CN1924034A - Method of producing high grade magnetic concentrate from sulfuric-acid residue composite pellet - Google Patents
Method of producing high grade magnetic concentrate from sulfuric-acid residue composite pellet Download PDFInfo
- Publication number
- CN1924034A CN1924034A CNA2005100320994A CN200510032099A CN1924034A CN 1924034 A CN1924034 A CN 1924034A CN A2005100320994 A CNA2005100320994 A CN A2005100320994A CN 200510032099 A CN200510032099 A CN 200510032099A CN 1924034 A CN1924034 A CN 1924034A
- Authority
- CN
- China
- Prior art keywords
- iron
- magnetic
- sulfuric
- sulfate slag
- concentrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (3)