CN201239759Y - 一种镶嵌轻质合金陶瓷的拉伸挤压模具 - Google Patents
一种镶嵌轻质合金陶瓷的拉伸挤压模具 Download PDFInfo
- Publication number
- CN201239759Y CN201239759Y CNU2008200087912U CN200820008791U CN201239759Y CN 201239759 Y CN201239759 Y CN 201239759Y CN U2008200087912 U CNU2008200087912 U CN U2008200087912U CN 200820008791 U CN200820008791 U CN 200820008791U CN 201239759 Y CN201239759 Y CN 201239759Y
- Authority
- CN
- China
- Prior art keywords
- light weight
- ceramal
- die
- stretching
- ceramic body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种镶嵌轻质合金陶瓷的拉伸挤压模具,主体是常规铬钢或45钢的基体,其特征在于:在基体内壁的工作面上开有阶梯槽孔,阶梯槽孔的槽上镶嵌有轻质合金陶瓷体,轻质合金陶瓷体上形成有用于拉伸、挤压的工作面,且阶梯槽孔的槽与轻质合金陶瓷体之间以1-2°的锥度紧密配合,这样的设计,以陶瓷材料为主的一种耐磨,耐热,耐酸碱的材料替代硬质合金,在增加模具使用寿命的同时,节约稀有、贵重金属材料。
Description
技术领域
本实用新型涉及五金加工模具的领域,特别是用于拉伸、挤压成型的模具。
背景技术
传统的五金加工成型模具主要是用优质的铬钢作基体的,但在上下模的巨大压力和拉伸、挤压间巨大的摩擦力作用下,使得模具的使用寿命不高,在15-20万次左右。随着技术的进步、发展,人们研制出硬质合金,其使用寿命可达100-300万次左右,但硬质合金在整个模具上应用是不可取的。硬质合金主要是以金属钨和各种稀有金属经过混和后压制、烧结而成的一种用于五金模具、陶瓷模具和耐磨件上的硬质耐磨材料。这种硬质合金是主要以钨为原料,因为钨为当今的一种稀有的金属,现在我国的含量急剧地下降,含钨量不断的减少,所以造成钨的价格不断的攀升。在硬质合金的其它配方上,也要用到多种稀有金属,这给我国的资源合理利用带来了不利的影响,浪费了我国的稀有金属资源。虽然这样的硬质合金模具的寿命得到明显的提高,但其生产成本,材料成本却极高,也造成贵重材料的浪费。
实用新型内容
本实用新型的目的就是要克服现有技术的不足之处,提出一种在增加模具寿命的同时,节约原材料成本,而使用寿命长,成本低,效益高的镶嵌轻质合金陶瓷的拉伸挤压模具。
本实用新型的目的是通过如下技术方案实现的:一种镶嵌轻质合金陶瓷的拉伸挤压模具,主体是常规铬钢或45钢的基体,其特征在于:在基体内壁的工作面上开有阶梯槽孔,阶梯槽孔的槽上镶嵌有轻质合金陶瓷体,轻质合金陶瓷体上形成有用于拉伸、挤压的工作面,且阶梯槽孔的槽与轻质合金陶瓷体之间以1--2°的锥度紧密配合。进一步地,轻质合金陶瓷体是包含有氧化锆30%-70%,氧化铝5%-30%,氧化铁3%-10%,氧化镍3%-15%,氧化铜1%-3%。的烧结合成轻质陶瓷体。且基体与轻质合金陶瓷体之间还可由粘合剂和热胀冷缩来固定。
这样的设计,本实用新型具有明显的优点和优势:
1.陶瓷体质轻而耐磨性能高,使用冲次可达150-300万次。
2.减少了模芯磨损而更换模具的次数,减轻劳动强度。
3.保证了产品的尺寸质量。
4.节约了贵重、稀有金属,使模具的生产成本有较大的降低。
5.轻质合金陶瓷具有很好的耐热性,在拉伸模具使用时不需要添加拉伸油,这也大大的减低了厂家的成本。不用添加拉伸油,这就节约了工时,提高了生产效率。不用添加拉伸油,这就不用使用后清洗了,这样就不会给环境带来污染了。
附图说明
图1是本实用新型的主视示意图;
图2是图1的侧视示意图;
图3是实施例二的主视示意图;
图4是图3的侧视示意图。
具体实施方式
见图1和图2,本实施例是圆形拉伸成型模具(局部),基本组成包括:模具基体1和轻质合金陶瓷体2。基体1采用的是常规的45钢,特别之处是在基体1中央开有圆形的阶梯槽孔11,阶梯槽孔11的槽呈上窄下宽的锥形,其锥度为2°,而轻质合金陶瓷体2其上也具有阶梯槽孔11对应相同的2°锥度,轻质合金陶瓷体2装嵌于阶梯槽11内并与之形成紧密的配合。轻质合金陶瓷体2的中央为拉伸工作面21,拉伸工作面21为圆孔,并与阶梯槽孔11的孔对应。其中,轻质合金陶瓷体2是由氧化锆30%-70%,氧化铝5%-30%,氧化铁3%-10%,氧化镍3%-15%,氧化铜1%-3%烧结合成,其耐热、耐磨,可承受600—1000度的工作温度。
见图3和图4,实施例二是长方形的铜铝挤压成型模具(局部),基本组成包括:模具基体3和轻质合金陶瓷体4。基体3采用的是常规的铬钢,特别之处是在基体3中央开有长方形阶梯槽孔31,阶梯槽孔31的槽呈上窄下宽的锥形,其锥度为1°,而轻质合金陶瓷体4其上也具有阶梯槽孔31对应相同的1°锥度,轻质合金陶瓷体2装嵌于阶梯槽孔内并与之形成紧密的配合。轻质合金陶瓷体4的中央为拉伸工作面41,拉伸工作面41为长方形,并与阶梯槽孔31的孔对应。轻质合金陶瓷体4的材质与实施例一相同。
当然,这里仅列举了两种较佳的实施方式,其它等同、类同的构造均应属于本专利的保护范畴,这里不再赘述。
Claims (2)
1、一种镶嵌轻质合金陶瓷的拉伸挤压模具,主体是常规铬钢或45钢的基体,其特征在于:在基体内壁的工作面上开有阶梯槽孔,阶梯槽孔的槽上镶嵌有轻质合金陶瓷体,轻质合金陶瓷体上形成有用于拉伸、挤压的工作面,且阶梯槽孔的槽与轻质合金陶瓷体之间以1--2°的锥度紧密配合。
2、根据权利要求1所述的拉伸挤压模具,其特征是基体与轻质合金陶瓷体之间还可由粘合剂和热胀冷缩来固定。