CN200992517Y - 拉制有色石英玻璃管的连熔炉 - Google Patents

拉制有色石英玻璃管的连熔炉 Download PDF

Info

Publication number
CN200992517Y
CN200992517Y CN 200720033651 CN200720033651U CN200992517Y CN 200992517 Y CN200992517 Y CN 200992517Y CN 200720033651 CN200720033651 CN 200720033651 CN 200720033651 U CN200720033651 U CN 200720033651U CN 200992517 Y CN200992517 Y CN 200992517Y
Authority
CN
China
Prior art keywords
crucible
quartz glass
tungsten crucible
glass tube
tungsten
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200720033651
Other languages
English (en)
Inventor
王绪东
王世平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200720033651 priority Critical patent/CN200992517Y/zh
Application granted granted Critical
Publication of CN200992517Y publication Critical patent/CN200992517Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种拉制有色石英玻璃管的连熔炉,它包括炉体和设在炉体内的钨坩锅,钨坩锅与炉体壁之间装有保温层,坩锅与保温层之间设有加热装置,钨坩锅底部设有圆形的成型出口,钨坩锅中部设有芯杆,由于添加有微量元素的高温石英液体的固化温度发生变化,则将成型器设在成型出口的下方坩锅的外部,为了防止添增了微量元素的高纯石英砂在熔融状态初期对钨坩锅的氧化,在其内部增加了一个钼坩锅;为了固定钼坩锅,在钨坩锅与钼坩锅之间增加一个六棱形耐高温、抗氧化支架。用于生产激光器用的滤紫外石英玻璃管、液下专用防淬超强度绿色石英玻璃管、电加热器及微波炉用的灰色石英玻璃管等,其稳定性和一致性好,成品尺寸误差小,实现高效率的连续生产。

Description

拉制有色石英玻璃管的连熔炉
技术领域
本实用新型涉及一种石英玻璃管的生产设备,特别是一种拉制有色石英玻璃管的连熔炉。
背景技术
激光器用的滤紫外石英玻璃管、液下专用防淬超强度绿色石英玻璃管、电加热器及微波炉用的灰色石英玻璃管,都是在高纯石英砂中加入微量元素通过连熔炉拉制而成的。由于加入了微量元素,对钨坩锅有较大氧化作用,同时使石英管的固化温度发生了变化,原有的普通连熔炉不能生产上述产品。
发明内容
本实用新型要解决的技术问题是针对现有技术的不足,提出了一种设备稳定性和一致性好的能够连续拉制有色石英玻璃管的连熔炉。
本实用新型要解决的技术问题是通过以下技术方案来实现的,一种拉制有色石英玻璃管的连熔炉,它包括炉体和设在炉体内的钨坩锅,钨坩锅与炉体壁之间装有保温层,坩锅与保温层之间设有加热装置,钨坩锅底部设有圆形的成型出口,钨坩锅中部设有芯杆,芯杆上部与炉体的炉盖相接,其特点是:在钨坩锅内的上部套装有个小口径的钼坩锅,在钨坩锅成型出口的下方设有成型器,成型器为与成型出口配套的圆台形,成型器向上与所述的芯杆相接。
本实用新型要解决的技术问题还可以通过以下技术方案来进一步实现,在钨坩锅与钼坩锅之间设有一个六棱形耐高温、抗氧化钼坩锅固定支架。
本实用新型与现有技术相比,由于有色石英玻璃管的固化温度发生变化,则将成型器设在成型出口的下方坩锅的外部,使连续熔融的添加有微量元素的高温石英液体通过成型出口与成型器之间的可调缝下料,成型为所需颜色的石英玻璃管,再通过牵引机和变频器调整到一定速度,使成型的石英玻璃管连续拉制为成品。为了防止添增了微量元素的高纯石英砂在熔融状态初期对钨坩锅的氧化,在其内部增加了一个钼坩锅;为了固定钼坩锅,在钨坩锅与钼坩锅之间增加一个六棱形耐高温、抗氧化支架。本连熔炉稳定性和一致性好,成品尺寸误差小,实现高效率的有色石英玻璃管连续生产。
附图说明
图1为本实用新型的结构简图。
具体实施方式
一种拉制有色石英玻璃管的连熔炉,它包括炉体1和设在炉体1内的钨坩锅4,在钨坩锅4内的上部套装有个小口径的钼坩锅8,在钨坩锅4与钼坩锅8之间设有一个六棱形耐高温、抗氧化钼坩锅固定支架9。钨坩锅4与炉体壁之间装有保温层2,坩锅4与保温层2之间设有加热装置3,钨坩锅4底部设有圆形的成型出口7,钨坩锅4中部设有芯杆5,芯杆5上部与炉体1的炉盖相接,在钨坩锅4成型出口7的下方设有成型器6,成型器6为与成型出口7配套的圆台形,成型器6向上与所述的芯杆5相接。将连熔炉进行连续升温,并加入含有微量元素的高纯石英粉,使其在高温1900~2200时形成融化待下料靠重力均匀下移,经过成型出口7与成型器6固化成型。在监控过程中,通过调节成型器6与成型出口7之间的间距,使其符合控制石英管的要求,在一步法连续生产过程中,要同时通过调整变频器保障石英管牵引机的最佳速度,最终使拉制出的玻璃管达到所需的技术标准。

Claims (2)

1.一种拉制有色石英玻璃管的连熔炉,它包括炉体(1)和设在炉体(1)内的钨坩锅(4),钨坩锅(4)与炉体壁之间装有保温层(2),钨坩锅(4)与保温层(2)之间设有加热装置(3),钨坩锅(4)底部设有圆形的成型出口(7),钨坩锅(4)中部设有芯杆(5),芯杆(5)上部与炉体(1)的炉盖相接,其特征在于:在钨坩锅(4)内的上部套装有个小口径的钼坩锅(8),在钨坩锅成型出口(7)的下方设有成型器(6),成型器(6)为与成型出口(7)配套的圆台形,成型器(6)向上与所述的芯杆(5)相接。
2.根据权利要求1所述的拉制有色石英玻璃管的连熔炉,其特征在于:在钨坩锅(4)与钼坩锅(8)之间设有钼坩锅固定支架(9)。
CN 200720033651 2007-01-19 2007-01-19 拉制有色石英玻璃管的连熔炉 Expired - Fee Related CN200992517Y (zh)