CN1669692A - 塑性成型螺纹接口薄壁三通管的制造方法 - Google Patents

塑性成型螺纹接口薄壁三通管的制造方法 Download PDF

Info

Publication number
CN1669692A
CN1669692A CN 200510034001 CN200510034001A CN1669692A CN 1669692 A CN1669692 A CN 1669692A CN 200510034001 CN200510034001 CN 200510034001 CN 200510034001 A CN200510034001 A CN 200510034001A CN 1669692 A CN1669692 A CN 1669692A
Authority
CN
China
Prior art keywords
wall
light
way pipe
pipe
moulding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200510034001
Other languages
English (en)
Inventor
王文辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200510034001 priority Critical patent/CN1669692A/zh
Publication of CN1669692A publication Critical patent/CN1669692A/zh
Pending legal-status Critical Current

Abstract

一种塑性成型螺纹接口薄壁三通管的制造方法,属于管道连接常用配件制造技术领域。本发明要解决的技术问题是提供一种加工方便、工艺简单、需用设备少、需用动力小的螺纹接口薄壁三通管的制造方法,能一次成型三通管体及三段接口螺纹,并降低制造成本。为此,在已放入两瓣膜模具内的薄壁管坯料内插入胶模,通过两侧轴柱向胶模施加轴向力,迫使薄壁管坯料产生塑性变形,按模具内成型腔室和模具内三段接口螺纹的形状成型。本发明主要适用于钢制薄壁三通管,特别是不锈钢三通管的制造,同时也适用于非金属材料三通管的制造。

Description

塑性成型螺纹接口薄壁三通管的制造方法
技术领域
本发明涉及管道连接常用配件制造技术领域,特别是一种塑性成型螺纹接口薄壁三通管的制造方法。
背景技术
三通管是液体输送管道连接中不可缺少的常用配件。现有的三通管制造方法大部分是用铸造工艺,由于铸造工艺的局限,制造出的三通管壁往往较厚,而且三通管的螺纹一般需要用车床车出,导致铸造三通管的材料成本及制造成本较高。还有另一种三通管制造方法是采用液体作介质进行挤压成型,其缺点是对密封性要求很高,成型所需动力较大,使得其制造设备较为复杂庞大,而且三通管的三段接口螺纹并非同时一次成型。
发明内容
本发明要解决的技术问题是提供一种加工方便、工艺简单、需用设备少、需用动力小的螺纹接口薄壁三通管的制造方法,能一次成型三通管体及三段接口螺纹,并降低制造成本。
本发明所提出的技术解决方案是一种塑性成型螺纹接口薄壁三通管的制造方法,其工艺步骤为:
(1)将薄壁管坯料放入两瓣膜组成的模具内,在薄壁管坯料内插入胶模,然后将轴柱分别插入薄壁管坯料的两端;
(2)对轴柱施加轴向力,所述胶模受轴向力压缩后产生胀形力,迫使薄壁管坯料中部对应模具内成型腔室的管壁以及对应模具内三段接口螺纹的管壁产生塑性变形,按成型腔室的形状成型,以及按模具接口螺纹的形状成型外螺纹;
(3)拆开模具,取出轴柱和胶模,将已成型的三通管的封闭端以及多余的端头切去,成为螺纹接口薄壁三通管。
与现有技术相比,本发明具有如下有益效果:采用本发明这种以胶模作为介质对薄壁管材进行冷挤压塑性成型的制造方法可以制造出管壁较薄的三通管,而且相比起用液体作为介质的制造方法,本发明对介质密封性的要求大大降低,成型所需动力较小,使得制造设备也相对简单、体积较小,而且制造出的三通管及其接口螺纹是同时一次成型的,大大降低了材料成本及制造成本。
本发明主要适用于钢制薄壁三通管,特别是不锈钢三通管的制造,同时也适用于非金属材料三通管的制造。
附图说明
图1是用胀形力成型螺纹接口薄壁三通管的加工示意图。
图2是图1所示成型脱模后的螺纹接口薄壁三通管的再加工示意图。
具体实施方式
通过下面实施例对本发明作进一步详细阐述。
如图1、图2所示,本实施例的一种塑性成型螺纹接口薄壁三通管的制造方法,其工艺步骤是把不锈钢管坯1插入两瓣膜组成的模具2内,把胶模3插入不锈钢管坯1内,再将轴柱4、5分别插入管坯1的两端,并对轴柱4、5施加20-50Mpa的轴向力P1、P2,令胶模3受轴向力P1、P2压缩后产生胀形力,迫使不锈钢管坯1中部靠近模具内成型腔室7的管壁以及靠近三段螺纹10、11、12的管壁处产生塑性变形,并从排气腔6排气,按成型腔室7的形状成型,以及按模具接口螺纹10、11、12的形状成型外螺纹。成型完毕后,拆开模具2,取出轴柱4、5和胶模3。将成型好的三通管的封闭端16及多余端头13、14、15切去,完成螺纹接口不锈钢管薄壁三通管的制作。

Claims (1)

1.一种塑性成型螺纹接口薄壁三通管的制造方法,其特征在于其工艺步骤为:
①将薄壁管坯料(1)放入两瓣膜组成的模具(2)内,在薄壁管坯料(1)内插入胶模(3),然后将轴柱(4、5)分别插入薄壁管坯料(1)的两端;
②对轴柱(4、5)施加轴向力(P1、P2),所述胶模(3)受轴向力(P1、P2)压缩后产生胀形力,迫使薄壁管坯料(1)中部对应模具(2)内成型腔室(7)的管壁以及对应模具(2)内三段接口螺纹(10、11、12)的管壁产生塑性变形,按成型腔室(7)的形状成型,以及按模具接口螺纹(10、11、12)的形状成型外螺纹;
③拆开模具(2),取出轴柱(4、5)和胶模(3),将已成型的三通管的封闭端(16)以及多余的端头(13、14、15)切去,成为螺纹接口薄壁三通管。
CN 200510034001 2005-04-04 2005-04-04 塑性成型螺纹接口薄壁三通管的制造方法 Pending CN1669692A (zh)