CN1670060A - Additive for paint and fertilizer and its processing method - Google Patents

Additive for paint and fertilizer and its processing method Download PDF

Info

Publication number
CN1670060A
CN1670060A CN 200410008719 CN200410008719A CN1670060A CN 1670060 A CN1670060 A CN 1670060A CN 200410008719 CN200410008719 CN 200410008719 CN 200410008719 A CN200410008719 A CN 200410008719A CN 1670060 A CN1670060 A CN 1670060A
Authority
CN
China
Prior art keywords
additive
metal salt
silico
inorganic oxide
following weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200410008719
Other languages
Chinese (zh)
Other versions
CN1290913C (en
Inventor
张洪宾
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beijing Red Stone Technology Co Ltd
Original Assignee
石向欣
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 石向欣 filed Critical 石向欣
Priority to CN 200410008719 priority Critical patent/CN1290913C/en
Publication of CN1670060A publication Critical patent/CN1670060A/en
Application granted granted Critical
Publication of CN1290913C publication Critical patent/CN1290913C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The invention relates to an addition agent using in paint and fertilizer, which is made of scallops, silicon calcium inorganic oxide, soluble metallic salt compounds and natural non-metallic minerals, and is processed using super fine wet processes by a lapping stripper. The said addition agent can be used in paint for eliminating contamination and peculiar smell, and in fertilizer for promoting vegetation, increasing agronomic crop product, decreasing rate of fertilizer application, improving soil harden condition and enhancing the capability of agronomic crop resisting pest.

Description

Be applied to the additive and the working method thereof of coating and fertilizer
Technical field
The present invention relates to a kind of additive.Specifically, relate to a kind of additive and working method thereof that is applied in coating and fertilizer.
Background technology
There is not to be applied to simultaneously the additive in coating and two fields of fertilizer in the market.
The similar products like of decontamination chamber internal contamination has " formaldehyde one spray is clean ", " formaldehyde-trapping agent " and " No. one, positive space " etc.Their defective mainly contains: the one, and individual event is removed and is polluted; The 2nd, poor removal effect; The 3rd, certain side effect is arranged; The 4th, cost and price is higher, is not easy large-scale promotion; The 5th, all belong to and remedy type afterwards; The 6th, some has energy consumption; The 7th, complete processing is relatively backward, causes poor product quality, and tooling cost is high on the contrary; The 8th, can not reach sterilization simultaneously and eliminate the carcinogens double goal.
The fertilizer additive that is used to increase production at present has a variety of, but not with the product of the identical principle of the present invention, particularly do not have to be applied to simultaneously the product of coating and fertilizer two big industries.
Summary of the invention
The purpose of this invention is to provide a kind of additive and working method thereof that can be applied to coating and two fields of fertilizer simultaneously.
The present invention adopts following technical scheme to realize.
The formulation by weight of raw material of the present invention: the mixture 10-20% of scallop shell 20-30%, silico-calcium class inorganic oxide and soluble metal salt, surplus is natural nonmetallic mineral.
Wherein, described scallop shell is a kind of natural marine organism; The mixture of described silico-calcium class inorganic oxide and soluble metal salt is made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 10-20%, and all the other are silicon oxide, calcium oxide, the weight ratio of the two be 2: 3 between 3: 2; Nonmetallic mineral is made up of the component of following weight proportion: mica 5%-25%, quartzy 1-5%, feldspar 1-5%, all the other are lithium, dravite.
As preferred version, the formulation by weight of raw material of the present invention: scallop shell 20-30%, titanium dioxide 10%-20%, silico-calcium class inorganic oxide and soluble metal salt mixture 10-20%, surplus is natural nonmetallic mineral.Titanium dioxide is as assistant agent.
As more preferably scheme, the formulation by weight of raw material of the present invention: scallop shell 20-30%, Rutile type Titanium Dioxide 10%-20%, silico-calcium class inorganic oxide and soluble metal salt mixture 10-20%, surplus is natural nonmetallic mineral.
The beneficial effect of additive of the present invention is embodied in:
One, because the crystalline structure of raw material of the present invention own is asymmetric, so itself forms permanent electrode, permanent electrode forms permanent electrostatic field on the surface of material, after airborne water molecules contacts, continuous passive granting negative ion, effectively remove the pollution that ammonia in the room air, benzene, formaldehyde etc. are poisonous, obnoxious flavour causes, purify the air of a room.Main by following dual mode: the one, physisorphtion can be ionized into airborne water molecules hydrogen ion and hydrogen-oxygen negative ion, hydrogen ion with become hydrogen after hydrogen ion combines and discharge, the hydrogen-oxygen negative ion then with water molecules formation hydroxyl negative ion.A large amount of negative ions fills the interior space, and their bags are attached on obnoxious flavour molecular grouping and the dust, and formation sedimentation nuclear back sedimentation also is adsorbed onto on the ground, thereby has dispeled airborne toxic and harmful.The 2nd, chemical reaction method, the hydroxide radical in the hydroxyl radical free radical can with gas generation chemical reactions such as ammonia, nitrogen oxide, form harmless objects such as water, nitrogen; Hydroxide radical and VOC reaction generate water, carbonic acid gas and other harmless objects; In the hydroxyl radical free radical in the unnecessary oxygen energy and objectionable impurities such as formaldehyde.
Two, antibiotic, antibacterial, sterilization, elimination peculiar smell.1, because this matrix material has the function of continuous release 2-18 micron waveband far infrared rays.Far-infrared radiation material has very strong radiation capacity (93%, near the blackbody radiation ability), except that having good health care effect such as regulate the life rhythm, stimulate circulation, it can be antibiotic, antibacterial, eliminates because of the peculiar smell that goes mouldy, oil smoke, animal, human body etc. distribute thereby reach.2, contain portion water solube metallic salt in this matrix material, as inorganic oxides such as silicon, calcium, these materials are positively charged, touch electronegative microorganism cells after, according to the enclosed pasture graviational interaction, mutually absorption also punctures cytolemma, makes the cell protein sex change, breathing again, metabolism and breeding, up to necrocytosis, finish sterilization, and antibiotic composition still keeps original antibacterial ability without any consumption, really accomplishes long acting antibiotic.
Three, promote animals and plants to grow the effect of metabolic function and far infrared rays by negative ion, promote animal and plant growth, improve crop yield, reduce applying quantity of chemical fertilizer, improve the soil compaction situation, strengthen the farm crop resistance against pests and diseases the comprehensive action of soil and animals and plants microcirculation improvement.Be added with the fertilizer of additive of the present invention, owing to have the permanent electrode crystalline material in the material, there are permanent electric field and little electric current, it has hormesis to plant root, therefore can promote the development growth of root, quicken absorption, improve the plant germination rate moisture and nutrition, accelerate speed of germination, splendid to the seed effect of various beans, flower class, greengrocery plant.The present invention also has softening water and improves water quality, reduces effects such as the surface tension of water, the penetrating power that improves water, adjustment potential of hydrogen, therefore can promote the development growth of root, quickens the absorption to moisture and nutrition.It also can infiltrate multiple element in the soil, helps promoting the element of plant-growth, growth as potassium, sodium, calcium, magnesium, iron, boron etc.
Four, cost is lower, and production cost of the present invention is in the market about half of like product cost.Use once, indoor as not fitting up once more, then need never to use, put things right once and for all.Without any need for the energy, natural permanent release negative oxygen ion, save energy meets the STRATEGIES OF SUSTAINABLE DEVELOPMENT requirement.
Embodiment
Specify the present invention below by embodiment.
[embodiment 1]
The weight proportion of raw material: scallop shell 20%, silico-calcium class inorganic oxide and soluble metal salt mixture 10%, surplus is natural nonmetallic mineral.Wherein, described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 10%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 2: 3.Nonmetallic mineral is made up of the component of following weight proportion: mica 5%, quartz 1%, feldspar 1%, all the other dravites.
The present invention adopts the existing grinding machine of delaminating, scallop shell is removed impurity after, carry out the grinding and processing of 200 order to 300 order fineness earlier, reinstate with natural nonmetallic mineral one then and grind the machine of delaminating and carry out super-fine processing, be worked into the nano level fineness; Add again with the silico-calcium class inorganic oxide of fineness and the mixture of soluble metal salt, process according to existing ultrafine powder wet method.As preferred version, add convert the water yield and powder man-hour at every turn weight ratio between 1: 2 to 1: 3, grinding medium adopts zirconium white and zirconium silicate.In first time during super-fine processing, with 1.8 to 2.4 millimeters fineness,,, adding man-hour for the third time with 0.8 to 1.2 millimeter fineness with 1.2 to 1.8 millimeters fineness in second time during super-fine processing, adding the fineness of man-hour for the 4th time with 0.4 to 0.8 millimeter.Substitute with four grinding machines of delaminating and to carry out repeatedly, during effective solution super-fine processing this kind material production agglomeration, product burnt hair and use in incident deposited phenomenon.
[embodiment 2]
The weight proportion of raw material: scallop shell 28%, silico-calcium class inorganic oxide and soluble metal salt mixture 20%, surplus is natural nonmetallic mineral.Wherein, described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 12% all the other be silicon oxide and calcium oxide, the weight ratio of the two is 3: 2.Nonmetallic mineral is made up of the component of following weight proportion: mica 25%, quartz 5%, feldspar 5%, all the other are elbaite.
Method according to embodiment 1 is processed into additive.
[embodiment 3]
The weight proportion of raw material: scallop shell 30%, silico-calcium class inorganic oxide and soluble metal salt mixture 11%, surplus is natural nonmetallic mineral.Described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 20%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 1: 1.Nonmetallic mineral is made up of the component of following weight proportion: mica 14%, quartz 3%, feldspar 2%, elbaite 40%, dravite 41%.
Method according to embodiment 1 is processed into additive.
[embodiment 4]
The formulation by weight of raw material: scallop shell 22%, titanium dioxide 10%, silico-calcium class inorganic oxide and soluble metal salt mixture 12%, surplus is natural nonmetallic mineral.Described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 19%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 1: 1.Nonmetallic mineral is made up of the component of following weight proportion: mica 6%, quartz 4.5%, feldspar 1.5%, elbaite 60%, dravite 28%.
Titanium dioxide, silico-calcium class inorganic oxide and soluble metal salt mixture add together, are processed into additive according to the method for embodiment 1.
[embodiment 5]
The formulation by weight of raw material: scallop shell 28%, titanium dioxide 20%, silico-calcium class inorganic oxide and soluble metal salt mixture 17%, surplus is natural nonmetallic mineral.Described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 14%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 3: 2; Nonmetallic mineral is made up of the component of following weight proportion: mica 23%, quartz 4.5%, feldspar 2.5%, all the other are elbaite 35%, dravite 35%.
Method according to embodiment 4 is processed into additive.
[embodiment 6]
The formulation by weight of raw material: scallop shell 25%, titanium dioxide 15%, silico-calcium class inorganic oxide and soluble metal salt mixture 19%, surplus is natural nonmetallic mineral.Described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 11%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 2: 3. Nonmetallic mineral is made up of the component of following weight proportion: mica 5.5%, quartz 1.5%, feldspar 2%, elbaite 30%, dravite 61%.
Method according to embodiment 4 is processed into additive.
[embodiment 7]
The formulation by weight of raw material: scallop shell 25%, Rutile type Titanium Dioxide 15%, silico-calcium class inorganic oxide and soluble metal salt mixture 15%, surplus is natural nonmetallic mineral.Described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 18%, and all the other are silicon oxide and calcium oxide, and the weight ratio of the two is 1: 1; Nonmetallic mineral is made up of the component of following weight proportion: mica 20%, quartz 5%, feldspar 5%, elbaite 60%, dravite 10%.
Method according to embodiment 4 is processed into additive.
The additive that embodiment 4,5,6 is made adds water paint for internal walls to according to the ratio of 2-8%, in coating such as Nippon, how happy scholar.Through the check of building materials quality supervision and inspection station, Beijing, meet the salable product index request in the GB/T9756-2001 standard.Sample is pressed GB/T18204.26-2000, GB/T18204.25-2000, GB11737-89 check, and the removal efficient to ammonia, formaldehyde, benzene was respectively 95.3%, 94.4%, 95.5% in 96 hours.
The additive that embodiment 7 is made adds in the various fertilizer according to the ratio of 0.1-0.6%, as various urea types, phosphorus potassium type fertilizer.Adopt pairing field test method test through the Fengtai District, Beijing City research of agricultural science, to balling romaine lettuce volume increase 18% (urea type), to rape yield increasing 8% (urea type), to cucumber production promoting 8.1% (urea type), to tomato production promoting 10.1% (urea type); To cucumber production promoting 6.8% (phosphorus potassium type), to tomato production promoting 7.1% (phosphorus potassium type).

Claims (4)

1, a kind of additive that can be applied to coating and two fields of fertilizer simultaneously, made by the raw material of following weight prescription: scallop shell 20-30%, silico-calcium class inorganic oxide and soluble metal salt mixture 10-20%, surplus are natural nonmetallic minerals;
Wherein, described silico-calcium class inorganic oxide and soluble metal salt mixture are made up of the component of following weight proportion: Silver Nitrate, cupric nitrate, zinc nitrate respectively account for 10-20%, and surplus is silicon oxide, calcium oxide, the weight ratio of the two be 2: 3 between 3: 2; Natural nonmetallic mineral is made up of the component of following weight proportion: mica 5%-25%, quartzy 1-5%, feldspar 1-5%, all the other are lithium, dravite.
2, the additive that can be applied to coating and two fields of fertilizer simultaneously according to claim 1, raw material by the following weight prescription is made: scallop shell 20-30%, titanium dioxide 10%-20%, silico-calcium class inorganic oxide and soluble metal salt mixture 10-20%, surplus is natural nonmetallic mineral.
3, the additive that can be applied to coating and two fields of fertilizer simultaneously according to claim 1, raw material by the following weight prescription is made: scallop shell 20-30%, Rutile type Titanium Dioxide 10%-20%, silico-calcium class inorganic oxide and soluble metal salt mixture 10-20%, surplus is natural nonmetallic mineral.
4, the described working method that can be applied to the additive in coating and two fields of fertilizer simultaneously of claim 1, adopt existing ultrafine powder wet method to process, it is characterized in that: add convert the water yield and powder man-hour at every turn weight ratio between 1: 2 to 1: 3, grinding medium adopts zirconium white and zirconium silicate, substitutes with four grinding machines of delaminating and carries out repeatedly.
CN 200410008719 2004-03-15 2004-03-15 Additive for paint and fertilizer and its processing method Expired - Fee Related CN1290913C (en)