保护气体,提高钢包喂线枪使用性能,喂线可靠。3、提高钙的收得率,利于环境保护,提高钢材产品质量,并取得了显著的综合经济效益。
下面将结合附图对本实用新型的实施方式作进一步详细描述。
附图说明
附图是本实用新型结构简图。
具体实施方式
参见附图,钢包喂线枪包括一个钢管1,钢管1下部一段箍有耐火材料保护层2。钢管1上部带有进气口3。枪体浇注耐火材料主料选用Al2O3SiO2系材质,以优质高铝矾土熟料及刚玉为主料,加入适量的热震稳定性好的基质原料,采用超微粉技术,添加高效外加剂和合理的颗粒级配,使组织结构达到致密。因此抗热震能力好,不产生穿孔、开裂、蚀损剥落等现象,进而保护喂线钢管内蕊,提高枪的使用寿命。
箍有耐火材料保护层2的钢管1表面上分布焊接有凸出的金属柱4,增加耐火材料保护层2的附着能力。
箍有耐火材料保护层2的钢管1为变径结构,钢管下部直径小,上部直径大,更利于喂线。

Claims (3)

  1. 【权利要求1】一种钢包喂线枪,其特征在于包括一个钢管(1),钢管(1)下部一段箍有耐火材料保护层(2),钢管(1)上部带有进气口(3)。
  2. 【权利要求2】按照权利要求1所述的钢包喂线枪,其特征在于箍有耐火材料保护层(2)的钢管(1)表面上分布焊接有凸出的金属柱(4)。
  3. 【权利要求3】按照权利要求1或2所述的钢包喂线枪,其特征在于箍有耐火材料保护层(2)的钢管(1)为变径结构,钢管下部直径小,上部直径大。
CNU2008203014542U 2008-07-07 2008-07-07 钢包喂线枪 Expired - Fee Related CN201288206Y (zh)