CN1519282A - 凝汽器管板、管口密封防腐专用涂料 - Google Patents
凝汽器管板、管口密封防腐专用涂料 Download PDFInfo
- Publication number
- CN1519282A CN1519282A CNA031032222A CN03103222A CN1519282A CN 1519282 A CN1519282 A CN 1519282A CN A031032222 A CNA031032222 A CN A031032222A CN 03103222 A CN03103222 A CN 03103222A CN 1519282 A CN1519282 A CN 1519282A
- Authority
- CN
- China
- Prior art keywords
- condenser
- pipe
- mouth
- tube sheet
- coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
凝汽器管板、管口密封防腐专用涂料,为添加碳化硅的酚醛环氧KD系列涂料。通过采用清扫、吹干、除锈、涂装、烘干等一系列先进施工工艺涂装在凝汽器管板、管口上,具有耐热水、耐酸碱、耐磨损、抗冲刷、耐水解、耐老化、附着力强、密封性能好、长期使用之功效,且保证六年以上不鼓泡、不龟裂、不脱落、有效防止管板腐蚀、管口冲刷腐蚀及胀口渗漏,减少电化学腐蚀,提高水汽品质。
Description
本发明为一种专用防腐涂料,采用专门施工工艺,可以有效防止火电厂凝汽器管板腐蚀、管口的冲刷腐蚀及胀口渗漏,延长凝汽器的使用寿命,保证凝结水品质。
由于水质的工业污染及水资源的紧缺,循环水浓缩倍率的提高,凝汽器管板腐蚀,管口的冲刷腐蚀及胀口的渗漏是每台凝汽器都存在的实际问题。这个问题降低了凝结水水质,加快锅炉受热面的腐蚀结垢,常引起锅炉爆管,造成非计划停机事故。为解决这一问题,通常的做法是更换凝汽器铜管(钢管),其施工难度大、工期长,而且维护和检修费用过高,增加了生产成本。
为了更有效地解决这一难题,本人历经四年多时间的涂料配方试验、模拟涂刷试验、现场涂刷试验以及施工工艺的研究,成功研制出添加碳化硅的酚醛环氧涂料(KD系列凝汽器管板、管口及专用防腐涂料),其基本配方为:
原 料 比例 功效
酚醛环氧涂料 84.5%
邻苯二甲酸二丁脂C6H4(C00C4Ha)2 0.5% 增加韧性
固化剂 10% 粘合固化
碳化硅S1C 5% 增加耐磨度
该涂料具有在凝汽器水侧环境下长期使用并且防止胀口渗漏,防止管口冲刷腐蚀和管板电偶腐蚀所需的各种性能。其特征是:具有优异的耐水性、密封性、柔韧性;具有高强度、抗冲刷、耐磨性能好;耐酸碱性和耐热性能突出,可以在100℃的温度条件下使用;对黄铜合金、镍铜合金、碳钢、不锈钢和钛材均具有很强的附着力。配套技术方案共分10步工艺流程:①凝汽器内部清扫,保证每根管子管口和管板清洁;②利用压缩空气,对凝汽器的每根管子、管板进行吹干;③利用专用金属刷对管口进行清除表面氧化层;④利用0.5~0.7Mpa压缩空气及钢砂,对管板进行喷砂除锈,喷砂前用专用皮塞将管口堵住,喷砂除锈后的管板要求见到金属本色,喷砂完成,取掉专用塞子;⑤利用压缩空气和吸尘器反复清扫管板、管口清除管口灰尘;⑥管板进行第一层涂装,管口进行第一层涂装(管口向内延伸100mm);⑦管板进行第二层涂装,管口第二涂装(管口向内延伸20~30mm);⑧管板进行第三层,管口第三层涂装(深80~100mm);⑨管板四层,管口四层涂装(深80~100mm)。⑩涂层面进行烤干。各涂层都要用碘钨灯进行烘干,碘钨灯电源需加装漏电保护器。
经过KD系列专用涂料涂装后的涂层,具有耐热水、酸碱、盐雾、油等化学品;耐磨损、抗冲击、耐水解、耐老化。涂层可保证六年以上不鼓泡、不龟裂、不脱落。有效防止冷却水从胀口渗漏到凝结水,防止管板腐蚀、管口冲刷腐蚀和电化学腐蚀,保证水汽品质及机组的安全运行,减少检修费用,降低生产成本。
Claims (1)
- 凝汽器密封防腐专用涂料为添加碳化硅的酚醛环氧KD系列涂料。主要用于火电厂凝汽器及其它行业的冷凝汽器管板、管口密封防腐。其特征是:采用相关配套施工工艺,把该涂料涂装在凝汽器管板和管口上,具有长期使用、耐热水、酸碱、盐雾、油等化学品,耐磨损、抗冲刷、耐老化、柔韧性强、密封性能好、附着力强等优点,有效防止胀口渗漏,管口冲刷腐蚀和管板电偶腐蚀,提高水汽品质,延长管子使用寿命,保证机组安全运行。