CN201256163Y - 锂电池阳极 - Google Patents

锂电池阳极 Download PDF

Info

Publication number
CN201256163Y
CN201256163Y CNU2008201901310U CN200820190131U CN201256163Y CN 201256163 Y CN201256163 Y CN 201256163Y CN U2008201901310 U CNU2008201901310 U CN U2008201901310U CN 200820190131 U CN200820190131 U CN 200820190131U CN 201256163 Y CN201256163 Y CN 201256163Y
Authority
CN
China
Prior art keywords
lithium
copper foil
affluxion body
anode
band
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008201901310U
Other languages
English (en)
Inventor
余章华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhan boesel Power Technology Co. Ltd.
Original Assignee
Wuhan Supercell Science & Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan Supercell Science & Technology Co Ltd filed Critical Wuhan Supercell Science & Technology Co Ltd
Priority to CNU2008201901310U priority Critical patent/CN201256163Y/zh
Application granted granted Critical
Publication of CN201256163Y publication Critical patent/CN201256163Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种锂电池阳极,它包括锂带,锂带一侧表面敷设的导电胶,导电胶粘结连接集流体铜箔。所述集流体铜箔厚度为8μm~50μm。由于铜箔很薄,所以这种结构几乎不影响电池的尺寸。或者说在同样尺寸下,可以设计更高的容量。可以有效的防止锂带断裂带来的问题,又不会产生粉末状金属锂沉积的问题。工艺简单可靠,易操作。

Description

锂电池阳极
技术领域
本实用新型属于锂电池,具体涉及一种锂电池阳极。
背景技术
一次锂电池(尤其是圆柱式和方形电池)中的阳极锂片在放电后期容易断裂,形成彼此没有连接的小片。这些小片一旦不能与极耳相连,就不能再参与阳极反应,从而导致这部分活性物质不能被利用,电池的容量不能充分发挥,造成电池提前失效。为了解决这个问题,目前有几种方法被使用:
第一种方法是在锂片的一个表面上贴一层胶带,由于胶带没有微孔,从而阻止了被胶带覆盖部分的金属锂参与反应,在放电后期,这一部分金属锂可以防止锂带完全断开。
这种方法工艺简单,但却带来两个负面影响,一是由于被胶带覆盖的部分在正常放电情况下不能反应,使锂片的实际反应面积减小,降低了电池的设计容量。虽然为了减小这种负面影响,一般设计胶带的宽度尽可能小,但对于小型电池而言,这种影响仍然是不可忽略的。另一个负面影响是当这种电池被强制放电时,被胶带覆盖的锂会通过另一面发生反应,并在阴极相应的区域沉积成粉末状的金属锂。这种粉末状的金属锂化学活性非常大,是造成电池起火爆炸的主要原因之一。
第二种方法是使用过量的金属锂,这种方法的主要缺点是在强制放电时,容易在阴极沉积粉末状的金属锂,从而降低电池的安全性能。
第三种方法是在金属锂片的一面复合一层不锈钢带,制作电池时只有另一面与阴极相对,不锈钢带作为集流体。这种方法的缺点是工艺复杂,不锈钢带的厚度较大,降低了电池的设计容量。
另外还有用金属丝嵌入锂带中的方法,缺点也是工艺较复杂。
发明内容
本实用新型的目的在于提供一种不易断裂工艺简单的锂电池阳极,以解决上述问题。
实现本实用新型的目的的技术方案为:锂电池阳极,它包括锂带,锂带一侧表面敷设的导电胶,导电胶粘结连接集流体铜箔。
所述集流体铜箔厚度为8μm~50μm。
所述集流体铜箔长度与锂带长度相同,集流体铜箔宽度小于锂带宽度。
采用本方案有以下优点:
由于铜箔很薄,所以这种结构几乎不影响电池的尺寸。或者说在同样尺寸下,可以设计更高的容量。可以有效的防止锂带断裂带来的问题,又不会产生粉末状金属锂沉积的问题。工艺简单可靠,易操作。
附图说明
图1锂电池阳极结构I示意图。
图2图1的俯视示意图。
图3锂电池阳极结构II示意图。
图4锂电池阳极结构III IV示意图。
图5锂电池阳极结构IV示意图。
具体实施方式
实施例1
如图12所示,锂带10为平面锂带,锂带10表面设有极耳12。锂带10及极耳12表面敷设的导电胶13,导电胶13粘结连接集流体铜箔14。集流体铜箔14长度与锂带10长度可以相同,集流体铜箔宽度与锂带宽度可以相同;集流体铜箔长度与锂带长度可以相同,集流体铜箔宽度也可以小于锂带宽度。本实施例中集流体铜箔宽度小于锂带宽度,这样实施比较容易,也有良好的防断裂效果。
实施例2
它是阳极将阴极包住的结构。如图3所示,锂带20通过隔膜21将阴极22包住;锂带20表面敷设的导电胶23,导电胶23粘结连接集流体铜箔24。
实施例3
它是阳极不对称折叠结构。如图4所示,集流体铜箔34表面设有导电胶33,可以是集流体铜箔34一个表面也可以是集流体铜箔34的两个表面。本实施例中为集流体铜箔34一个表面设有导电胶33,锂带30通过导电胶33粘接与集流体铜箔34连接,锂带30折叠后与集流体铜箔34压紧,折叠后锂带30一面的长度小于集流体铜箔34的长度,形成不对称折叠结构。锂带30与阴极32之间设隔膜31。
实施例4
它是阳极对称折叠的结构。如图5所示,集流体铜箔44表面设有导电胶43,可以是集流体铜箔44一个表面也可以是集流体铜箔44的两个表面。本实施例中为集流体铜箔44一个表面设有导电胶43,锂带40通过导电胶43粘接与集流体铜箔44连接,锂带40折叠后与集流体铜箔44压紧,折叠后锂带30一面的长度与集流体铜箔34的长度相同,形成对称折叠结构。锂带40与阴极42之间设隔膜41。
上述实施例的集流体铜箔厚度为8μm~50μm。上述导电胶可以是含碳或者银粉等导电材料的聚合物胶层,聚合物种类可以是聚丙烯酸酯,聚氨酯等高分子化合物。

Claims (6)

1、一种锂电池阳极,它包括锂带,其特征在于锂带一侧表面敷设的导电胶,导电胶粘结连接集流体铜箔。
2、如权利要求1所述锂电池阳极,其特征在于锂带表面与导电胶之间设置极耳。
3、如权利要求1所述锂电池阳极,其特征在于锂带折叠呈至少两层,锂带的折叠层之间设集流体铜箔,集流体铜箔一个表面或两个表面上敷设有导电胶,导电胶与锂带粘接。
4、如权利要求1所述锂电池阳极,其特征在于集流体铜箔长度与锂带长度相同,集流体铜箔宽度与锂带宽度相同。
5、如权利要求1所述锂电池阳极,其特征在于集流体铜箔宽度小于锂带宽度。
6、如权利要求1所述锂电池阳极,其特征在于集流体铜箔厚度为8μm~50μm。
CNU2008201901310U 2008-08-07 2008-08-07 锂电池阳极 Expired - Fee Related CN201256163Y (zh)