CN1253521C - Environment protecting sprayed glue and its prepn and use - Google Patents

Environment protecting sprayed glue and its prepn and use Download PDF

Info

Publication number
CN1253521C
CN1253521C CN 02115305 CN02115305A CN1253521C CN 1253521 C CN1253521 C CN 1253521C CN 02115305 CN02115305 CN 02115305 CN 02115305 A CN02115305 A CN 02115305A CN 1253521 C CN1253521 C CN 1253521C
Authority
CN
China
Prior art keywords
environment
glue
friendly type
spray glue
rosin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 02115305
Other languages
Chinese (zh)
Other versions
CN1388197A (en
Inventor
黄楚填
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huang Chutian
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 02115305 priority Critical patent/CN1253521C/en
Publication of CN1388197A publication Critical patent/CN1388197A/en
Application granted granted Critical
Publication of CN1253521C publication Critical patent/CN1253521C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The present invention discloses environment protecting sprayed glue. The sprayed glue optimally comprises by weight proportion: 8% of thermoplastic elastomers SBS, 6% of rosin, 7% of hydrogenated rosin, 4% of petroleum resin, 3% of tackifying resin, 49.5% of solvent oil 6, 5% of acetone, 15% of cyclohexane, 2% of quad-ester, and 0.5% of antioxidant. A preparation technological method of the present invention comprises: firstly, filling the quantitative solvent oil 6, the acetone and the cyclohexane in a stirrer and starting a machine so that the materials are uniformly stirred into a mixed solution; then, orderly filling the rosin, the hydrogenated rosin, the petroleum resin, the tackifying resin, the quad-ester and the antioxidant in the stirrer to be stirred about 6 hours at ordinary temperature so that all materials are completely dissolved into a light yellow glue solution; subsequently, filtering the materials by 80 meshes. The environment protecting sprayed glue of the present invention has the advantages of nontoxicity, low cost and rapid drying and is particularly suitable for being used as adhesive manufacturing soft furniture.

Description

Environment-friendly type spray glue and processing method and purposes
Technical field
The present invention relates to a kind of tackiness agent, relate in particular to a kind of environment-friendly type spray glue and manufacture craft and purposes.
Background technology
The thermoplastic elastomer SBS's solvent-borne type spray glue that occurs in the market, all different ratios contains triphen (benzene,toluene,xylene) and halocarbon class severe toxicity, high toxicity solvent, triphen can be carcinogenic, the halocarbon class can influence human body metabolism and cause liver to poison, no matter be Long contact time or short-time contact, the acute and chronic poisoning that human body is caused in the capital to some extent causes serious pollution to surrounding environment simultaneously.Though the patent No. is the problem that the prescription of the patent of invention of 90106727.X has solved toxic pollutant, but its cost is higher, and only limit to the glue of mounting as the color printing overlay film, in addition, because its prescription has adopted the 120# solvent oil, its time of drying is longer, thereby limits its application as software furniture tackiness agent.
Summary of the invention
The objective of the invention is to overcome the deficiencies in the prior art part and provide a kind of environment-friendly type spray glue and processing method and purposes of nontoxic, fast drying.
To achieve the above object of the invention, the weight proportion of environment-friendly type spray glue of the present invention is: thermoplastic elastomer SBS 5-15%, rosin 5-10%, staybelite 5-10%, petroleum resin 2-6%, tackifying resin 2-6%, soybean extracting solvent no.6 45-55%, acetone 2-10% and hexanaphthene 10-20%, in order to reach better effect, also add fourth fat and the 0.5-1.0% anti-aging agent of 1-3%, each component sum is 100%.
The processing method of making environment-friendly type spray glue of the present invention is as follows:
A. earlier quantitative soybean extracting solvent no.6, acetone, hexanaphthene are dropped in the agitator, machining stirs becomes mixing solutions;
B. more quantitative thermoplastic elastomer SBS is dropped in the agitator and stir;
C. at last quantitative rosin, staybelite, petroleum resin, tackifying resin, fourth fat and anti-aging agent are dropped in the agitator and stir;
D. above material all drops in the agitator back and continues stirring at normal temperature dissolving 6 hours, checks that all materials are dissolved into faint yellow glue fully, and 80 orders filter and get final product then.
Because environment-friendly type spray glue of the present invention is nontoxic and the soybean extracting solvent no.6 of employing fast drying, therefore is particularly suitable for being applied to the bonding of software furniture, this application also is one of emphasis of the present invention.Use the method for environment-friendly type spray glue software furniture of the present invention as follows:
A. clean the veneer of software furniture material to be pasted;
B. with spray gun environment-friendly type spray glue is sprayed on equably the veneer of material to be pasted;
C. placed 1 to 3 minute, and be as the criterion, get final product pressurized adhesion so that sprayed coating is tack-free.
Compared with prior art, environment-friendly type spray glue of the present invention has following advantage:
1, do not contain triphen in this prescription, and halocarbon class high toxicity solvent.
2, adopt soybean extracting solvent no.6, nontoxic substantially to human body, acetone, hexanaphthene all are low toxicity, micro-virus kind solvent; and content is very low, only accounts for the 15-20% of glue, so this prescription is harmless substantially to human body; surpass the nation's security standard, meet environmental protection and protection workman requirements of physical.
3, environment-friendly type spray glue of the present invention is tasteless, and spraying evenly, and is with low cost.
4, soybean extracting solvent no.6 fast drying, tradition brush coating time of drying, generally need 15 to 20 minutes, and environment-friendly type of the present invention spray glue only needs 1 to 3 minute time of drying, improve operating efficiency widely, thereby opened up the Application Areas of this product in making the software furniture.
5, it is long that environment-friendly type of the present invention is sprayed the tackiness open hour, can reach 15 to 20 minutes, and operating time elasticity is big.
Embodiment
The present invention is further illustrated with embodiment below:
The optimum weight proportioning of this spray glue is: thermoplastic elastomer SBS 8%, rosin 6%, staybelite 7%, petroleum resin 4%, tackifying resin 3%, soybean extracting solvent no.6 49.5%, acetone 5%, hexanaphthene 15%, fourth fat 2% and anti-aging agent 0.5%.
The processing method of making environment-friendly type spray glue of the present invention is as follows:
A. earlier quantitative soybean extracting solvent no.6, acetone, hexanaphthene are dropped in the agitator, machining stirs becomes mixing solutions;
B. more quantitative thermoplastic elastomer SBS is dropped in the agitator and stir;
C. at last quantitative rosin, staybelite, petroleum resin, tackifying resin, fourth fat and anti-aging agent are dropped in the agitator and stir;
D. above material all drops in the agitator back to be continued stirring at normal temperature and dissolved about 6 hours, checks that all materials are dissolved into faint yellow glue fully, and 80 orders filter and get final product then.
Environment-friendly type spray glue of the present invention is suitable for pasting the software furniture most, and this purposes is one of claimed emphasis of the present invention, and its constructional method comprises the steps:
A. clean the veneer of software furniture material to be pasted;
B. with spray gun environment-friendly type spray glue is sprayed on equably the veneer of material to be pasted;
C. placed 1 to 3 minute, and be as the criterion, get final product pressurized adhesion so that sprayed coating is tack-free.

Claims (6)

1, a kind of environment-friendly type spray glue, it is characterized in that: the weight proportion of this spray glue is: thermoplastic elastomer SBS 5-15%, rosin 5-10%, staybelite 5-10%, petroleum resin 2-6%, tackifying resin 2-6%, soybean extracting solvent no.6 45-55%, acetone 2-10% and hexanaphthene 10-20%; Each component sum is 100%.
2, environment-friendly type spray glue according to claim 1, it is characterized in that: the weight proportion of this spray glue also comprises fourth fat and the 0.5-1.0% anti-aging agent of 1-3%.
3, environment-friendly type spray glue according to claim 2, it is characterized in that: the optimum weight proportioning of this spray glue is: thermoplastic elastomer SBS 8%, rosin 6%, staybelite 7%, petroleum resin 4%, tackifying resin 3%, soybean extracting solvent no.6 49.5%, acetone 5%, hexanaphthene 15%, fourth fat 2% and anti-aging agent 0.5%.
4, a kind of compounding process of the spray of environment-friendly type according to claim 1 glue, it is characterized in that: this method comprises the steps:
A. earlier quantitative soybean extracting solvent no.6, acetone, hexanaphthene are dropped in the agitator, machining stirs becomes mixing solutions;
B. more quantitative thermoplastic elastomer SBS is dropped in the agitator and stir;
C. at last quantitative rosin, staybelite, petroleum resin and tackifying resin are dropped in the agitator and stir;
D. above material all drops in the agitator back and continues stirring at normal temperature dissolving 6 hours, checks that all materials are dissolved into faint yellow glue fully, and 80 orders filter and get final product then.
5, the compounding process of environment-friendly type spray glue according to claim 4 is characterized in that: drop into an amount of fourth fat and anti-aging agent and other material and fully mix after step C.
6, a kind of method of using claim 1 or 3 described environment-friendly type spray glue software furnitures, it is characterized in that: this method comprises the steps:
A. clean the veneer of software furniture material to be pasted;
B. with spray gun environment-friendly type spray glue is sprayed on equably the veneer of material to be pasted;
C. placed 1 to 3 minute, and be as the criterion, get final product pressurized adhesion so that sprayed coating is tack-free.
CN 02115305 2002-05-27 2002-05-27 Environment protecting sprayed glue and its prepn and use Expired - Fee Related CN1253521C (en)