CN201149776Y - 多层绝缘线 - Google Patents
多层绝缘线 Download PDFInfo
- Publication number
- CN201149776Y CN201149776Y CNU2007201792107U CN200720179210U CN201149776Y CN 201149776 Y CN201149776 Y CN 201149776Y CN U2007201792107 U CNU2007201792107 U CN U2007201792107U CN 200720179210 U CN200720179210 U CN 200720179210U CN 201149776 Y CN201149776 Y CN 201149776Y
- Authority
- CN
- China
- Prior art keywords
- layer
- insulation layer
- insulating barrier
- tin
- metal conductor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型所涉及一种多层绝缘线,其包括金属导体、第一绝缘层、第二绝缘层以及第三绝缘层,在金属导体与第一绝缘层之间设置有锡层。当进行软钎焊时,由于锡的熔点为230摄氏度,多层绝缘线浸泡在焊锡温度480摄氏度的锡液时,多层绝缘线上的锡层溶解于金属导体与第一绝缘层之间形成的容置空间内,使得第一绝缘层溶解后而剥离于金属导体,避免了在剥离绝缘层时所需要专用工具或者人手参与,从而达到提高生产效率的目的。同时,又因与现有同类产品的焊锡速度相比较,本实用新型中的焊层的速度比现有焊锡的速度快一倍左右,使得其可以达到快速焊锡的目的。另外,在使用该产品生产高频变压器等电器产品时,生产效率将大大提高,从而降低生产成本。
Description
【技术领域】
本实用新型涉及一种绝缘线,具体是指一种用于高频设备、线圈以及电路变压器的多层绝缘线。
【背景技术】
近几年来,为了适应高频设备的制作,绝大部分厂家为了改进导线的耐热性而采用高耐热性材料的绝缘层加工成绝缘线,该绝缘线虽然能够达到改进其耐热性,但是,剥离绝缘线连接终端的绝缘层十分困难。若采用化学或机械方式,则容易导致导体损伤或后续加工工序繁复。随后出现一种应用于变压器线圈内的三层绝缘线,该三层绝缘线中的绝缘层是由软钎焊的聚酯类耐热树脂和聚酰胺类树脂构成。所述的三层绝缘线虽然可以不剥除被绝缘层而直接进行软钎焊,但是,在设定焊锡温度为480摄氏度进行软钎焊时,由于绝缘层是耐热性树脂,在锡液中绝缘层溶解的速度慢,焊锡的时间长,导致长时间的高温焊锡容易损坏线圈架不利于连接。随后一些厂家采用电热剥皮钳进行剥除绝缘层,但是需要人手机械剥除绝缘层,导致生产效率低。
【实用新型内容】
本实用新型技术目的是为了解决上述现有技术存在不足的技术问题而提供一种可提高生产效率的多层绝缘线。
为实现上述技术目的,本实用新型所提供一种多层绝缘线,其包括金属导体、包裹于金属导体外围的第一绝缘层、包裹于第一绝缘层外围的第二绝缘层以及设置于第二绝缘层外围的第三绝缘层,在金属导体与第一绝缘层之间设置有锡层。
依据上述主要技术特征,所述的金属导体是由铜线构成的。
本实用新型的有益技术效果:因金属导体与第一绝缘层之间设置有锡层,当进行软钎焊的时,由于锡的熔点为230摄氏度,所述的多层绝缘线浸泡在焊锡温度480摄氏度的锡液的时,多层绝缘线上的锡层溶解于金属导体与第一绝缘层之间形成的容置空间内,使得第一绝缘层溶解后而剥离于金属导体,避免了在剥离所述的绝缘层时所需要专用工具或者人手参与,从而达到提高生产效率的目的。同时,又因与现有同类产品的焊锡速度相比较,本实用新型中的焊层的速度比现有焊锡的速度快一倍左右,即达到快速焊锡,从而达到提高生产效率的目的。
为对本实用新型的目的、构造特征及其功能有进一步的了解,兹配合附图详细说明如下:
【附图说明】
图1为本实用新型中多层绝缘线的立体图。
【具体实施方式】
请参阅图1所示,下面结合实施例来说明本实用新型所提供一种多层绝缘线,其包括金属导体1、包裹于金属导体1外围的第一绝缘层2、包裹于第一绝缘层2外围的第二绝缘层3以及设置于第二绝缘层3外围的第三绝缘层4,在金属导体1与第一绝缘层1之间涂覆有锡层5。
在本实施例中,所述的金属导体1是由铜线构成的。所述的第一绝缘层2、第二绝缘层3以及第三绝缘层4分别是由塑胶材料或者绝缘材料构成的。
当进行软钎焊的时,由于锡的熔点为230摄氏度,所述的多层绝缘线浸泡在焊锡温度480摄氏度的锡液的时,多层绝缘线上的锡层5溶解于金属导体1与第一绝缘层2之间形成的容置空间内,使得第一绝缘层2溶解后而剥离于金属导体1,避免了在剥离所述的绝缘层时所需要专用工具或者人手参与,又因与现有同类产品的焊锡速度相比较,本实用新型中的焊层的速度比现有焊锡的速度快一倍左右,即可达到快速焊锡,从而达到提高生产的效率的目的。
在本实施例中,所述的镀锡所增加成本不到总成本的1%,所述的绝缘层达到快速焊锡的效果,在绞合线(由预定数目的扭曲的多股绝缘线构成)焊锡的时候,优势更明显。
Claims (2)
1、一种多层绝缘线,其包括金属导体、包裹于金属导体外围的第一绝缘层、包裹于第一绝缘层外围的第二绝缘层以及设置于第二绝缘层外围的第三绝缘层,其特征在于:在金属导体与第一绝缘层之间设置有锡层。
2、如权利要求1所述的多层绝缘线,其特征在于:所述的金属导体是由铜线构成的。