CN1621180A - 铝轮毂铸造砂眼的修复技术 - Google Patents

铝轮毂铸造砂眼的修复技术 Download PDF

Info

Publication number
CN1621180A
CN1621180A CN 200410083000 CN200410083000A CN1621180A CN 1621180 A CN1621180 A CN 1621180A CN 200410083000 CN200410083000 CN 200410083000 CN 200410083000 A CN200410083000 A CN 200410083000A CN 1621180 A CN1621180 A CN 1621180A
Authority
CN
China
Prior art keywords
aluminium
hub
cast
sand
spray
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200410083000
Other languages
English (en)
Other versions
CN1295048C (zh
Inventor
徐兆督
安建
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Yueling Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2004100830009A priority Critical patent/CN1295048C/zh
Publication of CN1621180A publication Critical patent/CN1621180A/zh
Application granted granted Critical
Publication of CN1295048C publication Critical patent/CN1295048C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种对大型摩托车、汽车车轮铝轮毂铸造砂眼的修复技术,其特征在于:铝轮毂铸造砂眼的修复是按下列步骤进行的:1.在铝轮毂表面进行开砂处理,将铝轮毂表面渣质及铸造表面颗粒抛掉;2.采用金刚砂对铝轮毂表面进行喷砂处理;3.扩孔:对铝轮毂表面的砂眼进行扩孔处理成异形孔;4.将铝轮毂整体加热至为80~120℃;5.用金属喷涂枪将铝轮毂表面瞬间加热至重熔状态,铝丝熔化呈液体状态,喷铸到铝轮毂的异形孔内;6.喷铸后的铝轮毂表面进行抛光处理。本发明解决了大型摩托车、汽车铝轮毂砂眼电镀前的修复问题,具有加工工艺简单、费用低、时间短、质量好的特点,满足了大型摩托车、汽车铝轮毂生产的需要。

Description

铝轮毂铸造砂眼的修复技术
技术领域
本发明涉及一种对大型摩托车、汽车车轮铝轮毂铸造砂眼的修复技术。
背景技术
摩托车、汽车车轮的铝轮毂在铸造加工时会出现铸造砂眼,在传统的生产过程中,对少量的直径较小的砂眼,采用铁锤敲打进行封闭处理,对直径较大的砂眼要进行扩孔后用铆钉封闭处理。当工件上的砂眼数量过多时就要报废,采用回炉处理的方式。铝轮毂铸造生产的废品率很高,可以达到30~40%左右,造成大量的资金浪费。国内生产对外出口的大型摩托车、汽车车轮的铝轮毂,尤其是两面应用的摩托车铝轮毂,表面采用电镀工艺,所以表面需光滑,在铸造加工时,铝轮毂的一面就会有几百个纱眼产生。目前,这种大型摩托车铝轮毂砂眼电镀前的修复还没有更好的方法解决。
发明内容
本发明克服了上述存在的缺陷,目的是解决了大型摩托车铝轮毂铸造砂眼电镀前的修复,提供一种铝轮毂铸造砂眼的修复技术。
本发明铝轮毂铸造砂眼的修复技术内容简述:
本发明铝轮毂铸造砂眼的修复技术,其特征在于:铝轮毂铸造砂眼的修复是按下列步骤进行的:
1、开砂处理:在铝轮毂表面进行开砂处理,用抛光机将铝轮毂表面渣质及铸造表面颗粒抛掉;
2、喷砂处理:采用金刚砂对铝轮毂表面进行喷砂处理;
3、扩孔:对铝轮毂表面的砂眼进行扩孔处理成异形孔;
4、热处理:将铝轮毂整体加热,温度为80~120℃;
5、喷铸:用金属喷涂枪将铝轮毂表面瞬间加热至重熔状态,铝丝熔化呈液体状态,喷铸到铝轮毂的异形孔内,根据产品的大小金属喷涂枪与铝轮毂的距离控制在50~100mm,喷铸停留时间为0.5~60秒,可反复喷铸;
6、抛光处理:将喷铸后的铝轮毂表面进行抛光处理。
本发明铝轮毂铸造砂眼的修复技术,解决了大型摩托车、汽车铝轮毂砂眼电镀前的修复问题,具有加工工艺简单、费用低、时间短、质量好的特点,满足了大型摩托车、汽车铝轮毂生产的需要。
具体实施方式
本发明铝轮毂铸造砂眼的修复技术是这样实现的,首先对铝轮毂铸造砂眼的表面进行开砂处理,用抛光机将铝轮毂表面渣质及铸造表面颗粒抛掉。然后进行喷砂处理,采用金刚砂对铝轮毂表面进行喷砂处理。对铝轮毂表面的砂眼进行扩孔,在砂眼处进行扩孔处理成异形孔。将扩孔处理后的铝轮毂整体加热,温度为80~120℃。用金属喷涂枪将铝轮毂表面瞬间加热至重熔状态,铝丝熔化呈液体状态,喷铸到铝轮毂的异形孔内,根据产品的大小金属喷涂枪与铝轮毂的距离控制在50~100mm,喷铸停留时间为0.5~60秒,可反复喷铸;将喷铸后的铝轮毂表面进行抛光处理。经检测抛光处理不影响铝液与铝轮毂基体的结合强度,万全可以满足产品质量的要求。

Claims (1)

1、一种铝轮毂铸造砂眼的修复技术,其特征在于:铝轮毂铸造砂眼的修复是按下列步骤进行的:
(1)、开砂处理:在铝轮毂表面进行开砂处理,用抛光机将铝轮毂表面渣质及铸造表面颗粒抛掉;
(2)、喷砂处理:采用金刚砂对铝轮毂表面进行喷砂处理;
(3)、扩孔:对铝轮毂表面的砂眼进行扩孔处理成异形孔;
(4)、热处理:将铝轮毂整体加热,温度为80~120℃;
(5)、喷铸:用金属喷涂枪将铝轮毂表面瞬间加热至重熔状态,铝丝熔化呈液体状态,喷铸到铝轮毂的异形孔内,根据产品的大小金属喷涂枪与铝轮毂的距离控制在50~100mm,喷铸停留时间为0.5~60秒,可反复喷铸;
(6)、抛光处理:将喷铸后的铝轮毂表面进行抛光处理。
CNB2004100830009A 2004-12-17 2004-12-17 铝轮毂铸造砂眼的修复技术 Expired - Fee Related CN1295048C (zh)