Prior art keywords
weight percent
lubricant
accounts
described lubricant
graphite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 02154901
Other languages
English (en)
Inventor
阮震祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANG KEMING MECHANICAL EQUIPMENT CO Ltd
Original Assignee
SHANG KEMING MECHANICAL EQUIPMENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANG KEMING MECHANICAL EQUIPMENT CO Ltd filed Critical SHANG KEMING MECHANICAL EQUIPMENT CO Ltd
Priority to CN 02154901 priority Critical patent/CN1570049A/zh
Publication of CN1570049A publication Critical patent/CN1570049A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Lubricants (AREA)

Abstract

一种石墨润滑剂,所述的润滑剂由石墨微粉、甲基纤维素、亚甲基双钠磺酸钠、硅酸钠、及表面活性剂组合,其中,所述的石墨微粉占所述的润滑剂的重量百分比在60- 85%之间、所述的甲基纤维素占所述的润滑剂的重量百分比在1-1.5%之间、所述的亚甲基双钠磺酸钠占所述的润滑剂的重量百分比在4-10%之间、所述的硅酸钠占所述的润滑剂的重量百分比在9-30%之间、所述的表面活性剂占所述的润滑剂的重量百分比在0.2-1.5之间。本发明和已有技术相对照,提高了润滑剂的高温润滑特性,具有改善介质的润湿、扩散、乳化性能。

Description

一种石墨润滑剂
技术领域:
本实用新型涉及化学领域,尤其涉及一种润滑剂,具体来说是一种石墨润滑剂。
背景技术:
目前,在轧机上广泛使用的固体润滑剂,主要包括石墨及盐类等润滑剂,在石墨润滑剂中.以矿物油为介质.在烧制时,油份烧尽,产生的烟尘和烟气易污染设备和厂房.同时在高温下,石墨将丧失其耐磨性能,而影响钢管质量。
发明内容:
本发明所要解决的技术问题是:由于现有技术中,在轧机上广泛使用的固体润滑剂,主要包括石墨及盐类等润滑剂,在石墨润滑剂中.以矿物油为介质.在烧制时,油份烧尽,产生的烟尘和烟气易污染设备和厂房.同时在高温下,石墨将丧失其耐磨性能,而影响钢管质量。本发明为解决已有技术中的上述技术问题,所采用的技术方案是提供一种石墨润滑剂,所述的润滑剂由石墨微粉、甲基纤维素、亚甲基双钠磺酸钠、硅酸钠、及表面活性剂组合,其中,所述的石墨微粉占所述的润滑剂的重量百分比在60-85%之间、所述的甲基纤维素占所述的润滑剂的重量百分比在1-1.5%之间、所述的亚甲基双钠磺酸钠占所述的润滑剂的重量百分比在4-10%之间、所述的硅酸钠占所述的润滑剂的重量百分比在9-30%之间、所述的表面活性剂占所述的润滑剂的重量百分比在0.2-1.5之间。
本发明的制造方法采用已有技术中的制造方法制造。
本发明和已有技术相对照,提高了润滑剂的高温润滑特性,具有改善介质的润湿、扩散、乳化性能。
具体实施方式:
本发明一种石墨润滑剂,所述的润滑剂由石墨微粉、甲基纤维素、亚甲基双钠磺酸钠、硅酸钠、及表面活性剂组合,其中,所述的石墨微粉占所述的润滑剂的重量百分比在60-85%之间、所述的甲基纤维素占所述的润滑剂的重量百分比在1-1.5%之间、所述的亚甲基双钠磺酸钠占所述的润滑剂的重量百分比在4-10%之间、所述的硅酸钠占所述的润滑剂的重量百分比在9-30%之间、所述的表面活性剂占所述的润滑剂的重量百分比在0.2-1.5之间。

Claims (1)

1,一种石墨润滑剂,所述的润滑剂由石墨微粉、甲基纤维素、亚甲基双钠磺酸钠、硅酸钠、及表面活性剂组合,其特征在于:所述的石墨微粉占所述的润滑剂的重量百分比在60-85%之间、所述的甲基纤维素占所述的润滑剂的重量百分比在1-1.5%之间、所述的亚甲基双钠磺酸钠占所述的润滑剂的重量百分比在4-10%之间、所述的硅酸钠占所述的润滑剂的重量百分比在9-30%之间、所述的表面活性剂占所述的润滑剂的重量百分比在0.2-1.5之间。
CN 02154901 2002-12-13 2002-12-13 一种石墨润滑剂 Pending CN1570049A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 02154901 CN1570049A (zh) 2002-12-13 2002-12-13 一种石墨润滑剂

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 02154901 CN1570049A (zh) 2002-12-13 2002-12-13 一种石墨润滑剂

Publications (1)

Publication Number Publication Date
CN1570049A true CN1570049A (zh) 2005-01-26

Family

ID=34468857

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 02154901 Pending CN1570049A (zh) 2002-12-13 2002-12-13 一种石墨润滑剂

Country Status (1)

Country Link
CN (1) CN1570049A (zh)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101870907A (zh) * 2010-06-23 2010-10-27 河南省长城特种润滑脂有限公司 高温润滑脂及制备方法
CN101914412A (zh) * 2010-08-25 2010-12-15 新乡学院 一种水性石墨润滑剂
CN101914409A (zh) * 2010-08-25 2010-12-15 新乡学院 一种耐高温润滑剂的制备方法
CN101717621B (zh) * 2009-12-15 2012-12-26 吕桂军 钻井液用低荧光防卡润滑剂及其生产方法
CN109877272A (zh) * 2019-02-28 2019-06-14 宁波金田铜业(集团)股份有限公司 一种抛光黄铜锭浇铸脱模用的脱模剂及其制备方法

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101717621B (zh) * 2009-12-15 2012-12-26 吕桂军 钻井液用低荧光防卡润滑剂及其生产方法
CN101870907A (zh) * 2010-06-23 2010-10-27 河南省长城特种润滑脂有限公司 高温润滑脂及制备方法
CN101914412A (zh) * 2010-08-25 2010-12-15 新乡学院 一种水性石墨润滑剂
CN101914409A (zh) * 2010-08-25 2010-12-15 新乡学院 一种耐高温润滑剂的制备方法
CN101914409B (zh) * 2010-08-25 2013-01-09 新乡学院 一种耐高温润滑剂的制备方法
CN101914412B (zh) * 2010-08-25 2013-02-27 新乡学院 一种水性石墨润滑剂
CN109877272A (zh) * 2019-02-28 2019-06-14 宁波金田铜业(集团)股份有限公司 一种抛光黄铜锭浇铸脱模用的脱模剂及其制备方法

Similar Documents

Publication Publication Date Title
CN1063479C (zh) 用于金属热加工工件的润滑剂组合物
CN107201067B (zh) 一种耐高温隔热保温涂料及其制作方法
CN104450104B (zh) 一种生物可降解的润滑油的制备方法
CN108315085B (zh) 一种耐高温液态金属极压润滑剂及其制备方法
WO2007098523A3 (de) Betriebsbereites getriebe, betriebsflüssigkeit für ein solches und verfahren zu dessen erstinbetriebnahme
CN105441181A (zh) 金属切削液及其制备方法
CN101270317B (zh) 高润滑性环境友好型水基芯棒润滑剂
AU2003258223A1 (en) Organic acid salts as thickeners
CN103880027A (zh) 羟基硅酸镁纳米管抗磨材料及其制备方法
CN108690698A (zh) 一种高效抗磨节能润滑油组合物及其制备方法
CN104046407A (zh) 一种润滑油(脂)用抗磨减摩复合添加剂
CN1570049A (zh) 一种石墨润滑剂
CN101928631A (zh) 一种金属热塑性加工用环保型高温润滑剂及其使用方法
CN101886022A (zh) 基于碳纳米管的高效水基润滑液的制备方法
WO2008058053A3 (en) Anhydrous lithium hydroxide and/or lithium hydroxide monohydrate dispersions and grease compositions made from same
CN204477069U (zh) 一种高耐磨耐高温轴承
CA2493288A1 (en) Additive composition for transmission oil containing hydrated alkali metal borate and hexagonal boron nitride
CN110734804B (zh) 一种纳米切削油及其制备方法和应用
CN104830433A (zh) 一种柴油机用润滑油
CN102814348B (zh) 一种钛合金管材减壁拉拔用润滑剂及其使用方法
CN1122824A (zh) 用于连轧管机芯棒的胶体润滑剂
CN102093927A (zh) 石墨-氧化物复合型热轧无缝钢管用固体润滑剂及其制备方法
CN104073322A (zh) 金属加工液及其制备方法
CN102408940B (zh) 一种防粘扣钻具螺纹脂及其制备方法
CN201461762U (zh) 油密封万向节

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication