CN201244648Y - 油井管一次镦粗加厚装置 - Google Patents
油井管一次镦粗加厚装置 Download PDFInfo
- Publication number
- CN201244648Y CN201244648Y CNU2008200313612U CN200820031361U CN201244648Y CN 201244648 Y CN201244648 Y CN 201244648Y CN U2008200313612 U CNU2008200313612 U CN U2008200313612U CN 200820031361 U CN200820031361 U CN 200820031361U CN 201244648 Y CN201244648 Y CN 201244648Y
- Authority
- CN
- China
- Prior art keywords
- oil well
- jumping
- thickening
- well pipe
- heating furnace
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了油井管一次镦粗加厚装置,该油进管为60.3×4.83型,间隔式分布的送料机(1)贯穿依次安装的一号加热炉(2)、一号镦粗加厚机(3)、二号加热炉(4)和二号镦粗加厚机(5),在支架(6)上安装送料辊(7)通过电机(8)单辊传动;所述的加热炉由电源(9)、加热感应线圈(10)组成,在炉膛内安装连接电源(11)的加热感应线圈(10),在机架(11)的一端安装冲头(12),在机架(11)的另一端相对冲头(12)位置安装模板(13),两块模板(13)形成的成型腔(15)的顶端安装定位块(14)。本实用新型机械化作业,油井管两端实现一次镦粗加厚,加工时间短,劳动强度低,工作效率高,产品合格率99%。
Description
技术领域
本实用新型涉及加工机械,具体涉及油井管一次镦粗加厚装置。
背景技术
随着国际经济的发展,石油、天然气的需求不断扩大,一些油层深度较深的油井也开始进行开采,用于深井的油井管为了连接的稳定需要镦粗加厚,尤其是60.3×4.83油管由于壁厚薄、加厚过程中金属流量不足,一次加厚合格率过低,目前行业内生产采用二次加厚成型工艺,工人劳动强度大,工作效率低。
发明内容
本实用新型的目的在于:提供一种油井管一次镦粗加厚装置,采用镦粗加厚装置将60.3×4.83型油管一次镦粗加厚成型,降低工人劳动强度,缩短加工时间,提高工作效率,保证产品质量。
本实用新型的技术解决方案是:该镦粗加厚装置包括送料机、加热炉和镦粗加厚机,间隔式分布的送料机贯穿依次安装的一号加热炉、一号镦粗加厚机、二号加热炉和二号镦粗加厚机,所述的送料机由支架、送料辊、电机组成,在支架上安装送料辊通过电机单辊传动;所述的加热炉由电源、加热感应线圈组成,在炉膛内安装连接电源的加热感应线圈;所述的镦粗加厚机由机架、冲头、模板、定位块组成,在机架的一端安装冲头,在机架的另一端相对冲头位置安装模板,两板模板形成的成型腔的顶端安装定位块。
镦粗加厚时,首先,将60.3×4.83型油井管通过送料机输送到一号加热炉加热油井管的其中一加厚端;其次,通过送料机将油井管加厚端送到镦粗加厚机,油井管的被加热的加厚端放置成型腔内通过模板和定位块夹持定位,冲头穿过油井管锻压被加热的加厚端直至工艺设计要求的厚度;然后,拉出冲头,油井管经送料机输送到二号加热炉加热油井管的另一端,通过二号镦粗加厚机锻压加厚油井管另一端的加厚端;最后,两端被镦粗加厚的油井管通过送料机输送到下料台。
本实用新型机械化作业,60.3×4.83型油井管两端实现一次镦粗加厚,加工时间短,劳动强度低,工作效率高,产品质量好。
附图说明
图1为本实用新型生产流程结构示意图。
图2为图1的送料机结构示意图。
图3为图1的加热炉结构示意图。
图4为图1的镦粗加厚机结构示意图。
图中:1.送料机,2.一号加热炉,3.一号镦粗加厚机,4.二号加热炉,5.二号镦粗加厚机,6.支架,7.送料辊,8.电机,9.电源,10.加热感应线圈,11.机架,12.冲头,13.模板,14.定位块,15.成型腔。
具体实施方式
如图1-4所示,该镦粗加厚装置包括送料机、加热炉和镦粗加厚机,间隔式分布的送料机1贯穿依次安装的一号加热炉2、一号镦粗加厚机3、二号加热炉4和二号镦粗加厚机5,所述的送料机由支架6、送料辊7、电机8组成,在支架6上安装送料辊7通过电机8单辊传动;所述的加热炉由电源9、加热感应线圈10组成,在炉膛内安装连接电源11的加热感应线圈10,所述的镦粗加厚机由机架11、冲头12、模板13、定位块14组成,在机架11的一端安装冲头12,在机架11的另一端相对冲头12位置安装模板13,两块模板13形成的成型腔15的顶端安装定位块14。
镦粗加厚时,首先,60.3×4.83型油井管通过送料机1输送到一号加热炉2加热油井管的其中一加厚端;其次,通过送料机1将油井管加厚端送到镦粗加厚机3,油井管的被加热的加厚端放置成型腔15内通过模板13和定位块14夹持定位,冲头12穿过油井管锻压被加热的加厚端直至工艺设计要求的厚度;然后,拉出冲头12,油井管经送料机1输送到二号加热炉4加热油井管的另一端,通过二号镦粗加厚机5锻压加厚油井管另一端的加厚端;最后,两端被镦粗加厚的油井管通过送料机输送到下料台。
Claims (1)
1.油井管一次镦粗加厚装置,其特征在于:油井管为60.3×4.83型,该镦粗加厚装置包括送料机、加热炉和镦粗加厚机,间隔式分布的送料机(1)贯穿依次安装的一号加热炉(2)、一号镦粗加厚机(3)、二号加热炉(4)和二号镦粗加厚机(5),所述的送料机由支架(6)、送料辊(7)、电机(8)组成,在支架(6)上安装送料辊(7)通过电机(8)单辊传动;所述的加热炉由电源(9)、加热感应线圈(10)组成,在炉膛内安装连接电源(11)的加热感应线圈(10),所述的镦粗加厚机由机架(11)、冲头(12)、模板(13)、定位块(14)组成,在机架(11)的一端安装冲头(12),在机架(11)的另一端相对冲头(12)位置安装模板(13),两块模板(13)形成的成型腔(15)的顶端安装定位块(14)。