CN201070665Y - 一种有加强板的铸铁钢渣罐 - Google Patents
一种有加强板的铸铁钢渣罐 Download PDFInfo
- Publication number
- CN201070665Y CN201070665Y CNU2007200839619U CN200720083961U CN201070665Y CN 201070665 Y CN201070665 Y CN 201070665Y CN U2007200839619 U CNU2007200839619 U CN U2007200839619U CN 200720083961 U CN200720083961 U CN 200720083961U CN 201070665 Y CN201070665 Y CN 201070665Y
- Authority
- CN
- China
- Prior art keywords
- cast iron
- steel slag
- slag tank
- tank
- stiffener
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种有加强板(1)的铸铁钢渣罐。适用于作业中因冷、热应力作用而易使翻转吊钩(2)的一面产生自上而下的纵向或横向或者斜向的裂纹、开裂等损坏缺陷的钢渣罐强化再生利用。它是用直径20mm的强化螺钉(4)把加强板(1)固定在翻转吊钩(2)所在的面,距离罐口(5)280mm~350mm,距离耳轴(3)两边棱线各800mm~1200mm的位置。对已有的钢渣罐根据缺陷的位置及长短采用不同尺寸的加强板。本实用新型延长使用寿命,降低了生产成本,经济效益测算:原来200万吨钢每年消耗60个铸铁钢渣罐,现在200万吨钢每年消耗20多个铸铁钢渣罐,收到了意料不到的效果。
Description
技术领域
本实用新型涉及一种用于装载钢渣的铸铁钢渣罐,尤其是适用于作业中因冷、热应力作用而易使翻转吊钩所在的一面产生自上而下的纵向或横向或者斜向的裂纹、开裂损坏缺陷的铸铁钢渣罐。
背景技术
在炼钢出渣作业中,当钢渣注入铸铁钢渣罐时,因为钢渣的温度很高造成激剧的热膨胀,加上起吊时又是在极高的温度下进行,处于热膨胀的过程中有热应力,还有起吊时的上升力和向中间的挤压力使得受力也不均匀;另一方面铸铁钢渣罐在铸造时工艺掌握不是很精确也造成罐壁厚薄不均匀。同时根据罐形设计,耳轴所在的两面和翻转吊钩所在的两面各自都是镜面对称,耳轴所在面的面积小,罐壁厚,而翻转吊钩所在面的面积大,罐壁薄。经多次反复使用就造成纵向自上而下的小裂纹,然后逐渐增大裂口,在这种情况下长时期使用也会造成横向或者斜向的裂纹。铸铁钢渣罐有时用一两次就要换一个新的,有时也可以使用一定时期,但都会给生产造成影响,使成本增加。
发明内容
本实用新型的目的就是要提供一种有加强板的铸铁钢渣罐,以增强翻转吊钩所在面的机械强度和抗热应力的强度,节约成本,提高效率。
本实用新型是这样来实现的:
因应力(包括热应力)局部过大造成的裂纹、开裂缺陷,起初是许多不容易看到的极细微、孤立的裂纹在力F的作用下逐步由小到大形成的,而且形成裂纹、开裂缺陷绝大多数是在翻转吊钩所在的面由罐口向下裂开。在新的铸铁钢渣罐制造好后在翻转吊钩所在的面距离罐口280mm~350mm,距离耳轴两边的棱线各800mm~1200mm的位置,由16锰钢或其他低合金钢制成的长度是1000mm~1100mm、宽度是250mm~300mm、厚度是12mm~18mm的加强板,用直径20mm的强化锣钉把加强板固定住。强化锣钉的长度根据铸铁钢渣罐壁的厚度确定,强化锣钉的形状是锣帽为六方形、锣纹状。固定的方法是:先用直径17.5mm的钻头在铸铁钢渣罐上钻孔然后攻丝,铸铁钢渣罐壁不钻穿,以保持罐内平滑不挂渣,然后拧紧强化锣钉。这样加固增大了机械强度,提高了抗应力的力度。对于已有裂纹、开裂缺陷的铸铁钢渣罐根据裂纹、开裂缺陷的位置及开裂程度和裂纹的长短采用不同尺寸的加强板一样可以加固重复使用。强化锣钉的数量和排列方式根据加强板的尺寸确定。
本实用新型是一种有加强板的铸铁钢渣罐,其优点是延长使用寿命,降低了生产成本,经济效益测算:原来200万吨钢每年消耗60个铸铁钢渣罐,现在200万吨钢每年消耗20多个铸铁钢渣罐,收到意料不到的效果。
附图说明
图1为本实用新型示意图
1——加强板 2——翻转吊钩 3——耳轴
4——强化锣钉 5——罐口
具体实施方案
结合附图1对本实用新型作进一步的详细描述。
在新的铸铁钢渣罐制造好后在翻转吊钩(2)所在的面,距离罐口(5)280mm~350mm,距离耳轴(3)两边棱线各800mm~1200mm的位置,由16锰钢或其他低合金钢制成的长度是1000mm~1100mm、宽度是250mm~300mm、厚度是12mm~18mm的加强板(1),用直径20mm的强化锣钉(4)把加强板(1)固定住。强化锣钉(4)的长度根据铸铁钢渣罐壁的厚度确定,强化锣钉(4)的形状是锣帽为六方形。固定的方法是:先用直径17.5mm的钻头在铸铁钢渣罐上先钻孔然后攻丝,铸铁钢渣罐壁不钻穿,保持罐内平滑不挂渣,然后拧紧强化锣钉(4)。这样加固后增大了机械强度,提高了抗应力的力度,对于已有裂纹、开裂缺陷的铸铁钢渣罐一样可以加固重复使用。
Claims (4)
1.一种有加强板(1)的铸铁钢渣罐,其特征在于加强板(1)是固定在新的钢渣罐翻转吊钩(2)所在的面,距离罐口(5)280mm~350mm,距离耳轴(3)两边棱线各800mm~1200mm的位置。
2.根据权利要求1所述的一种有加强板(1)的铸铁钢渣罐,其特征在于加强板(1)的长度是1000mm~1100mm、宽度是250mm~300mm、厚度是12mm~18mm。
3.根据权利要求1所述的一种有加强板(1)的铸铁钢渣罐,其特征在于加强板(1)的材质是16锰钢或其他低合金钢。
4.根据权利要求1所述的一种有加强板(1)的铸铁钢渣罐,其特征在于对已有裂纹的旧钢渣罐固定的加强板(1)是根据裂纹的位置及长度采用不同尺寸。