CN1219957C - 屋面防水施工方法 - Google Patents
屋面防水施工方法 Download PDFInfo
- Publication number
- CN1219957C CN1219957C CN 03133893 CN03133893A CN1219957C CN 1219957 C CN1219957 C CN 1219957C CN 03133893 CN03133893 CN 03133893 CN 03133893 A CN03133893 A CN 03133893A CN 1219957 C CN1219957 C CN 1219957C
- Authority
- CN
- China
- Prior art keywords
- cloth
- ointment
- pvc
- waterproof
- pvc ointment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种屋面防水施工方法,首先用PVC油膏将布沾到屋面的边缘处,在屋面已铺好的布上面用刮板涂上一层PVC油膏,在PVC油膏上铺一层布,形成两布夹一层PVC油膏,在两布夹一层PVC油膏上铺一层防水卷材;防水卷材的边缘用PVC油膏粘接;在铺好的防水卷材的各搭接处刷PVC油膏,铺布,然后再刷PVC油膏;本发明由于采用了一种复合的施工方法,相当于在屋顶做了一个整体的防水层,能有效的防止由于温差变化和气体膨胀带来的防水层断裂、防水层掀起和屋面被损坏现象的发生。
Description
技术领域
本发明涉及建筑技术领域,特别是一种屋面防水施工方法。
背景技术
目前建筑防水用的防水材料主要有SBS防水卷材、或APP防水卷材、或聚乙烯复合防水卷材、或三元丁橡胶防水卷材,由于SBS防水卷材和APP防水卷材属于沥青材料制成,具有一定的局限性,特别是温差比较大的地区,在屋面变形的情况下,女儿墙、变形缝及雨水口等处出现漏水现象,这两种材料是液化气炉或喷灯烤材料时本身所带沥青部分被烤化贴接而成,如果全面烤,基面通过气体膨胀,容易发生防水层断裂;另外这两种防水材料本身的材质比较硬,在女儿墙和透气口处很难做好防水;而聚乙烯复合防水卷材采用水泥和107胶混合作粘接剂,表面再涂上一层水泥,由于我国的北方地区温差比较大,在热胀冷缩的作用下防水层容易发生断裂;三元丁橡胶防水卷材是目前抗老化性最强的防水材料,比较柔软,抗拉力和延伸力也比较强,其缺点是容易发生脱胶现象,另外它本身也比较薄,容易造成成屋面的损坏,目前的屋面防水施工方法是将防水卷材铺在屋顶上,防水效果差。
发明内容
本发明的目的是提供一种抗老化、抗基面断裂和不容易被风刮起的屋面防水施工方法。
本发明是这样实现的,其特征是:
1.1,首先用PVC油膏将布粘到屋面的边缘处,只粘布边,布的中间不粘PVC油膏,布与布之间搭边铺放,将屋面铺满,在布与布之间的搭接处也刷PVC油膏;
1.2,在屋面已铺好的布上面用刮板涂上一层PVC油膏,PVC油膏的加热温度为65-75℃,刮膏厚度为1.5-2.5毫米;
1.3,在用刮板涂完PVC油膏上面铺一层布,形成两层布夹一层PVC油膏;
1.4,在两层布夹一层PVC油膏的上面铺一层防水卷材,防水卷材的边缘用PVC油膏粘接;
1.5,在防水卷材的各搭接处刷PVC油膏,铺布,然后再刷一层PVC油膏;
1.6,最后在女儿墙、变形孔、出水口和透气孔处实行防水层加厚。
本发明由于采用了一种复合的施工方法,相当于在屋顶做了一个整体的防水层,能有效的防止温差变化和气体膨胀带来的防水层断裂、防水层掀起和屋面被损坏现象的发生。
具体实施方式
实施例1
对一建筑3000平方米的住宅楼进行防水施工,选用三元丁橡胶防水卷材和PVC塑料防水油膏,无纺布混合施工,首先用PVC塑料防水油膏将无纺布粘到屋面的边缘处,PVC油膏的加热温度为65——75℃,刮膏厚度为1.5-2.5毫米,无纺布只粘边,中间不粘油膏,无纺布与无纺布之间搭边铺放,将屋面铺满,在无纺布与无纺布之间的搭接处也刷PVC塑料防水油膏;在屋面已铺好的无纺布上面用刮板涂上一层PVC塑料防水油膏;在用刮板涂完PVC塑料防水油膏上面铺一层无纺布,形成两层布夹一层PVC塑料防水油膏结构;在两布夹一层PVC油膏的上面铺一层三元丁橡胶防水卷材,三元丁橡胶防水卷材的边缘用PVC塑料防水油膏粘接;在铺好的防水卷材的各搭接处刷PVC塑料防水油膏,铺布,然后再刷一层PVC油膏;最后在女儿墙、变形孔、出水口和透气孔处实行防水层加厚,防水卷材可以使用SBS防水卷材、或APP防水卷材、或聚乙烯复合防水卷材、或三元丁橡胶防水卷材;所述的布包括绵布、或化纤布、或无纺布。
Claims (3)
1、一种屋面防水施工方法,其特征是:
1.1,首先用PVC油膏将布粘到屋面的边缘处,只粘布边,布的中间不粘PVC油膏,布与布之间搭边铺放,将屋面铺满,在布与布之间的搭接处也刷PVC油膏;
1.2,在屋面已铺好的布上面用刮板涂上一层PVC油膏,PVC油膏的加热温度为65-75℃,刮膏厚度为15-25毫米;
1.3,在用刮板涂完PVC油膏上面铺一层布,形成两层布夹一层PVC油膏;
1.4,在两层布夹一层PVC油膏的上面铺一层防水卷材,防水卷材的边缘用PVC油膏粘接;
1.5,在防水卷材的各搭接处刷PVC油膏,铺布,然后再刷一层PVC油膏;
1.6,最后在女儿墙、变形孔、出水口和透气孔处实行防水层加厚。
2、根椐权利要求1所述的屋面防水施工方法,其特征是所述的防水卷材包括SBS防水卷材、或APP防水卷材、或聚乙烯复合防水卷材、或三元丁橡胶防水卷材。
3、根椐权利要求1所述的屋面防水施工方法,其特征是所述的布包括绵布、或化纤布、或无纺布。