CN201032142Y - 用于锅炉水冷壁管的梳形防磨导流片 - Google Patents
用于锅炉水冷壁管的梳形防磨导流片 Download PDFInfo
- Publication number
- CN201032142Y CN201032142Y CNU2007200904181U CN200720090418U CN201032142Y CN 201032142 Y CN201032142 Y CN 201032142Y CN U2007200904181 U CNU2007200904181 U CN U2007200904181U CN 200720090418 U CN200720090418 U CN 200720090418U CN 201032142 Y CN201032142 Y CN 201032142Y
- Authority
- CN
- China
- Prior art keywords
- cooling wall
- water cooling
- utility
- model
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种用于锅炉水冷壁管的梳形防磨导流片,包括与所述水冷壁固连在一起的防磨片,所述防磨片的一边开设有多个与水冷壁管外径相对应的内凹槽。为增加水冷壁管与防磨片之间的连接强度,所述内凹槽的侧角处为弧形过渡。本实用新型的优点在于按照需要将多片一边开设有多个与水冷壁管外径相对应的内凹槽的梳形防磨导流片焊接在水冷壁的侧面,使用中可以降低物料颗粒沿水冷壁管下落的终端速度,隔离物料流与水冷壁管接触,破坏物料流在不平滑管壁处形成的涡流,减少物料粒子与水冷壁管的碰撞,从而避免固体物料对水冷壁管的磨损,尤其是浇注料过渡区,不需要再采用其他任何防磨措施,对水冷壁管的防磨起到标本兼治的作用。
Description
技术领域
本实用新型涉及用于锅炉水冷壁管的防磨片,尤其是涉及用于锅炉水冷壁管的梳形防磨导流片。
背景技术
随着国内外经济的迅速发展,工业企业大量需求热源和电力资源,促使硫化床燃烧技术得到了很快的发展,目前循环流化床锅炉越来越成熟,容量也越来越大。电厂要实现安全经济运行,决定于循环流化床锅炉的连续运行周期,其根本问题是提高锅炉设备的可靠性和可用率。锅炉四面垂直墙(管子)组成的垂直水冷壁(管排)是锅炉重要的受热面,水冷壁管的磨损是锅炉磨损最严重的部位,水冷壁管因各种因素造成管壁不平滑,阻碍了炉膛内循环中的固体物料流沿水冷壁面向下运动,物料流向改变后与上行的烟气流形成局部涡流,与金属受热面碰撞形成磨损,所以解决好水冷壁管的磨损问题是保证锅炉高效运行的重要条件之一。
目前,多数电厂对循环流化床锅炉水冷壁管的防磨仍采用较原始的防护处理技术,如采用浇注料防磨、加焊防磨护瓦、水冷壁管喷涂处理等,这些防护措施只能治标,不能治本,即防磨措施做到哪个部位,哪个部位的端部重新产生磨损现象,不能从根本上解决水冷壁管的磨损问题。
实用新型内容
本实用新型的目的在于提供一种可对水冷壁管形成有效防护的用于锅炉水冷壁管的梳形防磨导流片。
为实现上述目的,本实用新型可采取下述技术方案:
本实用新型所述的用于锅炉水冷壁管的梳形防磨导流片,包括与所述水冷壁固连在一起的防磨片,所述防磨片的一边开设有多个与水冷壁管外径相对应的内凹槽。
为增加水冷壁管与防磨片之间的连接强度,所述内凹槽的侧角处为弧形过渡。
本实用新型的优点在于按照需要将多片一边开设有多个与水冷壁管外径相对应的内凹槽的梳形防磨导流片焊接在水冷壁的侧面,使用中可以降低物料颗粒沿水冷壁管下落的终端速度,隔离物料流与水冷壁管接触,破坏物料流在不平滑管壁处形成的涡流,减少物料粒子与水冷壁管的碰撞,从而避免固体物料对水冷壁管的磨损,尤其是浇注料过渡区,不需要再采用其他任何防磨措施,对水冷壁管的防磨起到标本兼治的作用。
附图说明
图1是本实用新型的结构示意图。
图2、图3为本实用新型的安装位置示意图。
具体实施方式
如图所示,本实用新型所述的用于锅炉水冷壁管的梳形防磨导流片,包括与所述水冷壁固连在一起的防磨片1,所述防磨片1的一边开设有多个与水冷壁管外径相对应的内凹槽2,为使水冷壁管与梳形防磨导流片之间有足够的连接强度,所述内凹槽2的侧角处为弧形过渡。
Claims (2)
1.一种用于锅炉水冷壁管的梳形防磨导流片,包括与所述水冷壁固连在一起的防磨片(1),其特征在于:所述防磨片(1)的一边开设有多个与水冷壁管外径相对应的内凹槽(2)。
2.根据权利要求1所述的用于锅炉水冷壁管的梳形防磨导流片,其特征在于:所述内凹槽(2)的侧角处为弧形过渡。